Dependence of pyrocarbon microstructure on the substrate and annealing during the initial stage of chemical vapor deposition
Source abstract
Abstract
Electron microscopic and electron spectroscopic techniques were applied to study interface properties, microstructure and texture of pyrolytic carbon obtained after short-time chemical vapor deposition (CVD) on planar Si substrates. The pyrolytic carbon was obtained in a hot-wall reactor from methane at a total pressure of 20 kPa and temperature of 1100 °C. Only short depositions between 2.5 and 240 min were performed. The carbon deposition starts with the nucleation of isolated islands. The increase of residence and deposition time leads to the formation of a continuous layer by larger island sizes and higher island densities, a transition from rough to smooth surfaces and formation of pores on smooth surfaces. An increased deposition rate during the first 15 min is observed which is correlated with a granular morphology of the carbon layer. Using BN-covered Si wafers with a surface roughness on a 100 nm scale reduces the texture degree in the vicinity of the interface and strengthens adhesion of the pyrolytic carbon compared to the smooth Si substrate. The texture of high-textured pyrolytic carbon is improved significantly by annealing at 1100 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research · Chemical and Physical Properties of Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Pyrocarbons (Review)10.1016/S0008-6223(01)00138-5 ↗
2. Chemical vapor deposition and infiltration processes of carbon materials (Review)10.1016/S0008-6223(01)00195-6 ↗
3. Consideration of reaction mechanisms leading to pyrolytic carbon of different textures10.1016/S0008-6223(02)00174-4 ↗
4. Influence of pressure, temperature and surface area/volume ratio on the texture of pyrolytic carbon deposited from methane10.1016/S0008-6223(02)00403-7 ↗
5. Carbon–carbon composites prepared by a rapid densification process II: structural and textural characterizations
6. Structural properties of the fiber–matrix interface in carbon–fiber/carbon–matrix composites and interfaces between carbon layers and planar substrates10.1515/ijmr-2006-0165 ↗
7. Pyrocarbon deposits on a graphite surface observed by STM10.1002/1521-3862(200105)7:3<125::AID-CVDE125>3.0.CO;2-B ↗
8. Deposition rates during the early stages of pyrolytic carbon deposition in a hot-wall reactor and the development of texture10.1016/j.carbon.2006.03.017 ↗
9. Preparation of boron nitride thin films by microwave PECVD and their analytical characterization10.1039/b106220b ↗
10. On the terminology for pyrolytic carbon10.1016/S0008-6223(01)00282-2 ↗
11. Micro- and nanostructure of the carbon matrix of infiltrated carbon fiber felts10.1016/S0008-6223(00)00116-0 ↗
12. The preparation of cross-section specimens for transmission electron microscopy10.1002/jemt.1060010106 ↗
13. Pyrocarbon anisotropy as measured by electron diffraction and polarized light10.1557/JMR.2000.0017 ↗
14. Atomic scale strain measurements by the digital analysis of transmission electron microscopic lattice images
15. 1994 · vol. 71
16. ELNES across interlayers in SiC (Nicalon) fibre-reinforced Duran glass10.1088/0022-3727/29/7/005 ↗
17. Deposition process of laminar pyrocarbon from propane
18. The effect of cooling rate on hydrogen release from a pyrolytic carbon coating and its resulting morphology10.1016/j.carbon.2005.12.014 ↗
19. Silicon carbide whiskers synthesized from SiO2–CH4–Na3AlF6 system10.1023/A:1004544701084 ↗
20. Low voltage electron diffraction study of the oxidation and reduction of silicon10.1063/1.1728901 ↗
21. Kinetics and mechanisms of low-pressure, high-temperature oxidation of silicon10.1007/BF00603483 ↗