journal article·2014-08

Evaluation of a method for treatment of iron gall ink corrosion on paper

Jasna Malešič, Martin Šala, Vid Simon Šelih, Drago Kočar

Cellulose· Volume 21· Issue 4
Publisher page

Abstract

Iron gall ink was the most widely used writing ink for paper from the Middle Ages to the twentieth century. Unfortunately, the ink ingredients contain corrosive transition metal ions and acids that cause severe damage to the paper carrier. New or improved paper conservation methods for iron gall ink stabilization are constantly sought. The aim of the study was evaluation of a recently proposed stabilization treatment, adapted to lower relative humidity, applied to various model and historical paper samples containing iron gall ink. The effect of stabilization treatment on paper samples during artificial thermal aging was followed by the determination of the molecular weight distribution by size exclusion chromatography and colorimetry. Migration of iron and copper compounds from the ink lines was monitored by laser ablation inductively coupled plasma mass spectrometry. The results demonstrate that effective stabilization of iron gall ink-containing paper can be successfully achieved by interleaving with papers impregnated with the antioxidant tetrabutylammonium bromide and alkaline buffer under experimental conditions. Negative side effects of the stabilization treatment, such as migration of iron or copper ions from the ink lines and changes of color after the treatment and after accelerated thermal degradation, were limited, proving that the proposed stabilization treatment can be considered for future use by conservators.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Cultural Heritage Materials Analysis · Conservation Techniques and Studies · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Baty JW, Maitland CL, Minter W, Hubbe MA, Jordan-Mowery SK (2010) Deacidification for the conservation and preservation of paper-based works: a review. Bio Res 5:1955–2023
2. Ekenstam A (1936) Behavior of cellulose in solutions of mineral acids. Part II: a Kinetic study of cellulose degradation in acid solutions. Ber 69:553–55910.1002/cber.19360690315 ↗
3. Eusman E (1998) Iron gall ink—ingredients The Iron Gall Ink Website. http://ink-corrosion.org/igi_indexee73.html . Accessed 13 Nov 2013
4. Eusman E, Mensch K (2000) Washing and Humidifying Iron Gall Ink on paper: effects on iron migration. In: The book and paper group annual. http://cool.conservation-us.org/coolaic/sg/bpg/annual/v19/bp19-09.html . Accessed 13 Nov 2013
5. Henniges U, Reibke R, Banik G, Huhsmann E, Hahner U, Prohaska T, Potthast A (2008) Iron gall ink-induced corrosion of cellulose: aging, degradation and stabilization. Part 2: application on historic sample material. Cellul 15:861–87010.1007/s10570-008-9238-0 ↗
6. Kanngießer B, Hahn O, Wilke M, Nekat B, Malzer W, Erko A (2004) Investigation of oxidation and migration processes of inorganic compounds in ink-corroded manuscripts. Spechim Acta Part B At Spectrosc 59:1511–151610.1016/j.sab.2004.07.013 ↗
7. Kolar J (1997) Mechanism of autoxidative degradation of cellulose. Restaurator 18:163–17610.1515/rest.1997.18.4.163 ↗
8. Kolar J, Strlič M (2004) Evaluating the effects of treatments on iron gall ink corroded documents. Restaurator 25:94–10310.1515/REST.2004.94 ↗
9. Kolar J, Strlič M (2006) Ageing and stabilisation of paper contatining iron gall ink. In: Kolar J, Strlič M (ed) Iron gall inks: on manufacture, characterisation, degradation and stabilisation. National and university library, Ljubljana, pp 181–194
10. Kolar J, Strlič M, Budnar M, Malešič J, Šelih VS, Simčič J (2003) Stabilisation of corrosive iron gall inks. Acta Chim Slov 50:763–770
11. Kolar J, Možir A, Balažic A, Strlič M, Ceres G, Conte V, Miruzzo V, Steemers T, de Bruin G (2008) New antioxidants for treatment of transition metal containing inks and pigments. Restaurator 29:184–198
12. Kolar J, Malešič J, Kočar D, Strlič M, de Bruin G, Koleša D (2012) Characterisation of paper containing iron gall ink using size exclusion chromatography. Polym Degrad Stab 97:2212–221610.1016/j.polymdegradstab.2012.08.005 ↗
13. Malešič J, Strlič M, Kolar J, Polanc S (2005a) The influence of halide and pseudo-halide antioxidants in Fenton-like reaction systems containing copper(II) ions. J Mol Catal A: Chem 241:126–13210.1016/j.molcata.2005.06.047 ↗
14. Malešič J, Kolar J, Strlič M, Polanc S (2005b) The use of halides for stabilisation of iron gall ink containing paper: the pronounced effect of cation. E Preserv Sci 2:13–18
15. Malešič J, Kolar J, Strlič M, Polanc S (2006) The influence of halide and pseudo-halide antioxidants in Fenton-like reaction systems. Acta Chim Slov 53:450–456
16. Malešič J, Kočar D, Balažic A (2012) Stabilization of copper and iron containing papers in mildly alkaline environment. Polym Degrad Stab 97:118–12310.1016/j.polymdegradstab.2011.09.025 ↗
17. Neevel J (1995) Phytate: a potential conservation agent for treatment of ink corrosion caused by iron gall inks. Restaurator 16:143–16010.1515/rest.1995.16.3.143 ↗
18. Neevel J (2006) The development of in situ methods for identification of iron gall inks. In: Kolar J, Strlič M (ed) Iron gall inks: on manufacture, characterisation, degradation and stabilisation. National and university library, Ljubljana, pp 147–173
19. Neevel JG, Mensch K (1999) The behaviour of iron ions and sulphuric acid during iron-gall ink corrosion. Preprints of the 12th triennial meeting of the ICOM committee for conservation, vol II. International Council of Museums, Lyon, pp 528–533
20. Page DH, Scallan MA, Middleton SR, Zou X (1995) Method for the deacidification of papers and books. Patent US (ed) Pulp and Paper Research Institute of Canada
21. Potthast A, Henniges U, Banik G (2008) Iron gall ink-induced corrosion of cellulose: aging, degradation and stabilization. Part 1: model paper studies. Cellulose 15:849–85910.1007/s10570-008-9237-1 ↗
22. Reissland B, de Groot S (1999) Ink corrosion: comparison of currently used aqueous treatments of paper objects. http://www.iada-home.org/ta99_121.pdf . Accessed 13 Nov 2013
23. Reissland B, van Gulik R, de la Chapelle A (2006) Non-aqueous prototype treatment agents for ink-corroded papers: evaluation of side effects. In: Kolar J, Strlič M (ed) Iron gall inks: on manufacture, characterisation, degradation and stabilisation. National and university library, Ljubljana, pp 215–246
24. Reissland B, Scheper K, Fleischer S (2007) Phytate-treatment. The Iron Gall Ink Website. http://irongallink.org/igi_index43e7.html . Accessed 13 Nov 2013
25. Rouchon V, Durocher B, Pellizzi E, Stordiau-Pallot J (2009) The water sensitivity of iron gall ink and its risk assessment. Stud Conserv 54:236–25410.1179/sic.2009.54.4.236 ↗
26. Rouchon V, Duranton M, Burgaud C, Pellizzi E, Lavédrine B, Janssens K, de Nolf W, Nuyts G, Vanmeert F, Hellemans K (2011a) Room-temperature study of iron gall ink impregnated paper degradation under various oxygen and humidity conditions: time-dependent monitoring by viscosity and X-ray absorption near-edge spectrometry measurements. Anal Chem 83:2589–259710.1021/ac1029242 ↗
27. Rouchon V, Pellizzi E, Duranton M, Vanmeert F, Janssens K (2011b) Combining Xanes, ICP-AES and SEM/EDS for the study of phytate chelating treatments used on iron gall ink damages manuscripts. J Anal Atom Spectrom 26:2434–244110.1039/c1ja10185d ↗
28. Rouchon V, Duranton M, Belhadj O, Bastier-Deroches M, Duplat V, Walbert C, Vinther Hansen B (2013) The use of halide charged interleaves for treatment of iron gall ink damaged papers. Polym Degrade Stab 89:1339–134710.1016/j.polymdegradstab.2013.03.028 ↗
29. Scholten S (1997) Proceedings European workshop on iron-gall ink corrosion. Instituut Collectie Nederland, Amsterdam, pp 9–12
30. Šelih VS, Strlič M, Kolar J, Pihlar B (2007) The role of transition metals in oxidative degradation of cellulose. Polym Degrad Stab 92:1476–148110.1016/j.polymdegradstab.2007.05.006 ↗
31. Shahani CJ, Hengemihle FH (1986) In: Zeronian SH, Needles H (ed) Preservation of historic textile and paper materials. Advances in Chemistry Series, No. 212. American Chemical Society, Washington, pp 387–41010.1021/ba-1986-0212.ch022 ↗
32. Stijnman A (2006) Iron gall inks in history: ingredients and production. In: Kolar J, Strlič M (ed) Iron gall inks: on manufacture, characterisation, degradation and stabilization. National and University Library, Ljubljana, pp. 25–68
33. Stol R, Pedersoli JL Jr, Poppe H, Kok WTh (2002) Application of size exclusion electrochromatography to the microanalytical determination of the molecular mass from objects of cultural and historical value. Anal Chem 74:2314–232010.1021/ac0111309 ↗
34. Strlič M, Kolar J (2005) Ageing and stabilisation of paper. National and university library, Ljubljana
35. Strlič M, Kolar J, Kočar D, Drnovšek T, Šelih VS, Susič R, Pihlar B (2004) What is the pH of alkaline paper? E Preserv Sci 1:35–47
36. Strlič M, Šelih VS, Kolar J (2006) Model studies of the catalytic role of transition metals. In: Kolar J, Strlič M (ed) Iron gall inks: on manufacture, characterisation, degradation and stabilisation. National and university library, Ljubljana, pp 173–181
37. Vinter Hansen B (2005) Improving ageing properties of paper with iron-gall ink by interleaving with papers impregnated with alkaline buffer and antioxidant. Restaurator 26:190–202
38. Williams JC, Fowler CS, Lyon MS, Merrill TL (1977) Metallic catalysts in the oxidative degradation of paper. In: William JC (ed) Preservation of paper and textiles of historic and artistic value. Advances in Chemistry Series, No. 164. American Chemical Society, Washington, pp 37–61
39. Wilson H, Chris Carr, Hacke M (2012) Production and validation of model iron-tannate dyed textiles for use as historic textile substitutes in stabilization treatment studies. Chem Cent J 6:4410.1186/1752-153X-6-44 ↗
40. Zou X, Gurnagul N, Uesaka T, Bouchard J (1994) Accelerated aging of papers of pure cellulose: mechanism of cellulose degradation and paper embrittlement. Polym Degrad Stab 4:393–40210.1016/0141-3910(94)90011-6 ↗