journal article·2010-08

Effects of thermal and thermomechanical induced mechanical changes of C/C composites

Lotta Gaab, Dietmar Koch, Georg Grathwohl

Carbon· Volume 48· Issue 10
Publisher page

Abstract

Carbon fiber reinforced carbon composites are produced by modified chemical vapor infiltration (CVI) of a textile fiber preform. The modified process called rapid CVI (r-CVI) allows a fast production of the matrix as well as the adjustment of graphene orientation of the matrix. At a processing temperature of 1200 °C graphene stacks are produced which are oriented roughly in fiber orientation. Mechanical testing at different temperatures as well as after temperature treatment and optional surface siliconization was carried out on C/C. Thermal treatment leads to growth and realignment of the graphene stacks in the matrix resulting in an intensified anisotropy of the composite. High temperature tests beyond processing temperature on C/C lead to mechanically induced straightening of graphene stacks in loading direction. The improved orientation of the graphene structure which is proven by XRD measurements leads to higher loading capacity and therefore to better mechanical properties in 0/90° fiber direction and to reduced mechanical performance in ±70° fiber orientation. This effect is also shown in transverse tensile tests when the graphene layers in the matrix are loaded perpendicular to their orientation. Furthermore a new method to microstructural assessment is presented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fiber-reinforced polymer composites · Advanced ceramic materials synthesis · Graphene research and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. The future of carbon–carbon composites10.1016/0008-6223(87)90116-3 ↗
2. The structure of carbon fibres
3. Savage · 1993
4. Fitzer · 1998
5. X-ray studies on preferred orientation of carbon fibres10.1063/1.1710176 ↗
6. Radiation-induced dimensional changes in pyrolytic carbons deposited in a fluidized bed10.1016/0008-6223(66)90057-1 ↗
7. Influence of heat treatment on microstructure and properties of highly textured pyrocarbons deposited during CVD at about 1100°C and above 2000°C10.1016/j.compscitech.2007.07.019 ↗
8. Influence of the matrix microstructure on the mechanical properties of CVI-infiltrated carbon fiber felts10.1016/j.carbon.2005.03.006 ↗
9. Some observations on stress graphitization in carbon–carbon composites10.1016/0008-6223(91)90033-F ↗
10. Mechanisms of orientation and graphitization of hard-carbon matrices in carbon–carbon composites10.1557/JMR.1992.2798 ↗
11. Stress graphitization of C/C composite reinforced by carbon nanofiber10.1016/j.carbon.2005.01.034 ↗
12. Effects of the interface on the graphitization of a carbon fiber/pyrolytic carbon composite10.1016/S0008-6223(02)00398-6 ↗
13. Luedenbach G. Charakterisierung des Festigkeitsverhaltens von C/C-Verbundwerkstoffen in Abhängigkeit von Behandlungs- und Prüftemperatur, doctoral thesis. RWTH Aachen University; 1997.
14. The tensile behavior of carbon fibers at high temperatures up to 2400°C10.1016/j.carbon.2003.11.020 ↗
15. The tensile properties of carbon matrices at temperatures up to 2200°C10.1016/j.carbon.2005.03.020 ↗
16. Thermomechanical properties of carbon fibres at high temperatures (up to 2000°C)10.1016/S0266-3538(01)00140-3 ↗
17. Tensile strength and deformation of a two-dimensional carbon–carbon composite at elevated temperatures10.1111/j.1151-2916.2003.tb03620.x ↗
18. Advanced composite materials for current and future propulsion and industrial applications10.4028/www.scientific.net/AST.50.174 ↗
19. Herstellung von Hochleistungsverbundwerkstoffen mit Hilfe des Rapid-CVI-Verfahrens
20. Thermophysical properties of carbon/carbon composites and physical mechanism of thermal expansion and thermal conductivity10.1016/j.carbon.2004.06.024 ↗
21. Morgan · 2005
22. Pyrocarbon anisotropy as measured by electron diffraction and polarized light10.1557/JMR.2000.0017 ↗
23. Hegermann R. 2009. Personal communication.
24. Ceramic fiber composites: experimental analysis and modeling of mechanical properties10.1016/j.compscitech.2007.06.029 ↗
25. Kinking of a crack out of an interface10.1115/1.3176078 ↗
26. Micro-indentation method for evaluation of fracture toughness and thermal residual stresses of SiC coating on carbon/carbon composite10.1163/156855103772658533 ↗