Reversible Raman D-band changes: A new probe into the pressure-induced collapse of carbon nanotubes
Source abstract
Abstract
The control of the geometry of carbon nanotubes has a high potential for electro-optical technology develop- ments. We report here the use of a new spectroscopic signature for the detection and characterization of the pressure induced radial buckling of single walled carbon nanotubes using Raman spectroscopy combined with sapphire anvil cell pressure systems. We follow the appearance of a defect-free Raman D-band contribution in bundled samples which is assigned to the pressure-induced radial buckling, as already shown on radially collapsed nanotubes at ambient pressure. On pressure release, this contribution to the D-band disappears, confirming the reversibility of the process. We applied this approach to the study of isolated tubes and followed the collapse transition of a 1.7 nm diameter tube, most likely identified as a (16,8) chirality, starting at 1 GPa and ending at 2 GPa. Our study further illustrates the potential of utilizing the D-band as a new spectroscopic probe to explore geometrical changes in carbon nanotubes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Carbon Nanotubes in Composites · Diamond and Carbon-based Materials Research · Mechanical and Optical Resonators
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Universality of Moiré physics in collapsed chiral carbon nanotubes10.1016/j.carbon.2023.01.052 ↗
2. Effect of extreme mechanical densification on the electrical properties of carbon nanotube micro-yarns10.1088/1361-6528/ac6039 ↗
3. Intense Raman D band without disorder in flattened carbon nanotubes10.1021/acsnano.0c06048 ↗
4. Fabrication and characterization of fully flattened carbon nanotubes: A new graphene nanoribbon analogue10.1038/srep01617 ↗
5. Bandgap closure of a flattened semiconductor carbon nanotube: A first-principles study10.1063/1.126096 ↗
6. Gating individual nanotubes and crosses with scanning probes10.1063/1.125611 ↗
7. Hydrostatic pressure effects on the structural and electronic properties of carbon nanotubes10.1002/pssb.200405253 ↗
8. Collapse phase diagram of carbon nanotubes with arbitrary number of walls. Collapse modes and macroscopic analog10.1016/j.carbon.2021.03.031 ↗
9. Collapse of single-wall carbon nanotubes is diameter dependent10.1103/PhysRevLett.92.095501 ↗
10. Structural transformations of carbon nanotubes under hydrostatic pressure10.1021/nl051637p ↗
11. Transition states and minimum energy pathways for the collapse of carbon nanotubes
12. Pressure-induced collapse in double-walled carbon nanotubes: Chemical and mechanical screening effects10.1021/jp110675e ↗
13. Resonant Raman spectroscopy of single-wall carbon nanotubes under pressure10.1103/PhysRevB.72.035409 ↗
14. Raman signature to identify the structural transition of single-wall carbon nanotubes under high pressure10.1103/PhysRevB.78.205411 ↗
15. G-mode behaviour of closed ended single wall carbon nanotubes under pressure10.1002/pssb.200880503 ↗
16. Pressure-induced selectivity for probing inner tubes in double- and triple-walled carbon nanotubes: A resonance Raman study10.1021/jp4126045 ↗
17. Radial collapse of carbon nanotubes for conductivity optimized polymer composites10.1016/j.carbon.2016.05.004 ↗
18. Pressure-induced radial collapse in few-wall carbon nanotubes: A combined theoretical and experimental study10.1016/j.carbon.2017.09.044 ↗
19. From high pressure radial collapse to graphene ribbon formation in triple-wall carbon nanotubes10.1016/j.carbon.2018.09.076 ↗
20. Perspective: High pressure transformations in nanomaterials and opportunities in material design10.1063/1.5045563 ↗
21. High-pressure behavior of polyiodides confined into single-walled carbon nanotubes: A Raman study10.1103/PhysRevB.82.205403 ↗
22. Chirality-dependent mechanical response of empty and water-filled single-wall carbon nanotubes at high pressure10.1016/j.carbon.2015.08.032 ↗
23. Superior carbon nanotube stability by molecular filling:a single-chirality study at extreme pressures10.1016/j.carbon.2021.07.068 ↗
24. Defect characterization in graphene and carbon nanotubes using Raman spectroscopy10.1098/rsta.2010.0213 ↗
25. Disentangling contributions of point and line defects in the Raman spectra of graphene-related materials
26. Raman characterization of defects and dopants in graphene
27. Strain-induced D band observed in carbon nanotubes10.1007/s12274-012-0269-3 ↗
28. Hydrostatic limits of 11 pressure transmitting media10.1088/0022-3727/42/7/075413 ↗
29. Raman spectroscopy of carbon nanotubes10.1016/j.physrep.2004.10.006 ↗
30. High pressure–high temperature synthesis of diamond from single-wall pristine and iodine doped carbon nanotube bundles10.1016/j.carbon.2009.02.014 ↗
31. From mesoscale to nanoscale mechanics in single-wall carbon nanotubes10.1016/j.carbon.2017.07.036 ↗
32. Dielectric constant model for environmental effects on the exciton energies of single wall carbon nanotubes10.1063/1.3485293 ↗
33. Structural and phonon properties of bundled single- and double-wall carbon nanotubes under pressure10.1021/jp3093176 ↗