journal article·2021-10

Synergetic enhancement of strength and ductility for titanium-based composites reinforced with nickel metallized multi-walled carbon nanotubes

L.L. Dong, W. Zhang, Y.Q. Fu, J.W. Lu, Y. Liu, Y.S. Zhang

Carbon· Volume 184
Publisher page

Abstract

Poor ductility of titanium matrix composites with medium/high-strength reinforced with carbonaceous nanomaterials (eg., graphene, carbon nanotubes etc.), has seriously restricted their wide-range engineering and practical industry utility. Herein, we propose a new methodology to significantly and simultaneously enhance both ductility and tensile strength of the titanium matrix composites. We ball milled Ti-6Al-4V (TC4) powders with in-situ chemically synthetized Ni decorated multi-walled carbon nanotubes (i.e MWCNTs@Ni), and then sintered the composites powders using spark plasma sintering (SPS). We achieved both a significant balanced between superior strength and increased ductility of the composite using the MWCNTs@Ni nanopowders. The enhanced strength in composites is mainly attributed to the interfacial structures for effectively enhanced load transfer capability between MWCNTs@Ni and Ti matrix, e.g., the formation of coherent/semi-coherent interfaces among interfacial phases Ti2Ni, TiC and Ti matrix. Furthermore, we applied the dislocation theory to reveal the toughening mechanisms of MWCNTs@Ni in the MWCNTs@Ni/TC4 composites. This study provides a new methodology of fabricating metal matrix composites (reinforced with carbon based nanomaterial) with both high strength and good ductility.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (84)

Show source-provided references
1. 1982
2. Room temperature tensile fracture characteristics of in situ TiBw/Ti6Al4V composites with a quasi-continuous network architecture10.1016/j.scriptamat.2011.01.011 ↗
3. Mechanical property and microstructure evolution of nitrogen-modified Ti-6Al-4V alloy with core-shell structure by hot compression10.1016/j.matchar.2018.05.051 ↗
4. Processing-structure-property aspects of particulate - and whisker-reinforced titanium matrix composites10.1016/j.compscitech.2007.07.016 ↗
5. Low volume fraction in situ (Ti5Si3+Ti2C)/Ti hybrid composites with network microstructure fabricated by reaction hot pressing of Ti–SiC system10.1016/j.compscitech.2013.03.025 ↗
6. In situ TiBw/Ti–6Al–4V composites with novel reinforcement architecture fabricated by reaction hot pressing10.1016/j.scriptamat.2009.02.032 ↗
7. Microstructure and mechanical property evolutions of bulk core-shell structured Ti-N alloys during annealing10.1016/j.jallcom.2017.03.254 ↗
8. Microstructure, mechanical and wear properties of core-shell structural particle reinforced Ti-O alloys10.1016/j.vacuum.2017.02.006 ↗
9. Microstructure and mechanical properties of a high-oxygen core-shell network structured Ti6Al4V alloy10.1016/j.vacuum.2017.12.036 ↗
10. Transformation-induced plasticity and high strength in beta titanium alloy manufactured by selective laser melting10.1016/j.mtla.2019.100299 ↗
11. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
12. Microstructure and mechanical properties of selective laser melted Ti-3Al-8V-6Cr-4Zr-4Mo compared to Ti-6Al-4V10.1016/j.msea.2018.12.100 ↗
13. Effect of transition layer on the performance of hydroxyapatite/titanium nitride coating developed on Ti-6Al-4V alloy by magnetron sputtering10.1016/j.ceramint.2018.11.183 ↗
14. Strength distribution of Ti/SiC metal-matrix composites under monotonic loading10.1016/j.engfracmech.2018.03.015 ↗
15. Microstructure and mechanical properties of SiC nanowires reinforced titanium matrix composites10.1016/j.jallcom.2019.152953 ↗
16. High temperature tensile properties of in situ TiBw/Ti6Al4V composites with a novel network reinforcement architecture10.1016/j.msea.2011.12.028 ↗
17. High tensile-strength and ductile titanium matrix composites strengthened by TiB nanowires10.1016/j.scriptamat.2017.08.007 ↗
18. Microstructure and superior mechanical property of in situ (TiBw + TiCp)/Ti composites with laminated structure10.1016/j.ceramint.2020.12.269 ↗
19. Mechanical properties of Ti-6Al-4V/TiB composites with randomly oriented and aligned TiB reinforcements10.1016/S1359-6454(02)00510-4 ↗
20. Development of titanium boride (TiB) dispersed titanium (Ti) matrix composite by direct laser cladding10.1016/j.matlet.2009.12.007 ↗
21. Fabrication of TiCp/Ti–6Al–4V surface composite via friction stir processing (FSP): process optimization, particle dispersion-refinement behavior and hardening mechanism10.1016/j.msea.2013.03.019 ↗
22. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB+TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
23. Effect of TiB2 addition on the microstructure and wear resistance of Ti-6Al-4V alloy fabricated through direct metal laser sintering (DMLS)10.1016/j.jallcom.2018.10.308 ↗
24. Sintering effect on microstructural evolution and mechanical properties of spark plasma sintered Ti matrix composites reinforced by reduced graphene oxides10.1016/j.ceramint.2018.06.252 ↗
25. Carbonaceous nanomaterial reinforced Ti-6Al-4V matrix composites: properties, interfacial structures and strengthening mechanisms10.1016/j.carbon.2020.04.009 ↗
26. Tensile loading of ropes of single wall carbon nanotubes and their mechanical properties10.1103/PhysRevLett.84.5552 ↗
27. Thermal transport measurements of individual multiwalled nanotubes10.1103/PhysRevLett.87.215502 ↗
28. Strengthening in carbon nanotube/aluminium (CNT/Al) composites10.1016/j.scriptamat.2005.07.022 ↗
29. Microstructures and tensile behavior of carbon nanotube reinforced Cu matrix nanocomposites10.1016/j.msea.2006.04.085 ↗
30. MWCNTs/AZ31 surface composites fabricated by friction stir processing10.1016/j.msea.2006.01.016 ↗
31. Mechanical characteristics and preparation of carbon nanotube fiber-reinforced Ti composite10.1002/1527-2648(200007)2:7<416::AID-ADEM416>3.0.CO;2-Y ↗
32. Fabrication of carbon nanotube reinforced iron based magnetic alloy composites by spark plasma sintering10.1016/j.jallcom.2014.02.169 ↗
33. Interface analysis of ultra-high strength carbon nanotube/nickel composites processed by molecular level mixing10.1016/j.carbon.2013.01.075 ↗
34. Strengthening of copper matrix composites by nickel-coated single-walled carbon nanotube reinforcements10.1016/j.synthmet.2008.10.017 ↗
35. Ag/CNT nanocomposites and their single-and double-layer electromagnetic wave absorption properties10.1016/j.synthmet.2015.08.017 ↗
36. Interdependencies between graphitization of carbon nanotubes and strengthening mechanisms in titanium matrix composites10.1016/j.mtla.2018.08.015 ↗
37. Microstructure and mechanical properties of carbon nanotubes reinforced titanium matrix composites fabricated via spark plasma sintering10.1016/j.msea.2017.02.019 ↗
38. Improving the strengthening efficiency of carbon nanotubes in titanium metal matrix composites10.1016/j.msea.2017.04.026 ↗
39. Rapid and low temperature spark plasma sintering synthesis of novel carbon nanotube reinforced titanium matrix composites10.1016/j.carbon.2015.08.061 ↗
40. Metallurgical challenges in carbon nanotube-reinforced metal matrix nanocomposites10.3390/met7100384 ↗
41. Pulsed current field assisted surface modification of carbon nanotubes with nanocrystalline titanium carbide10.1016/j.carbon.2016.02.012 ↗
42. Direct observation of toughening mechanisms in carbon nanotube ceramic matrix composites10.1016/j.actamat.2003.10.050 ↗
43. Agarwal · 2010
44. Powder metallurgy titanium metal matrix composites reinforced with carbon nanotubes and graphite10.1016/j.compositesa.2012.12.005 ↗
45. In-situ CVD synthesis of Ni@N-CNTs/carbon paper electrode forelectro-reduction of CO210.1016/j.carbon.2020.10.044 ↗
46. TLP bonding of Ti-6Al-4V and Mg-AZ31 alloys using pure Ni electro-deposited coats10.1016/j.jmatprotec.2014.07.028 ↗
47. The effect of a small addition of boron on the sintering densification, microstructure and mechanical properties of powder metallurgy Ti–7Ni alloy10.1016/j.jallcom.2012.12.068 ↗
48. A comparison of Ti–Ni and Ti-Sn binary alloys processed using powder metallurgy10.1016/j.msea.2015.07.085 ↗
49. Suitability of nickel as alloying element in titanium sintered in solid state10.1179/003258908X336391 ↗
50. Effect of nickel addition on densification, microstructure and wear behaviour of spark plasma sintered CP-titanium10.1016/j.matchemphys.2019.122130 ↗
51. Synthesis, microstructural and phase evolution in Ti–2Ni and Ti–10Ni binary alloys consolidated by spark plasma sintering technique10.1007/s00170-019-03950-5 ↗
52. Microstructure and tribological properties of titanium matrix nanocomposites through powder metallurgy using graphene oxide nanosheets enhanced copper powders and spark plasma sintering10.1016/j.jallcom.2021.159093 ↗
53. Identifying and understanding the effect of milling energy on the synthesis of carbon nanotubes reinforced titanium metal matrix composites10.1016/j.carbon.2015.12.041 ↗
54. Effect of dispersion method on the deterioration, interfacial interactions and re-agglomeration of carbon nanotubes in titanium metal matrix composites10.1016/j.matdes.2015.08.112 ↗
55. Interdependencies between graphitization of carbon nanotubes and strengthening mechanisms in titanium matrix composites10.1016/j.mtla.2018.08.015 ↗
56. Y. Zhou, L.L. Dong, Q.H. Yang, W.T. Huo, Y.Q. Fu, Y.J. Shi, Y. Liu, Y.S. Zhang. Controlled interfacial reactions and superior mechanical properties of high energy ball milled/spark plasma sintered Ti-6Al-4V-graphene composite. Adv. Eng. Mater. 2021, 2001411.10.1002/adem.202001411 ↗
57. Role of process control agent in the synthesis of multi-walled carbon nanotubes reinforced titanium metal matrix powder mixtures10.1002/adem.201500346 ↗
58. Electronic structure of Ti–Ni alloys: an XPS and NEXAFS study10.1016/j.jallcom.2012.05.059 ↗
59. Formation of intermetallic phase in Ni/Ti multilayer structure by ion implantation and thermal annealing10.1016/j.intermet.2012.02.007 ↗
60. Graphene defect engineering for optimizing the interface and mechanical properties of graphene/copper composites10.1016/j.carbon.2018.08.004 ↗
61. Interface and mechanical/thermal properties of graphene/copper composite with Mo2C nanoparticles grown on graphene10.1016/j.compositesa.2018.03.014 ↗
62. Formation of TiCx during reactive spark plasma sintering of mechanically milled Ti/carbon nanotube mixtures10.1016/j.jallcom.2017.03.216 ↗
63. Effects of first-scale TiBw on secondary-scale Ti5Si3 characteristics and mechanical properties of in-situ (Ti5Si3+TiBw)/Ti6Al4V composites10.1016/j.jallcom.2017.02.044 ↗
64. Microstructure and mechanical properties of in situ synthesised (TiC+TiB)/Ti-6Al-4V composites prepared by powder metallurgy10.1179/174328409X421988 ↗
65. Fabrication and characterisation of titanium matrix composites obtained using a combination of self propagating high temperature synthesis and spark plasma sintering10.1016/j.msea.2015.12.050 ↗
66. Synthesis and mechanical properties of TiAl particle reinforced Ti-6Al-4V10.1016/j.msea.2016.08.011 ↗
67. In situ (TiBw + TiCp)/Ti6Al4V composites with a network reinforcement distribution10.1016/j.msea.2010.07.025 ↗
68. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
69. In situ synthesis of (TiC+Ti3SiC2+Ti5Si3)/Ti6Al4V composites with tailored two-scale architecture10.1002/adem.201400585 ↗
70. Interface engineering of graphene/copper matrix composites decorated with tungsten carbide for enhanced physico-mechanical properties10.1016/j.carbon.2020.10.091 ↗
71. Solid-state interfacial reaction and load transfer efficiency in carbon nanotubes (CNTs)-reinforced aluminum matrix composites10.1016/j.carbon.2016.12.013 ↗
72. Strengthening mechanisms in carbon nanotube-reinforced aluminum composites10.1016/j.carbon.2015.08.112 ↗
73. Interface and mechanical/thermal properties of graphene/copper composite with Mo2C nanoparticles grown on graphene10.1016/j.compositesa.2018.03.014 ↗
74. Uniform dispersion and interface analysis of nickel coated graphene nanoflakes/pure titanium matrix composites10.1016/j.carbon.2018.05.013 ↗
75. Solid-state interfacial reaction and load transfer efficiency in carbon nanotubes (CNTs)-reinforced aluminum matrix composites10.1016/j.carbon.2016.12.013 ↗
76. Powder metallurgy Ti–TiC metal matrix composites prepared by in situ reactive processing of Ti-VGCFs system10.1016/j.carbon.2013.04.088 ↗
77. Interface structure and strengthening behavior of graphene/CuCr composites10.1016/j.carbon.2018.03.018 ↗
78. Titanium/nanodiamond nanocomposites: effect of nanodiamond on microstructure and mechanical properties of titanium10.1016/j.matdes.2017.06.015 ↗
79. Nanodiamonds reinforced titanium matrix nanocomposites with network architecture10.1016/j.compositesb.2018.11.110 ↗
80. Improvement of interfacial interaction and mechanical properties in copper matrix composites reinforced with copper coated carbon nanotubes10.1016/j.msea.2018.01.005 ↗
81. Enhanced tensile plasticity in ultrafine-grained metallic composite fabricated by friction stir process10.1016/j.scriptamat.2008.06.040 ↗
82. Deformation behavior of aluminum alloy matrix composites reinforced with few-layer graphene10.1016/j.compositesa.2015.08.001 ↗
83. Simultaneously enhancing the strength, ductility and conductivity of copper matrix composites with graphene nanoribbons10.1016/j.carbon.2017.03.055 ↗
84. Simultaneously enhancing strength and ductility of carbon nanotube/aluminum composites by improving bonding conditions10.1016/j.scriptamat.2015.11.011 ↗