journal article·2002-08

FTIR investigation of polymerisation and polyacid neutralisation kinetics in resin-modified glass-ionomer dental cements

A.M. Young

Biomaterials· Volume 23· Issue 15
Publisher page

Abstract

A new diamond ATR FTIR method has been developed to quantify the processes occurring in the resin-modified glass-ionomer cement (RMGIC). Fuji II LC (Improved), at 1 mm depth from the cement/water interface. With Fuji II LC (Improved) various changes in the spectra due to 90% monomer polymerisation were observed within 1 min after 20 s exposure to a dental light. Following polymerisation further different peak shifts with time were detected. Comparison with spectral changes seen during setting of the conventional glass-ionomer cement, Fuji IX, showed these could be assigned to water sorption and/or polyacid neutralisation. Any absorbance change due to the acid/glass reaction alone exhibited 2 linear regions when plotted against square root of time. Such behaviour suggests two separate diffusion mechanisms for acid neutralisation. The first faster one ceases at 30 or 150 min after mixing in Fuji IX and Fuji II LC (Improved), respectively. It was proposed that these were the times at which all the water (a required component of the reaction) in the original formulation is used up. The slower process was the same acid/glass reaction but initiated by water sorption. The initial rates of absorbance change due to acid neutralisation were 17 times faster for Fuji IX than Fuji II LC (Improved). By 4 days however, the total absorbance change due to acid neutralisation for Fuji IX was only 4 times that for Fuji II LC (Improved). Such results can help to explain changes in cement properties with time.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Chemistry of glass-ionomer cements10.1016/S0142-9612(97)00128-2 ↗
2. Microhardness of in vitro caries inhibition zone adjacent to conventional and resin-modified glass ionomer cements10.1016/S0109-5641(98)00026-8 ↗
3. Development of glass-ionomer cement systems10.1016/S0142-9612(97)00126-9 ↗
4. Mechanical properties and microstructures of glass-ionomer cements10.1016/S0109-5641(99)00093-7 ↗
5. A simple method for the measurement of polymerization shrinkage in dental composites10.1016/S0109-5641(99)00073-1 ↗
6. Bonding agent is a decisive factor in determining the marginal leakage of dental composites subjected to thermal cycling10.1046/j.1365-2842.2001.00609.x ↗
7. Resin-modified glass-ionomers10.1016/S0142-9612(98)00132-X ↗
8. Long-term flexural strengths of resin-modified glass-ionomer cements10.1016/S0142-9612(98)00079-9 ↗
9. Fluoride release from glass-ionomer cements, compomers and resin composites10.1046/j.1365-2842.2001.00635.x ↗
10. Effect of the application of dentin primers and a dentin bonding agent on the adhesion between the resin-modified glass-ionomer cement and dentin10.1016/S0109-5641(98)00040-2 ↗
11. Visco-elastic parameters of dental restorative materials during setting10.1177/00220345000790030601 ↗
12. An in vitro investigation of a poly (vinyl phosphonic acid) based cement with four conventional glass-ionomer cements. Part 210.1016/S0300-5712(98)00062-1 ↗
13. Factors influencing the setting reaction of glass polyalkenoate (ionomer) cements10.1016/0300-5712(88)90101-7 ↗
14. Thermal analysis of visible-light-activated dental composites10.1016/0040-6031(95)02367-4 ↗
15. Reactions in glass-ionomer cements10.1177/00220345740530062001 ↗
16. FTIR study of the role of tartaric acid in glass-ionomer dental cements10.1177/00220345880670120201 ↗
17. Use of Raman spectroscopy to investigate the acid base reaction in glass-ionomer cements10.1016/S0142-9612(00)00081-8 ↗
18. Calibration of FTIR conversion analysis of contemporary dental resin composites10.1016/S0109-5641(05)80005-3 ↗
19. The micro-Raman spectroscopy, a useful tool to determine the degree of conversion of light-activated composite resins10.1002/(SICI)1097-4636(1999)48:5<675::AID-JBM11>3.0.CO;2-P ↗
20. An FTIR study on the setting mechanism of resin-modified glass ionomer restoratives10.1016/S0109-5641(96)80017-0 ↗
21. Acid base complex reactions in resin-modified and conventional class ionomer cements10.1002/(SICI)1097-4636(1999)48:5<700::AID-JBM15>3.0.CO;2-1 ↗
22. Acid–base reaction and fluoride release profiles in visible light-cured and polyacid–modified composite restoratives (compomers)10.1016/S0109-5641(98)00010-4 ↗
23. Off-line monitoring of butyl acrylate, methyl methacrylate and vinyl acetate homo-and copolymerizations in toluene using ATR-FTIR spectroscopy10.1016/S0032-3861(01)00085-4 ↗
24. Young AM. unpublished data.
25. Young AM, Sherpa A, Pearson GJ, Schottlander B. Spectroscopic characterisation of new fluoride releasing aesthetic dental restoratives. PIMS 2000, Ninth International Conference on Polymers in Medicine and Surgery, IOM Communications Ltd., 2000.