The combined effect of porosity and reactivity of the carbon preforms on the properties of SiC produced by reactive infiltration with liquid Si
Source abstract
Abstract
This study is focused on the effect of the porosity and chemical reactivity with silicon of the carbon preforms on the properties of SiC pieces produced by reactive infiltration. Petroleum residues were selected as carbon precursor because of their unique combination of properties. On the one hand, semicoke powders with optimum self-sinterability can be obtained from them to develop a wide range of porous carbon preforms without addition of binder to carry out the porosity study. On the other hand, reactivity of the carbon material with silicon can be modified by employing semicokes with different mesophase microstructure obtained from petroleum residues with different chemical composition. SiC yield was strongly affected by the degree of anisotropy of the carbon material, the most ordered carbon being more reactive. SiC pieces made from the optimum carbon preforms (made up by combining the most graphitic carbon and 40% of open porosity) achieved bending strength values of around 260 MPa. Chemical reactivity of carbon substrates was also modified by graphitization treatment. An improvement in the mechanical properties of SiC pieces up to 66% was achieved due to the structural modification caused by graphitization of the carbon preforms. Bending strengths twice the value of commercially available ones were achieved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Microstructural evolution in reaction-bonded silicon-carbide10.1007/BF00553278 ↗
2. The preparation of dense self-bonded silicon carbide
3. Hucke EE. Composite bodies comprising a continuous framework and an impregnated metallic material and methods for their production. Patent US Patent 3,235,346; 1966.
4. Reaction-formed silicon carbide10.1016/0921-5093(91)90210-E ↗
5. Reaction-bonded silicon carbide by reactive infiltration10.1021/ie001029e ↗
6. Reaction-infiltrated, net-shape Sic composites10.1016/0921-5093(94)06512-8 ↗
7. Reactive-infiltration processing of SiC–metal and SiC–intermetallic composites10.1557/JMR.1996.0298 ↗
8. Fabrication and characterization of some novel reaction-bonded silicon-carbide materials10.1007/BF02403904 ↗
9. Bormann R, Mazzone G, Shull RD, Averback RS, Ziolo RF, editors. Processing and mechanical properties of SiC–metal interpenetrating composites. 95 November 27, Massachusetts Inst of Technology, Cambridge, United States. Boston, MA, USA: Materials Research Society; 1996.
10. Liquid-phase reaction-bonding of silicon-carbide using alloyed silicon molybdenum melts10.1111/j.1151-2916.1990.tb05179.x ↗
11. Reactive infiltration of silicon melt through microporous amorphous carbon preforms10.1007/s11663-999-0099-1 ↗
12. Microstructure and mechanical properties of reaction-formed silicon carbide (RFSC) ceramics10.1016/0921-5093(94)90346-8 ↗
13. Reactive melt infiltration of silicon–niobium alloys in microporous carbons10.1557/JMR.1994.1701 ↗
14. Reactive melt infiltration of silicon–molybdenum alloys into microporous carbon preforms10.1016/0921-5093(94)09663-5 ↗
15. Morphological characterization of microporous carbon materials10.1023/A:1018512910724 ↗
16. The effect of porous carbon preform and the infiltration process on the properties of reaction-formed SiC10.1016/j.carbon.2004.03.018 ↗
17. Influence of the carbon material on the synthesis of silicon carbide10.1016/S0008-6223(99)00045-7 ↗
18. Self-sintering of carbon mesophase powders: effect of extraction/washing with solvents10.1016/S0008-6223(99)00169-4 ↗
19. Chemistry of carbonization10.1016/0008-6223(82)90089-6 ↗
20. Semicokes from pitch pyrolysis: mechanisms and kinetics10.1016/S0008-6223(98)00205-X ↗
21. Marsh · 1997
22. Mochida · 1994
23. Pyrolysis of petroleum residues: I. Yields and product analyses10.1016/S0008-6223(99)00028-7 ↗
24. Influence of pressure variations on the formation and development of mesophase in a petroleum residue10.1016/S0008-6223(98)00211-5 ↗
25. Modification of the sintering behaviour of mesophase powder from a petroleum residue10.1016/S0008-6223(02)00205-1 ↗
26. Pyrolysis of petroleum residues: analysis of semicokes by X-ray diffraction10.1016/S0008-6223(99)00085-8 ↗
27. Pyrolysis of petroleum residues III. Kinetics of pyrolysis10.1016/S0008-6223(00)00073-7 ↗
28. Pyrolysis of petroleum residues II. Chemistry of pyrolysis10.1016/S0008-6223(99)00133-5 ↗
29. Sintering of powders of polyaromatic mesophase to high-strength isotropic carbons – I. Influence of the raw material and sintering conditions on the properties of the carbon materials10.1016/0008-6223(94)90218-6 ↗
30. Carbon disc of high density and strength prepared from synthetic pitch-derived mesocarbon microbeads10.1016/S0008-6223(98)00298-X ↗
31. Carbonization and graphitization10.1016/0008-6223(84)90086-1 ↗
32. High temperature load-deflection behaviour of reaction bonded SiC (RBSC)10.1016/S0272-8842(00)00120-6 ↗
33. Fabrication of functionally graded reaction infiltrated SiC–Si composite by three-dimensional printing (3DP (TM)) process10.1016/S0921-5093(00)01282-X ↗
34. Mechanical behavior of biomorphic Si/SiC porous composites10.1016/j.scriptamat.2005.07.033 ↗
35. Microstructure and fracture properties of biomorphic SiC10.1016/j.ijrmhm.2005.07.003 ↗