Characterisation of resin–dentine interfaces by compressive cyclic loading
Source abstract
Abstract
The aims of this in vitro study were to evaluate the ultra-morphological changes in resin-dentine interfaces after different amounts of thermomechanical load (TML), and to determine the corresponding microtensile bond strengths (microTBS). Enamel/dentine discs with a thickness of 2 mm were cut from 24 human third molars and bonded with four adhesives involving different adhesion approaches: Syntac (Ivoclar Vivadent; used as multi-step etch-and-rinse adhesive), Clearfil SE Bond (Kuraray; two-step self-etch adhesive), Xeno III (Dentsply DeTrey; mixed all-in-one self-etch primer adhesive system), and iBond (Heraeus Kulzer; non-mixed all-in-one self-etch adhesive). The resin-dentine discs were cut into beams (width 2 mm; 2 mm dentine, 2 mm resin composite) and subsequently subjected to cyclic TML using ascending amounts of mechanical/thermal cycles (20 N at 0.5 Hz of mechanical load and 5-55 degrees C of thermal cycles: for 0/0, 100/3, 1,000/25, 10,000/250, 100,000/2,500 cycles). Loaded specimens were either cut perpendicularly in order to measure microTBS (n=20; crosshead speed: 1 mm/min) or were immersed in an aqueous tracer solution consisting of 50 wt% ammoniacal silver nitrate and processed for ultra-morphological nanoleakage examination using transmission electron microscopy (TEM). microTBS were significantly decreased by increasing amounts of TML for all adhesives (p<0.05). Bond strengths after 0 vs. 100,000 thermomechanical cycles were: Syntac: 41.3/30.1 MPa; Clearfil SE Bond 44.8/32.5 MPa; Xeno III 27.5/13.7 MPa; iBond 27.0/6.2 MPa. Relatively early, a certain amount of nanoleakage was observed in all groups by TEM, which was more pronounced for Xeno III and iBond. The incidence of nanoleakage remained stable or was even reduced with increasing load cycles for all adhesives except iBond, where exact failure origins were detected within the adhesive and at the top of the hybrid layer.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Buonocore memorial lecture. Adhesion to enamel and dentine
2. Use of posterior composite resin restorations by Dutch dental practitioners
3. Dentine adhesives
4. Composite resin fillings and inlays. An 11-year evaluation10.1007/s00784-003-0201-z ↗
5. Short- and long-term clinical evaluation of post-operative sensitivity of a new resin-based restorative material and self-etching primer
6. Clinical relevance of laboratory fatigue studies10.1016/0300-5712(94)90010-8 ↗
7. Fatigue of composites—fatigue modulus concept and life prediction10.1177/002199838602000203 ↗
8. Fatigue behaviour of different dentine adhesives10.1007/s007840050072 ↗
9. De Munck J, Braem M, Wevers M, Lambrechts P, Van Meerbeek B. Micro-rotary fatigue of tooth–biomaterial interfaces. Biomaterials, in press, available online: June 2004, doi: 10.1016/j.biomaterials.2004.04.01310.1016/j.biomaterials.2004.04.013 ↗
10. Testing mode and surface treatment effects on dentine bonding10.1002/(SICI)1097-4636(199612)32:4<533::AID-JBM6>3.0.CO;2-S ↗
11. In vitro fatigue testing of a dental bonding system on enamel10.1002/jbm.820290316 ↗
12. Crack propagation at the bone–cement interface
13. The prediction of crack growth in bonded joints under cyclic-fatigue loading. I. Experimental studies10.1016/S0143-7496(03)00074-5 ↗
14. Fatigue crack growth in structural adhesives10.1080/00218468008078911 ↗
15. Mode I fracture of epoxy bonded composite joints10.1016/S0143-7496(01)00050-1 ↗
16. Observations of fatigue crack initiation and propagation in an expoxy adhesive10.1016/S0143-7496(96)00044-9 ↗
17. Long-term durability of resin–dentine interface
18. The effect of six years water storage on resin composite bonding to human dentine10.1002/jbm.b.20024 ↗
19. Aging affects two modes of nanoleakage expression in bonded dentine10.1177/154405910308200710 ↗
20. Four-year water degradation of total-etch adhesives bonded to dentine10.1177/154405910308200212 ↗
21. Resin reinforced dentine due to infiltration of monomers into dentine at the adhesive interface
22. Hybridization efficiency of the adhesive/dentine interface with wet bonding10.1177/154405910308200213 ↗
23. Comparative SEM and TEM observations of nanoleakage within the hybrid layer
24. Nanoleakage
25. Adhesive phase separation at the dentine interface under wet bonding conditions10.1002/jbm.10364 ↗
26. Water treeing—a potential mechanism for degradation of dentine adhesives
27. How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously?
28. Two modes of nanoleakage expression in single-step adhesives10.1177/154405910208100708 ↗
29. Single-step adhesives are permeable membranes10.1016/S0300-5712(02)00064-7 ↗
30. Aging affects two modes of nanoleakage expression in bonded dentine10.1177/154405910308200710 ↗
31. Adhesive permeability affects composite coupling to dentine treated with a self-etch adhesive
32. Stress dependence of water diffusion in epoxy resin10.1002/pc.750010205 ↗
33. Coupling between stresses and moisture diffusion in polymeric adhesives10.1002/pen.760271006 ↗
34. Dynamic percolation theory for particle diffusion in a polymer network10.1063/1.1481763 ↗
35. Probing the molecular interactions in the diffusion of water through epoxy and epoxy-bismaleimide networks10.1002/polb.10147 ↗
36. Epoxy and glass composites in water studied with 2H-NMR10.1002/pen.10506 ↗
37. Relationships between stoichiometry, microstructure, and properties for amine-cured epoxies10.1002/(SICI)1097-4628(19990131)71:5<699::AID-APP4>3.0.CO;2-D ↗
38. Bonding to dentine with a self-etching primer10.1016/S0109-5641(00)00049-X ↗
39. The influence of c-factor and layering technique on microtensile bond strength to dentin10.1016/j.dental.2003.08.001 ↗
40. Fatigue behavior of the resin–dentin bond using different evaluation methods10.1002/jbm.b.10052 ↗
41. Distribution of nanofillers from a simplified-step adhesive in acid-conditioned dentine
42. Effect of thermal and mechanical load cycling on microtensile bond strength of a total-etch adhesive system
43. Masticatory function—a review of the literature (II) Speed of movement of the mandible, rate of chewing and forces developed in chewing10.1111/j.1365-2842.1975.tb01535.x ↗