journal article·2002

Sharp indentation behavior of carbon/carbon composites and varieties of carbon

Pascal Diss, Jacques Lamon, L Carpentier, J.L Loubet, Ph Kapsa

Carbon· Volume 40· Issue 14
Publisher page

Abstract

Abstract Sharp indentation tests on carbon fiber and carbon matrix composites (C/C composite) were carried out over a wide load range from 0 to 2 N on three different cross sections: normal, parallel and inclined to the fiber axis. For comparison purposes, a variety of carbons including HOPG, glassy C, and pyrocarbon films was also examined. Both the fibers and the matrices displayed first a purely elastic response and second crack-induced damage. A purely elastic behavior was also observed with most of the varieties of carbon considered. Young’s modulus was extracted from the indentation curves either at maximum or at various forces, using the Sneddon equation of elastic response on loading (elastic indentation) or a classical equation based on elastic recovery on unloading (elastoplastic indentation). Results are discussed with respect to features of structure and heterogeneity of material in the stressed volume.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Microindentations in metals
2. Indentation of brittle materials
3. Deformation and cracking during high temperature scratching of a glass10.1007/BF01033842 ↗
4. Micro/nanomechanical and tribological characterization of ultrathin amorphous carbon coatings10.1557/JMR.1999.0309 ↗
5. Umemura · Phil Mag A · 1996 · 74 · 114310.1080/01418619608239715 ↗
6. Nanoindentation and scratch resistance testing on magnetic tape heads coated with ultra-thin amorphous carbon layers10.1016/S0043-1648(00)00439-7 ↗
7. The indentation characterization of the mechanical properties of various carbon materials: glassy carbon, coke and pyrolytic carbon10.1016/S0008-6223(96)00071-1 ↗
8. Nanoindentation behavior of a two-dimensional carbon–carbon composite for nuclear applications10.1016/S0008-6223(97)00042-0 ↗
9. Nanoindentation of diamond, graphite and fullerene films10.1016/S0925-9635(00)00188-6 ↗
10. Hofmann · 1997
11. Indentation-induced contact deformation and damage of glasslike carbon10.1111/j.1151-2916.1995.tb08429.x ↗
12. Physical properties of superhard and ultrahard fullerites treated from solid C60 by high-pressure–high temperature treatment10.1007/s003390050474 ↗
13. Mechanical properties of carbon–carbon composite components determined using nanoindentation10.1016/S0008-6223(98)00239-5 ↗
14. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
15. Vickers indentation curves on elastoplastic materials
16. Pulse chemical vapor deposition and infiltration of pyrocarbon in model pores with rectangular cross-sections. Part 1–Study of the pulsed process of deposition10.1007/BF00975086 ↗
17. McClintock · 1966
18. The relation between load and penetration in the axisymmetric Bousssinesq problem for a punch of arbitrary profile10.1016/0020-7225(65)90019-4 ↗
19. Influence of substrate on the elastic reaction of films for the microindentation test
20. Effect of soft substrate on the indentation damage in silicon carbide deposited on graphite10.1023/A:1004778614890 ↗
21. Determination of elastic modulus of thin layers using nanoindentation10.1557/JMR.1997.0327 ↗
22. Modelling of the stress/strain behavior of a carbon/carbon composite with a 2.5 dimensional fibre architecture under tensile and shear loads at room temperature10.1016/S0266-3538(97)00241-8 ↗
23. Effect of fibre microstructure upon the modulus of PAN-pitch-based carbon fibers10.1016/0008-6223(94)00109-D ↗
24. Tensile deformation of carbon fibers and the relationship with the modulus for shear between the basal planes10.1016/0008-6223(91)90046-L ↗
25. The relationship between preferred orientation and Young’s modulus of carbon fibers
26. Ceramic reinforcements