The effect of high temperature heat-treatment on the strength of C/C to C/C–SiC joints
Source abstract
Abstract
Joining of carbon fiber reinforced C–SiC dual matrix composite (denoted by C/C–SiC) is critical for its aeronautical and astronautical applications. Joining of C/C–SiC has been realized through a reaction joining process using boron-modified phenolic resin with micro-size B4C and nano-size SiO2 powder additives. The effect of the heat-treatment temperature on the retained strength of the joints, calculated by dividing the strength of the heat-treated joints by the strength of the joints before heat-treatment, was studied. The maximum retained strength of the joints is as high as 96.0% after the heat-treatment at 1200 °C for 30 min in vacuum, indicating good heat resistance of the joints. The thickness of the interlayer of the joint after the heat-treatment is about 18 μm and it is uniform and densified. There are no obvious cracks or pores at the interfaces. During the heat-treatment, carbon, oxygen, silicon, and boron diffuse at the interfacial area. The interlayer is composed of B4C, SiO2, glassy carbon, amorphous B2O3, and borosilicate glass. SiC appears in the interlayer of the joint heat-treated at 1400 °C for 30 min in vacuum. The addition of B4C and SiO2 powders contributes to the densification of the interlayer, the bonding at the interfaces and the heat resistance of the joints.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Joining of partially sintered alumina to alumina, titanium, hastealloy and C–SiC composite using Ag–Cu brazes10.1016/j.jeurceramsoc.2007.06.017 ↗
2. Comparison of braze and solder materials for joining titanium to composites
3. Joining of SiC based ceramics and composites with Si–16Ti and Si–18Cr eutectic alloys10.1504/IJMPT.2004.004778 ↗
4. Diffusion bonding of silicon carbide ceramics using titanium interlayers10.1002/9780470291313.ch13 ↗
5. Effects of carbon fiber orientation and graphitization on solid state bonding of C/C composite to nickel10.2320/matertrans.44.148 ↗
6. Joining of carbon–carbon composites using boron and titanium disilicide interlayers10.1111/j.1151-2916.1997.tb02800.x ↗
7. Interdiffusion involved in SHS welding of SiC ceramic to itself and to Ni-based superalloy10.1016/S0263-4368(00)00008-1 ↗
8. Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications10.1016/S0022-3115(99)00268-8 ↗
9. Green state joining of SiC without applied pressure10.1111/j.1151-2916.2001.tb01039.x ↗
10. Development and testing of anticorrosive SiO2/phenolic–formaldehydic resin coatings10.1016/j.surfcoat.2006.01.070 ↗
11. Synthesis and characterization of boron-doped carbons10.1016/0008-6223(94)00160-2 ↗
12. LPCVD and characterization of boron-containing pyrocarbon materials10.1016/0008-6223(96)00075-9 ↗
13. The microstructural changes of carbon fiber pores in carbon–carbon composites during pyrolysis10.1016/S0266-3538(03)00165-9 ↗
14. Formation and oxidation resistance of the coating formed on carbon material composed of B4C–SiC powders10.1016/0008-6223(94)00164-U ↗
15. Investigations of low-energy ion irradiation influence on glassy polymeric carbon
16. Glassy carbon particles as component to modification of tribological properties10.1016/j.jmatprotec.2005.04.054 ↗
17. Study on the structural evolution of modified phenol–formaldehyde resin adhesive for the high-temperature bonding of graphite10.1016/j.jnucmat.2005.09.008 ↗
18. The Effects of boron additives on the oxidation behavior of carbons10.1016/0008-6223(84)90083-6 ↗
19. Manufacture and characterisation of a low cost carbon fibre reinforced C/SiC dual matrix composite10.1016/j.carbon.2006.01.025 ↗
20. The high-temperatures bonding of graphite/ceramics by organ resin matrix adhesive10.1016/j.ijadhadh.2005.07.005 ↗