journal article·2003-06

Volumetric contraction and methacrylate conversion in photo-polymerized amorphous calcium phosphate/methacrylate composites

D Skrtic, J.W Stansbury, J.M Antonucci

Biomaterials· Volume 24· Issue 14
Publisher page

Abstract

Because of its relatively high solubility in aqueous media and its rapid transformation to hydroxyapatite, amorphous calcium phosphate (ACP) has been utilized as the filler phase of resin-based bioactive composites that have remineralization potential. The objectives of this study were to determine how various methacrylate resins and various types of ACP fillers affect acrylic vinyl conversion and polymerization shrinkage (PS). Several types of photo-crosslinkable resin systems were prepared and admixed with a mass fraction of 40% of either unhybridized, silica- or zirconia-hybridized ACP. After visible light-activated photo-polymerization ACP composites were assessed by near infrared spectroscopy for degree of vinyl conversion and by mercury dilatometry for PS. It was found for these composites that vinyl conversion was independent of filler type but strongly dependent on the type and composition of the resin phase. PS, on the other hand, showed more complex dependence both on the resin type and composition and, in some cases, on the type of ACP. In order to obtain ACP/methacrylate-based composites with maximal vinyl conversion, resin type and composition are of primary importance. However, in order to minimize volume contraction on polymerization it appears necessary to consider both the resin and filler type of these bioactive composites.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Photopolymerization techniques and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Bioactive dental materials based on amorphous calcium phosphate
2. Remineralizing dental composites based on amorphous calcium phosphate
3. Quantitative assessment of the efficacy of amorphous calcium phosphate/methacrylate composites in remineralizing caries-like lesions artificially produced in bovine enamel10.1177/00220345960750091001 ↗
4. Improved properties of amorphous calcium phosphate fillers in remineralizing resin composites10.1016/S0109-5641(96)80037-6 ↗
5. Polymeric calcium phosphate composites with remineralization potential
6. Molecularly designed dental polymers
7. Intermediate states in the precipitation of hydroxyapatite10.1038/208365a0 ↗
8. Volumetric contraction measured by a computer-controlled mercury dilatometer
9. Determination of double bond conversion in dental resins by near infrared spectroscopy10.1016/S0109-5641(00)00062-2 ↗
10. Polymerization contraction and conversion of light-curing BisGMa-based methacrylate resins10.1016/0142-9612(93)90010-Y ↗
11. Light intensity effects on resin-composite degree of conversion and shrinkage strain10.1016/S0109-5641(00)00020-8 ↗
12. Contraction stress related to degree of conversion and reaction kinetics10.1177/154405910208100206 ↗
13. Effects of composition and reactivity on the reaction kinetics of dimethacrylate/dimethacrylate copolymerizations10.1021/ma990258d ↗
14. Stansbury JW, Dickens SH, Unpublished results.
15. Effect of heat expansion and contraction on polymerization shrinkage measurement with mercury dilatometer
16. Polymer matrix effects on the properties of amorphous calcium phosphate-filled composites
17. Effect of the monomer and filler systems on the remineralizing potential of bioactive dental composites based on amorphous calcium phosphate10.1002/pat.119 ↗
18. Polymerization shrinkage and elasticity of flowable composites and filled adhesives10.1016/S0109-5641(99)00022-6 ↗
19. Effect of stepped light exposure on the volumetric polymerization shrinkage and bulk modulus of dental composites and an unfilled resin