journal article·2004-08

Effects of resin formulation and nanofiller surface treatment on the properties of experimental hybrid resin composite

Lawrence Musanje, Jack L. Ferracane

Biomaterials· Volume 25· Issue 18
Publisher page

Abstract

This study evaluated the effects of nanofiller surface treatment and resin viscosity on the early and long-term properties of experimental hybrid composites. Three resin formulations (low, medium and high viscosity) were prepared by varying the ratio of TEGDMA:UDMA:bis-GMA (47:33:16 wt%; 30:33:33 wt%; 12:33:51 wt%). Composites contained 71.3 wt% silanated strontium glass (1-3 microm) and 12.6 wt% of either silanated or unsilanated silica (OX-50; 0.04 microm). Specimens (n=10) for flexural strength, flexural modulus, fracture toughness and Knoop hardness were tested after 24 h, 1 and 6 months exposure to water at 37 degrees C. Degree of conversion (DC) was determined 24 h after photoinitiation using FTIR. Resin viscosity only had a marginal influence on the mechanical response of composites but it can be adjusted to achieve a balance between DC and mechanical properties. Adding non-bonded nanofiller to hybrid composites had no systematic effect on DC. Non-bonded nanofillers had no significant effect on the long-term properties of hybrid composites.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Reduction of composite contraction stress through non-bonded micro-filler particles10.1016/S0109-5641(98)00036-0 ↗
2. Reduced polymerization stress through non-bonded nanofiller particles10.1016/S0142-9612(02)00099-6 ↗
3. Quantitative determination of stress reduction by flow in composite restorations10.1016/0109-5641(90)90023-8 ↗
4. Quality and durability of marginal adaptation in bonded composite restorations10.1016/0109-5641(91)90055-4 ↗
5. Effect of cavity depth and application technique on marginal adaptation of resins in dentin cavities10.1177/00220345860650110701 ↗
6. Effect of soft-start irradiation on depth of cure and marginal adaptation to dentin
7. Comparison of marginal integrity of in vivo and in vitro class II composite restorations10.1016/0300-5712(93)90026-M ↗
8. Effect of composite resin placement techniques on the microleakage of two self-etching dentin-bonding agents
9. Relaxation of polymerization contraction stresses by flow in dental composites10.1177/00220345840630021001 ↗
10. In vitro aging of dental composites in water—effect of degree of conversion, filler volume, and filler/matrix coupling10.1002/(SICI)1097-4636(19981205)42:3<465::AID-JBM17>3.0.CO;2-F ↗
11. Heap · 1969
12. Remaining methacrylate groups in composite restorative materials10.3109/00016357809027569 ↗
13. Factors affecting the quantity of remaining double bond in restorative resin polymers
14. Fourier transform infrared analysis of degree of polymerization in unfilled resins—methods comparison10.1177/00220345840630081901 ↗
15. Effect of chemical structure on degree of conversion in light-cured dimethacrylate-based dental resins10.1016/S0142-9612(01)00308-8 ↗
16. Influence of UEDMA, Bis-GMA and TEGDMA on selected mechanical properties of experimental resins composites10.1016/S0109-5641(98)00009-8 ↗
17. The effect of environment aging on the fracture toughness of dental composites10.1177/00220345870660030301 ↗
18. Variables affecting the fracture toughness of resin-based inlay/onlay systems10.1111/j.1365-2842.1993.tb01626.x ↗
19. KIc of dental composites using the short-rod KIc test10.1177/00220345860650110501 ↗
20. Long-term water-aging of whisker-reinforced polymer-matrix composites10.1177/154405910308200111 ↗
21. Filler leachability of composites stored in distilled water or artificial saliva10.1177/00220345960750091201 ↗
22. Influence of filler type and water exposure on flexural strength of experimental composite resins10.1177/00220345880670050801 ↗
23. Effect of 180-week water storage on the flexural properties of E-glass and silica fibre acrylic resin composite
24. Annealing as a mechanism of increasing wear resistance of composites10.1016/S0109-5641(05)80008-9 ↗
25. Water sorption and mechanical behaviour of cosmetic direct restorative materials in artificial saliva10.1016/S0109-5641(00)00097-X ↗
26. Changes in expansion and mechanical strength during water storage of a traditional and three modified resin composites10.1080/000163502760147954 ↗
27. Water absorption characteristics of dental microfine composite filling materials. II. Experimental materials10.1016/0142-9612(84)90039-5 ↗
28. Water sorption and solubility of glass fibre-reinforced denture polymethyl methacrylate resin10.1016/S0022-3913(97)70147-1 ↗
29. Effect of resin matrix ratio, storage medium, and time upon the physical properties of a radiopaque dental composite10.1177/088532820001400306 ↗
30. Water sorption and mechanical properties of dental composites10.1016/0142-9612(90)90159-N ↗
31. Physical and mechanical properties of anterior and posterior composite restorative materials10.1016/0109-5641(89)90100-0 ↗