An Optimal Thermo-Hydro-Mechanical Densification (THM) Process for Densifying Balsam Fir Wood

Ling Li, Meng Gong, Naxin Yuan, Dagang Li

BioResources· Volume 8· Issue 3

Abstract

To better utilize low-density softwood, a thermo-hydro-mechanical densification process performed in an open system was studied to enable the manufacture of densified wood with a hard surface, strong bonding, and good dimensional stability. This study was aimed at optimizing three densification parameters, i.e., compression ratio (CR), temperature, and time, for balsam fir (Abies balsamea (L.) Mill.). The Brinell surface hardness, bond strength, and thickness recovery ratio of densified fir were examined. It was found that the optimal densification parameters were a CR of 60%, a temperature of 230 ºC, and a time of 20 minutes. The surface hardness and bond strength of optimized densified fir were about 30 and 8 MPa, respectively. The thickness recovery ratio of the densified fir after a 2-hour cold water soaking and another 2-hour boiling treatment was about 10%. Because the densified fir in this study was used for indoor applications only, its thickness recovery ratio could be minimal under conditions of use.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Forest ecology and management · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.