Comparative hardness and modulus of tooth-colored restoratives: A depth-sensing microindentation study
Source abstract
Abstract
The objective of this study was to compare the hardness and modulus of the continuum of direct tooth-colored restorative materials using a depth-sensing microindentation approach. The effects of thermal fatigue on mechanical properties were also evaluated. Six restorative materials representing the continuum were selected. They included an ormocer (Admira [AM], Voco), a giomer (Beautifil [BF], Shofu), a compomer (Dyract Extra [DE], Dentsply), a minifill composite (Esthet-X [EX], Dentsply), resin-modified (Fuji II LC [FL], GC) and highly viscous (Fuji IX [FN], GC) glass ionomer cements (GICs). Fourteen specimens (3 mm wide x 3 mm long x 2 mm deep) were made for each material. The specimens were randomly divided into two groups and treated as follows: Group A--stored in distilled water at 37 degrees C for 30 days; Group B--thermal cycled for 5000 cycles (35 degrees C [28s], 15 degrees C [2s], 35 degrees C [28s], 45 degrees C [2s]) and stored for 26.5 days. Hardness and modulus of the materials were determined using depth-sensing microindentation testing with the Instron MicroTester. Hardness was computed by dividing the peak load over the maximum projected contact area while modulus was calculated by analysis of the loading/unloading load-displacement (P-h) curves and the analytical model according to Oliver and Pharr (J. Mater. Res. 7 (1992) 1564). Results were analyzed using ANOVA/Scheffe's post hoc test and independent samples T-test (p<0.05). Hardness ranged 46.44-72.65 and 49.11-78.97 HV, while modulus ranged 7.86-12.78 and 8.12-13.13 GPa for Groups A and B, respectively. Although the ranking of mechanical properties were generally similar for both groups, disparities in statistical differences between materials were observed between Groups A and B for both hardness and modulus. For both groups, BF was significantly harder than DE, AM, FL and EX was significantly harder than FL. The modulus of FN was significantly greater than EX, DE, AM and FL was significantly stiffer than AM. With the exception of BF, no significant change in hardness and modulus was observed for all materials with thermocycling. The hardness and modulus of some glass ionomer-based/containing materials may be comparable or even superior to minifill and ormocer composites. Thermal fatigue should be considered when comparing mechanical properties between materials.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Proposed nomenclature for glass ionomer cements and related materials
2. Surface finish of a new hybrid aesthetic restorative material
3. The glass ionomer phase in resin-based restorative materials10.1177/00220345010800090701 ↗
4. Roberts TA, Miyai K, Ikemura K, Fuchigami K, Kitamura T. Fluoride ion sustained release pre-formed glass ionomer filler and dental compositions containing the same. 1999; US patent no. 5883, p. 153.
5. International Standards Organization. Dental materials—water-based cements Part 1—powder/liquid acid–base cement. 2001; ISO 9917-1.
6. International Standards Organization. Dentistry—resin-basedfilling, restorative and luting materials. 2000; ISO 4049.
7. International Standards Organization. Dental water-based cements Part 2—light activated cements. 1998; ISO 9917-2.
8. O’Brien WJ. Dental materials, their selection. Chicago: Quintessence Publishing Co; 1997. p. 18.
9. Anusavice KL. Phillip's science of dental materials, 10th ed. Philadelphia: WB Saunders Co; 1996. p. 69.
10. Dynamic and static moduli of elasticity of resin-based materials10.1016/S0109-5641(01)00021-5 ↗
11. Evaluation of clinical performance of posterior composite resins and dentin adhesives
12. Hardness and Young's modulus determined by nanoindentation technique of filler particles of dental restorative materials compared with human enamel10.1002/jbm.820270607 ↗
13. Indentation modulus and hardness of whisker-reinforced heat-cured dental resin composites
14. The hardness and modulus of elasticity of primary teeth10.1016/S0300-5712(00)00043-9 ↗
15. Continuous measurements of load-penetration curves with spherical micro-indenters and the estimation of mechanical properties10.1557/JMR.1998.0197 ↗
16. Thermal-cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
17. A method for interpreting the data from depth-sensing indentation instrumentations10.1557/JMR.1986.0601 ↗
18. The relation between load and penetration in the axissymmetric Boussinesq problem for a punch of arbitrary profile10.1016/0020-7225(65)90019-4 ↗
19. Elastic recovery of conical indentations10.1088/0370-1328/78/2/302 ↗
20. Determining Young's modulus from the indentation penetration diagram
21. Simmons G, Wang H. Single crystal elastic constants and calculated aggregate properties: a handbook, 2nd ed. Cambridge: MIT Press; 1971.
22. Elastic analysis of some punch problems for a layered medium
23. Elastic properties of dental resin restorative materials10.1177/00220345740530050901 ↗
24. Measurement at low strain rates of the elastic properties of dental polymeric materials10.1016/S0109-5641(99)00011-1 ↗
25. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
26. Analysis of Vickers indentation10.1016/0020-7683(94)90225-9 ↗
27. Determination of elastoplastic properties by instrumented sharp indentation10.1016/S1359-6462(99)00011-1 ↗
28. Computationaly modeling of the forward and reverse problems in instrumented sharp indentations10.1016/S1359-6454(01)00295-6 ↗
29. Changes in flexural properties of composite restoratives after aging in water
30. Comparison of flexural properties of composite restoratives using the ISO and mini-flexural tests10.1046/j.1365-2842.2003.01004.x ↗
31. Leaking of fillers in dental composites10.1177/00220345830620020801 ↗
32. Surface permeability and degradation of dental composites resulting from oral temperature changes10.1016/0109-5641(89)90070-5 ↗
33. Effect of surface conditioning on the abrasion rate of dental composites10.1016/0300-5712(91)90099-K ↗
34. Influence of thermal cycling on OCA wear of composite restoratives
35. Effects of cyclic temperature changes on hardness of composite restoratives
36. The effect of curing light intensity and test temperature on the dynamic properties of two polymer composite10.1046/j.1365-2842.1999.00432.x ↗
37. Current trends in dental composites10.1177/10454411950060040301 ↗
38. Mechanical properties of an improved visible light-cured resin-modified glass ionomer cement
39. Water sorption characteristics of resin-modified glass ionomer cements10.1016/S0142-9612(96)00124-X ↗
40. Resin-modified glass ionomer cements. A comparison of water sorption characteristics10.1016/0142-9612(95)00344-4 ↗