Abstract This paper describes the development of tough, high reliability sintered carbon materials by the incorporation of graphite flakes into a sintered mesophase-based carbon matrix, a kind of carbon–carbon composite. The bending strengths are lower than those of the matrix alone because of the presence of misaligned flakes at the surface. However, multiple fracture and high work of fracture can be obtained depending upon the size, volume fraction and orientation of the graphite flakes. The fracture toughness is increased by factors of 2–3, due to energy dissipating mechanisms such as crack deflection, crack bridging and pull-out, all caused by the presence of the flakes in the composite. The reliability of the composites in terms of Weibull modulus is also increased by a factor of 2–3, because the defect population is effectively controlled by the flakes, which are mostly un-bonded to the matrix. A qualitative model is proposed to account for the correlation between failure probability, strength and microstructure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fiber-reinforced polymer composites · Advanced ceramic materials synthesis · Mechanical Behavior of Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Fracture in polycrystalline graphite
2. High strength, sintered carbons and graphites
3. Disclination structures in the carbonaceous mesophase10.1016/B978-0-12-025005-9.50011-4 ↗
4. A mechanism for the control of crack propagation in all-brittle materials
5. Preparation and piezoelectric response of PZT ceramics with anisotropic pores
6. Structured micro voids in ceramic PZT
7. Rice RW, Kahn M, Shadwell DE. Ceramic body with ordered pores. US Patent 4, 683,161, July 28, 1987.
8. Rutt T, Stynes JU. Ceramic matrices for electronic devices and process for forming same. US Patent 4353957, Oct. 12, 1982.
9. A simple way to make tough ceramics10.1038/347455a0 ↗
10. Enhanced crack-bridging by unbonded inclusions in a brittle matrix10.1016/S0955-2219(01)00242-4 ↗
11. Graphite flake carbon composites with a ‘sinterable’ microbead matrix – I. Mechanical properties10.1016/S0008-6223(03)00113-1 ↗
12. A bending method for direct measurement of fracture surface energy of brittle materials10.1143/JJAP.3.422 ↗
13. The work of fracture and its measurement in metals, ceramics and other materials10.1007/BF00550177 ↗
14. The dependence of strength-controlling fracture energy on the flaw size to grain size ratio10.1111/j.1151-2916.1980.tb10676.x ↗
15. A statistical theory of fracture