journal article·2005-02

Analysis and evaluation of a biomedical polycarbonate urethane tested in an in vitro study and an ovine arthroplasty model. Part II: in vivo investigation

Imran Khan, Nigel Smith, Eric Jones, Dudley S Finch, Ruth Elizabeth Cameron

Biomaterials· Volume 26· Issue 6
Publisher page

Abstract

The polyurethane (PU) elastomer Corethane 80A (Corvita) is being considered as the acetabular bearing material in a novel total replacement hip joint. Its biostability was investigated in vitro (Analysis and evaluation of a biomedical polycarbonate urethane tested in an in vitro study and an ovine arthroplasty model. Part I: material selection and evaluation, Biomaterials, in press) together with three other commercially available biomedical PUs: Pellethane 2363-80A (DOW Chemical), a polyhexamethylene oxide based PU, PHMO-PU (CSIRO, not supplied as a commercial product) and ChronoFlex AL-80A (CardioTech). From the in vitro studies, Corethane 80A displayed the best overall resistance to hydrolysis, ESC, MIO and calcification, followed by ChronoFlex 80A and PHMO-PU, with Pellethane 80A being the least stable. Building on the in vitro investigation, the follow-up in vivo study (reported here) assessed Corethane 80A as the bearing layer in a prototype compliant layer acetabular cup, in a fully functioning ovine total hip arthoplasty (THA) model. PU degradation in the retrieved cups was analysed using a range of analytical and physical-testing methods including mechanical testing, differential scanning calorimetry, Fourier transform infrared spectroscopy and environmental scanning electron microscopy. The Corethane 80A functioned well in the THA model, with the bearing surfaces of the retrieved hip cups showing no significant evidence of biodegradation or wear damage after 3 years in vivo. The findings in this study provide compelling evidence for the biostability and effectiveness of acetabular cups incorporating a Corethane 80A compliant bearing layer.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Khan I, Cameron RE, Smith N. Analysis and evaluation of a biomedical polycarbonate urethane tested in an in vitro study and an ovine arthroplasty model. Part I: material selection and evaluation. (Biomaterials, in press).
2. Okumura Y, Omori H, Ooki HH, Baba MO. The effects of cup abduction angle on the stability, PE wear of acetabular component in cementless total hip arthroplasty. Transactions of the 45th Annual Meeting, Orthopaedic Research Society, 1999. p. 928.
3. Malchau H, Herberts P. Revision and re-revision rate in THR: a revision––risk study of 148 359 primary operations. Prognosis of total hip replacement, Department of orthopaedics, University of Göteborg, Sweden; 1998.
4. Alexander JW, Kamaric E, Noble PC. The accuracy of acetabular reaming in total hip replacement. Transactions of the 45th Annual Meeting, Orthopaedic Research Society, 1999. p. 906.
5. Moody J, DiGioia A, Jaramaz B, Blackwell M, Colgan B, Nikou C. Inaccuracy of mechanical guides used for acetabular component alignment in total hip replacement. Transactions of the 45th Annual Meeting, Orthopaedic Research Society, 1999. p. 278.
6. The contribution of frictional torque to loosening at the cement-bone interface in Tharies hip replacements10.2106/00004623-199604000-00004 ↗
7. Composition, morphology of wear debris in failed uncemented total hip replacement10.1302/0301-620X.76B1.8300684 ↗
9. Polyethylene debris-induced osteolysis and loosening in uncemented total hip arthroplasty
10. The acetabular component in total hip arthroplasty
11. Advances in the processing, sterilization and crosslinking of ultra high molecular weight polyethylene for total joint arthroplasty10.1016/S0142-9612(99)00053-8 ↗
12. Wear of gamma-crosslinked polyethylene acetabular components10.1097/00003086-199912000-00008 ↗
13. The comparison of the wear behaviour of four different types of cross-linked acetabular components10.1016/S0736-0266(01)00059-6 ↗
14. Laurent MP, Yao JQ, Gilbertson LN, Swarts DF, Crowninshield RD. Wear of highly cross-linked UHMWPE acetabular liners under adverse conditions. Transactions of the 25th Annual Meeting of the Society of Biomaterials, 2000. p. 874.
15. Current concepts review UHMWPE10.2106/00004623-199407000-00020 ↗
16. Laurent MP, Yao JQ, Bhambri SK, Gselli RA, Gilbertson LN, Swarts DF, Crowninshield RD. High cycle wear of highly cross-linked UHMWPE acetabular liners evaluated in hip simulator. Transactions of the 26th Annual Meeting of the Society of Biomaterials, 2000. p. 851.
17. Kellop HA, Di Maio WG, Shen F-W, LuB. Wear of gamma radiation crosslinked polyethylene acetabularcups after ageing and against roughened femoral heads. Transactions of the 45th Annual Meeting, Orthopaedic Research Society, 1999. p. 76.
18. Muratoglu OK, Bragdon CR, O’Connor DO, Jasty M, Harris WH. A comparison of 5 different types of highly cross-linked UHMWPEs: physical properties and wear behaviour. Transactions of the 45th Annual Meeting, Orthopaedic Research Society, 1999. p. 77.
19. Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements10.1002/jor.1100170203 ↗
20. Clinical wear of 63 ultra- high molecular weight polyethylene acetabular components10.1002/(SICI)1097-4636(1999)48:3<374::AID-JBM23>3.0.CO;2-O ↗
21. Shaw JH. The effect of gamma irradiation of UHMWPE medical devices agency––lit review; 1997. http://www.medical-devices.gov.uk
22. Irradiation of UHMWPE
23. Radiation-induced physical changes in UHMWPE implant components10.3928/0147-7447-19970201-11 ↗
24. Technique and results for total hip replacement in sheep10.1055/s-0038-1632523 ↗
25. Radiographic and histological analysis of cemented double-tapered femoral stems10.1097/00003086-199810000-00024 ↗
26. Hip joint forces in sheep10.1016/S0021-9290(99)00068-8 ↗
27. A comparison of hip joint forces in sheep, dog and man10.1016/0021-9290(84)90004-6 ↗
28. Technique and results for total hip replacement in sheep10.1055/s-0038-1632523 ↗
29. Recent developments in the tribology of artificial joints10.1016/0301-679X(95)00027-2 ↗
30. Dowson D. The lubrication of synovial joints. Proceedings of the 9th Canadian Congress of Applied Mechanics, University Saskatchewan, Canada; 1983, p. 15–30.
31. Design considerations in cushion form bearings for artificial hip joints
32. Smith N, Doyle C, Jones E. Prosthetic bearing element and process for making such an element European Patent No EP698382, 1996.
33. An ovine model for total hip replacement10.1055/s-0038-1632670 ↗
34. Vernon-Roberts B. Institutional ethics committee guidelines, University of Adelade, Australia. Personal communication; April 1997.
35. Carbone A, McGee M, Field J, Howie AH, Smith N, Jones E. Compliant layer sheep hip arthroplasty project: results of an in vivo time series study. Vet J Biomater, in draft.
36. Start up and steady-state friction of thin polyurethane layers10.1016/0043-1648(93)90420-Q ↗
37. The effect of average soft segment length on morphology and properties of a series of polyurethane elastomers. 2. SAXS-DSC annealing study10.1002/(SICI)1097-4628(19970425)64:4<803::AID-APP20>3.0.CO;2-T ↗
38. The effect of thermal annealing on the thermal properties and molecular weight of a segmented polyurethane copolymer10.1002/polb.1994.090320304 ↗
39. Advances in Elastomers and Rubber Elasticity
40. The effect of hard segment size on the hydrolytic stability of polyether-urea-urethanes when exposed to cholesterol esterase10.1002/(SICI)1097-4636(199708)36:2<223::AID-JBM11>3.0.CO;2-H ↗
41. The enzymatic degradation of polymers in vitro10.1002/jbm.820210805 ↗
42. Elastase-induced hydrolysis of synthetic solid substrates
43. Enzyme-biomaterial interactions10.1002/jbm.820270113 ↗
44. Biodegradation evaluation of polyesterurethanes with oxidative and hydrolytic enzymes10.1002/jbm.820281009 ↗
45. The enzymatic hydrolysis of a synthetic biomembrane10.1163/156856294X00293 ↗
46. Enzyme-induced biodegradation of polycarbonate polyurethanes10.1002/1097-4636(20010915)56:4<516::AID-JBM1123>3.0.CO;2-B ↗
47. Enzyme-induced biodegradation of polycarbonate-polyurethanes10.1002/1097-4636(20011215)57:4<597::AID-JBM1207>3.0.CO;2-T ↗
48. Influence of surface morphology and chemistry on the enzyme catalyzed biodegradation of polycarbonate-urethanes10.1163/156856202320253965 ↗
49. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
50. An FTIR-ATR investigation of in vivo poly (etherurethane) degradation10.1002/app.1992.070460202 ↗
51. Dillon · 1989
52. Dowson D. Fluid film lubrication Osborne Reynolds Centenary. Proceedings of the 13th Leeds–Lyon Symposium on Tribology, Leeds, 1986.