Reliability performance of titanium sputter coated Ni–Ti arch wires: Mechanical performance and nickel release evaluation
Source abstract
Abstract
The present research was aimed at developing surface coatings on NiTi archwires capable of protection against nickel release and to investigate the stability, mechanical performance and prevention of nickel release of titanium sputter coated NiTi arch wires. Coated and uncoated specimens immersed in artificial saliva were subjected to critical evaluation of parameters such as surface analysis, mechanical testing, element release, friction coefficient and adhesion of the coating. Titanium coatings exhibited high reliability on exposure even for a prolonged period of 30 days in artificial saliva. The coatings were found to be relatively stable on linear scratch test with reduced frictional coefficient compared to uncoated samples. Titanium sputtering adhered well with the Ni-Ti substrates at the molecular level, this was further confirmed by Inductive coupled plasma emission spectroscopy (ICPE) analysis which showed no dissolution of nickel in the artificial saliva. Titanium sputter coatings seem to be promising for nickel sensitive patients. The study confirmed the superior nature of the coating, evident as reduced surface roughness, friction coefficient, good adhesion and minimal hardness and elastic modulus variations in artificial saliva over a given time period.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Mechanical stress and fatigue analysis · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Orthodontics, Sree Anjaneya Institute of Dental Sciences, Calicut, India
Department of Orthodontics, Amrita School of Dentistry, Kochi, India
Technocommercial Innovation Center, English Indian Clay limited, Trivandrum, India
References (28)
Show source-provided references
1. Inhibition of Ni release from NiTi alloy by hydroxyapatite, alumina, and titanium sputtered coatings
2. The effect of short-term temperature changes on superelastic nickel–titanium archwires activated in orthodontic bending10.1067/mod.2001.112451 ↗
3. Load-deflection characteristics of superelastic nickel–titanium wires10.2319/101206-423.1 ↗
4. The super-elastic property of Japanese NiTi alloy wire for use in orthodontics10.1016/0889-5406(86)90021-1 ↗
5. Force levels of nickel titanium initial archwires
6. Allergic contact dermatitis associated with the use of Interlandi headgear in a patient with a history of atopy10.1038/sj.bdj.4808226 ↗
7. Nickel allergy in adolescents in relation to orthodontic treatment and piercing of ears10.1016/S0889-5406(96)70175-0 ↗
8. Establishment of nickel-specific T cell lines from patients with allergic contact dermatitis: Comparison of three different protocols10.1006/clin.1994.1180 ↗
9. T-lymphocyte and Langerhans cell distribution in normal and allergically-induced oral mucosa in contact with nickel-containing dental alloys10.1111/j.1600-0714.1988.tb01899.x ↗
10. Nickel allergy and orthodontics10.1093/ortho/30.2.171 ↗
11. Ex vivo surface and mechanical properties of coated orthodontic archwires10.1093/ejo/cjn057 ↗
12. Corrosion behaviour of ultra fine grained titanium in simulated body fluid for implant application
13. Deterioration in the superelasticity of Ti sputter coated on NiTi orthodontic wire
14. [14]J.-H. Park, Chemical Vapor Deposition, 1st edn, ASM International, 2001.
15. The anticorrosion ability of titanium nitride (TiN) plating on an orthodontic metal bracket and its biocompatibility10.1002/jbm.10484 ↗
16. The release of nickel from orthodontic NiTi wires is increased by dynamic mechanical loading but not constrained by surface nitridation10.1002/jbm.a.31097 ↗
17. Corrosion of stainless steel, nickel–titanium, coated nickel–titanium, and titanium orthodontic wires
18. Development and evaluation of two PVD-coated b-titanium orthodontic archwires for fluoride-induced corrosion protection10.1016/j.actbio.2010.11.026 ↗
19. Laboratory test simulation of aluminium cold forming – Influence from PVD tool coatings on the tendency to galling10.1016/j.surfcoat.2010.04.025 ↗
20. Influence of surface topography of arc-deposited TiN and sputter-deposited WC/C coatings on the initial material transfer tendency and friction characteristics under dry sliding contact conditions10.1016/j.surfcoat.2008.12.011 ↗
21. [21]C.S. Solanki, Solar Photovoltaics: Fundamentals, Technologies and Applications, 2nd edn, PHI Learning Pvt. Ltd, New Delhi, 2009.
22. Artificial salivas for in vitro studies of dental materials10.1016/S0300-5712(96)00068-1 ↗
23. Tan · Biomaterials · 2003 · 24 · 393110.1016/S0142-9612(03)00271-0 ↗
24. Corrosion of orthodontic wires
25. Static frictional force and surface roughness of nickel–titanium arch wires10.1016/0889-5406(91)70072-5 ↗
26. Comparisons of nanoindentation, 3-point bending, and tension tests for orthodontic wires10.1016/j.ajodo.2009.11.015 ↗
27. Particle growth in a sputtering discharge10.1116/1.581951 ↗
28. Effect of loading force on the dissolution behavior and surface properties of nickel–titanium orthodontic archwires in artificial saliva10.1016/j.ajodo.2010.03.031 ↗