Isothermal crystallization through annealing at 115 degrees C was conducted to increase the degree of crystallinity of poly (lactide-co-glycolide) (PLGA). The maximum increase in the degree of crystallinity (approximately 21%) was achieved after 60 min of annealing. The crystal size/perfection was observed to increase with annealing time. The annealed PLGA films were then hydrolytically degraded in phosphate buffered saline solution of pH 7.4 at 37 degrees C for up to 150 days. Minimal mass loss was observed throughout the time investigated, suggesting that the samples were still in the first phase of degradation. The increase in the degree of crystallinity of the PLGA samples annealed at 15 and 30 min was found to retard their overall rate of hydrolytic degradation, when compared to those samples with higher initial crystallinity (annealed for 45 and 60 min) that had faster degradation rates. The increased degradation rate at higher crystallinity was associated with the loss of amorphous material and the formation of voids during annealing, which decreases the glass transition temperature and increases the average water uptake in the samples annealed for longer times. Therefore, the increase in degree of crystallinity is found to retard hydrolytic degradation but only to a certain extent, beyond which the formation of voids through annealing increases the rate of hydrolytic degradation.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: biodegradable polymer synthesis and properties · Bone Tissue Engineering Materials · Polymer Surface Interaction Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Peppas NA, Huang Y, Torres-Lugo M, Ward JH, Zhang J. Physicochemical foundations and structural design of hydrogels in medicine and biology. Ann Rev Biomed Eng 2000;(2):9–27.10.1146/annurev.bioeng.2.1.9 ↗
2. Wu · 1995
3. Griffith LG. Polymeric biomaterials. Acta Mater 2000;(48): 263–77.10.1016/S1359-6454(99)00299-2 ↗
4. Tice · 1991
5. Perspectives on the in vivo responses of biodegradable polymers
6. Biodegradation of aliphatic polyesters
7. Degradation and biocompatibility of synthetic absorbable suture materials
8. Lewis · 1990
9. Gilding DK, Reed AM. Biodegradable polymers for use in surgery—Polyglycolic/polylactic acid homo- and copolymers. Polymer 1979;(20):1459–64.10.1016/0032-3861(79)90009-0 ↗
10. Holland SJ, Tighe BJ. In: Ganderton D, Jones TJ, editors. Biodegradable polymers. Advances in pharmaceutical sciences, vol. 6. London: Academic Press; 1992. p. 101–64.
11. Munk · 2002
12. Cowie · 1991
13. Loo SCJ, Ooi CP, Boey YCF. Radiation effects on poly(lactide-co-glycolide) (PLGA) and poly(l-lactide) (PLLA). Polym Degrad Stab 2004;(83):259–65.10.1016/S0141-3910(03)00271-4 ↗
14. Cullity · 1978
15. Biodegradable delivery system for single step immunization with tetanus toxoid10.1016/0378-5173(93)90188-L ↗