The use of polyamidoamines for the conservation of iron-gall inked paper
Source abstract
Abstract
A new approach to the conservation of paper manuscripts is proposed that leads to both deacidification and strengthening of paper. The study was carried out by using polyamidoamines (PAAOHs) functionalized with alcoholic groups, in their native form (PAAb) or neutralized with boric acid (PAAn). They were applied on model paper samples containing iron-gall ink spots through agar rigid gel or by brushing. Preliminary evaluation of the effects of polymer concentration, methods, and duration of application have been tested on model ink-free paper samples. The improvements induced by PAAOHs on paper samples was revealed by surface pH (evaluated in ink-free areas, inside ink spots and on the edges between them) and by measurements of alkaline reserve according to TAPPI T 553 pm-92. The results showed the different behaviour of ink-free and inked regions due to high acidity of iron gall ink. In fact, although a treatment with solutions having low concentration (i.e. 0.1 and 0.15 M) is sufficient for preserving ink-free paper samples from ageing, higher concentration of polymer (0.3 M) or extra brushing application are needed in order to get a complete deacidification of the ink spots. As a side-effect of deacidification treatments, PAAOHs promoted a significant reduction of thermo-hygrometric ageing effects and water smearing at the edge of iron-gall ink spots, as suggested by Raman spectroscopy and mechanical analyses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Cultural Heritage Materials Analysis · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Anzani M, Berzioli M, Cagna M, Campani E, Casoli A, Cremonesi P, Fratelli M, Rabbolini A, Riggiardi D (2008) Use of rigid agar gels for cleaning of plaster objects. Quaderno n.6/Cesmar7, Il Prato Casa Editrice, Saonara, p 55
2. Ball P (2002) Nanotechnologies for conservation of cultural heritage: paper and canvas deacidification. Nature News (Online), Oct 22. https://doi.org/10.1038/news021021-1 . Accessed 19 Nov 201510.1038/news021021-1 ↗
3. Banik G, Sobotka WK (1988) Deacidification and strengthening of bound newspapers through aqueous immersion. In: Luner P (ed) Paper preservation, current issue and recent developments. Tappi Press, Atlanta, p 137
4. Baty JW, Maitland CL, Minter W, Hubbe MA, Jordan-Movery SK (2010) Deacidification for conservation. BioResources 5(3):1955–202310.15376/biores.5.3.1955-2023 ↗
5. Bicchieri M, Brusa P (1997) The bleaching of paper by reduction with the borane terzbutylamine complex. Restaurator 18:1–11
6. Bicchieri M, Bella M, Semetilli F (1999) A quantitative measure of borane terzbutylamine complex effectiveness in carbonyl reduction of aged papers. Restaurator 20:22–29
7. Bicchieri M, Semetilli F, Sodo A (2000) Application of seven borane complexes in paper conservation. Restaurator 21:213–228
8. Bicchieri M, Monti M, Piantanida G, Pinzari F, Iannuccelli S, Sotgiu S, Tireni L (2011) The Indian drawings of the poet Cesare Pascarella: non-destructive analyses and conservation treatments. Anal Bioanal Chem 402:1517–152810.1007/s00216-011-5229-3 ↗
9. Blüher A, Vogelsanger B (2001) Mass deacidification of paper. Chimia 55:981–98910.2533/chimia.2001.981 ↗
10. Campani E, Casoli A, Cremonesi P, Saccani I, Signorini E (2007) Use of agarose and agar for preparing rigid gels. Quaderno n.4/Cesmar7, Il Prato Casa Editrice, Saonara, p 50
11. Clark RJH, Jibbs PJ, Jarjis RA (1998) An investigation into the deacidification of paper by ethoxymagnesium ethylcarbonate. J Mater Chem 8:2685–269010.1039/a804453h ↗
12. Cremonesi P (2012) L’ambiente acquoso per il trattamento di opere policrome. Il Prato casa Editrice, Saonara, p 111
13. Dey RK, Ray AR (2003) Synthesis, characterization and blood compatibility of polyamidoamines copolymers. Biomaterials 24:2985–299310.1016/S0142-9612(03)00122-4 ↗
14. Dupont AL, Lavédrine B, Cheradame H (2010) Mass deacidification and reinforcement of papers and books VI: study of aminopropylmethyldiethoxysilane treated papers. Polym Degrad Stab 95:2300–230810.1016/j.polymdegradstab.2010.09.002 ↗
15. Erhardt D, Mecklenburg MF (1995) Accelerated vs natural aging: Effect of aging conditions on the aging process of cellulose. In: Materials issues in art and archaeology IV, materials research society symposium proceedings, vol 352, pp 247–27010.1557/PROC-352-247 ↗
16. Erhardt D, Tumosa CS, Mecklenburg MF (1999) Material consequence of the aging of paper. In: 12th triennal meeting Lyon, 29 Aug–3 Sept, vol II, pp 501–506
17. Erhardt D, Tumosa CS, Mecklenburg MF (2000) Chapter 3: Chemical and physical changes in naturally and accelerated aged cellulose. In: Cardamone JM, Baker M (eds) Historic textiles, papers and polymers in museums, symposium 779. American Chemical Society, Washington, pp 23–3710.1021/bk-2001-0779.ch003 ↗
18. Federici C, Rossi L (1983) Manuale di conservazione e restauro del libro. La Nuova Italia Scientifica, Roma, p 260
19. Ferruti P (2013) Poly(amidoamine)s: past, present, and perspectives. J Polym Sci Pol Chem 51:2319–235310.1002/pola.26632 ↗
20. Giorgi R, Dei L, Ceccato M, Schettino CV, Baglioni P (2002) Nanotechnologies for conservation of cultural heritage: paper and canvas deacidification. Langmuir 18:8198–820310.1021/la025964d ↗
21. Giorgi R, Bozzi C, Dei L, Gabbiani C, Ninham BW, Baglioni P (2005a) Nanoparticles of Mg(OH)2: synthesis and application to paper conservation. Langmuir 21:8495–850110.1021/la050564m ↗
22. Giorgi R, Chelazzi D, Baglioni P (2005b) Nanoparticles of calcium hydroxide for wood conservation. The deacidification of the Vasa warship. Langmuir 21:10743–1074810.1021/la0506731 ↗
23. Girardi F, Bergamonti L, Isca C, Predieri G, Graiff C, Lottici PP, Cappelletto E, Ataollahi N, Di Maggio R (2017) Chemical–physical characterization of ancient paper with functionalized polyamidoamines (PAAs). Cellulose 24:105710.1007/s10570-016-1159-8 ↗
24. Graiff C, Pontiroli D, Bergamonti L, Cavallari C, Lottici PP, Predieri G (2015) Structural investigation of N-N′-Methylenebisacrylamide via X-ray diffraction assisted by crystal structure prediction. J Appl Crystallogr 48:550–55710.1107/S1600576715004161 ↗
25. Holmes J (1988) Mass deacidification of books at the national archives and the national library of Canada. In: Luner P (ed) Paper preservation, current issues and recent developments. Tappi Press, Atlanta, p 144
26. Hubbe MA, Smith RD, Zou X, Katuscak S, Potthast A, Ahn K (2017) Deacidification of acidic books and paper by means of non-aqueous dispersions of alkaline particles: a review focusing on completeness of the reaction. BioResources 12(2):4410–447710.15376/biores.12.2.Hubbe ↗
27. Huhsmann E, Hänner U (2008) Work standard for the treatment of 18th and 19th century iron-gall ink documents with calcium phytate and calcium hydrogen carbonate. Restaurator 29:264–318
28. Iannuccelli S, Sotgiu S (2010) Wet treatments of work of art on paper with rigid gellan gels. In: The book and paper group annual 29, book and paper group session, AIC’s 38th annual meeting, Milwaukee, Wisconsin, pp 25–39
29. Isca C (2014) The use of polysaccharide rigid gels. Multi analytical approach for the study of their performance, effectiveness and interference with paper artworks, Ph.D. thesis in chemical science, University of Parma
30. Isca C, D’Avorgna S, Graiff G, Montanari M, Ugozzoli F, Predieri G (2016) Paper preservation with polyammidoammine: a preliminary study. Cellulose 23:1415–143210.1007/s10570-016-0880-7 ↗
31. Kolar J, Strlič M, Budnar M, Malešič J, Šelih VS, Simčič J (2003) Stabilisation of corrosive iron gall inks. Acta Chim Slov 50:763–770
32. Kolar J, Sala M, Strlič M, Šelih VS (2005) Stabilisation of paper containing iron-gall ink with current aqueous processes. Restaurator 26:181–189
33. Kolar J, Alenka Možir, Strlič M, de Bruin G, Pihlar B, Steemers T (2007) Stabilization of iron gall ink: aqueous treatment with magnesium phytate. E-Preserv Sci. www.morana-rtd.com , e-PS, 2007, vol 4, pp 19–24 (ISSN: 1581-9280 web edition)
34. Kozak JJ, Spartz RE (1988) Deacidification of paper by bookeeper process. In: Luner P (ed) Paper preservation, current issues and recent developments. Tappi Press, Atlanta, p 129
35. Lattuati-Derieux A, Bonnassies-Termes S, Lavédrine B (2004) Identification of volatile organic compounds emitted by a naturally aged book using solid-phase microextraction/gas chromatography/mass spectrometry. J Chromatogr A 1026:9–1810.1016/j.chroma.2003.11.069 ↗
36. Lee AS, Mahon PJ, Creagh DC (2006) Raman analysis of iron gall inks on parchment. Vib Spectrosc 41:170–17510.1016/j.vibspec.2005.11.006 ↗
37. Liers J, Schwerdt P (1995) The battelle mass deacidification process equipment and technology. Restaurator 16(1):1–9
38. Liers J, Vogelsanger B (1997) Das Massenentsäuerungsverfahren der Deutschen bibliothek. Das Papier 51:118–126
39. Margutti S, Conio G, Calvini P, Pedemonte E (2001) Hydrolitic and oxidative degradation of paper. Restaurator 22(2):67–83
40. Mazzuca C, Bocchinfuso G, Cacciotti I, Micheli L, Palleschi G, Palleschi A (2013) Versatile hydrogels: an efficient way to clean paper artworks. RSC Adv 3:22896–2289910.1039/c3ra44387f ↗
41. Mazzuca C, Micheli L, Carbone M, Basoli F, Cervelli E, Iannuccelli S, Sotgiu S, Palleschi A (2014a) Gellan hydrogel as a powerful tool in paper cleaning process: a detailed study. J Colloid Interface Sci 416:205–21110.1016/j.jcis.2013.10.062 ↗
42. Mazzuca C, Micheli L, Marini F, Bevilacqua M, Bocchinfuso G, Palleschi G, Palleschi A (2014b) Rheoreversible hydrogels in paper restoration processes: a versatile tool. Chem Cent J 8(10):1–11
43. Piovesan C, Dupont AL, Fabre-Francke I, Fichet O, Lavédrine B, Chéradame H (2014) Strengthening by polyaminoalkylalkoxysilane copolymer networks applied by spray or immersion: a model study. Cellulose 21:705–71510.1007/s10570-013-0151-9 ↗
44. Poggi G, Giorgi R, Toccafondi N, Katzur V, Baglioni P (2010) Hydroxide nanoparticles for deacidification and concomitant inhibition of iron-gall ink corrosion paper. Langmuir 26(24):19084–1909010.1021/la1030944 ↗
45. Poggi G, Toccafondi N, Melita LN, Knowles JC, Bozec L, Giorgi R, Baglioni P (2014) Calcium hydroxide nanoparticles for the conservation of cultural heritage: new formulation for the deacidification of cellulose-based artifacts. Apply Phys A 114:685–69310.1007/s00339-013-8172-7 ↗
46. Poggi G, Sistach MC, Marin E, Garcia JF, Giorgi R, Baglioni P (2016) Calcium hydroxide nanoparticles in hydroalcoholic gelatin solutions(GeolNan) for the deacidification and strengthening of papers containing iron gall ink. J Cult Herit 18:250–25710.1016/j.culher.2015.10.005 ↗
47. Ponce A, Brostoff LB, Gibbons SK, Zavalij P, Viragh C, Hooper J, Alnemrat S, Gaskell KJ, Eichhorn B (2016) Elucidation of the Fe(III) gallate structure in historical iron gall ink. Anal Chem 88:5152–515810.1021/acs.analchem.6b00088 ↗
48. Potthast A, Henniges U, Banik G (2008) Iron gall ink-induced corrosion of cellulose: aging, degradation and stabilization. Part 1: model paper studies. Cellulose 15(6):849–85910.1007/s10570-008-9237-1 ↗
49. Senvaitiene J, Beganskiene A, Kareiva A (2005) Spectroscopic evaluation and characterization of different historical writing inks. Vib Spectrosc 37:61–6710.1016/j.vibspec.2004.06.004 ↗
50. Sequeira S, Casanova C, Cabrita EJ (2006) Deacidification paper using dispersion of Ca(OH)2 nanoparticles in isopropanol: study of efficiency. J Cult Herit 7:264–27210.1016/j.culher.2006.04.004 ↗
51. Smith RD (1987) Mass deacidification at the public archives of Canada. In: Petherbridge G (ed) Conservation of library and archive materials and the graphic arts. Butterworths, London, p 125
52. Smith AW (2011) Aqueous deacidification of paper. In: Banik G, Brückle I (eds) Paper and water, a guide for conservators. Taylor & Francis, Milton Park, pp 341–388
53. Strlič M, Kolar J, Šelih VS, Kocar D, Pihlar B (2003) A comparative study of several transition metals in Fenton-like reaction system at circum-neutral. Acta Chim Slov 50:619–632
54. Strlič M, Menart E, Cigi IK, Kolar J, De Bruin G, Cassar M (2010) Emission of reactive oxygen species during degradation of iron gall ink. Polym Degrad Stab 95:66–7110.1016/j.polymdegradstab.2009.10.011 ↗
55. Strlič M, Cigi IK, Možir A, Kolar J, Cassar M (2011) The effect of volatile organic compounds and hypoxia on paper degradation. Polym Degrad Stab 96:608–61510.1016/j.polymdegradstab.2010.12.017 ↗
56. Sullivan M, Brogdon-Grantham S, Taira K (2014) New approaches to cleaning works of art on paper and photographs, vol 2. Winterthur/University of Delaware Program in Art Conservation, ANAGPIC, Newark
57. Whitmore PM (2011) Paper ageing and the influence of water. In: Banik G, Brückle I (eds) Paper and water, a guide for conservators. Taylor & Francis, Milton Park, pp 219–253
58. Wolbers R (2000) Cleaning painted surfaces, aqueous methods. Archetype Publications, London
59. Wolbers R (2004) Un approccio acquoso alla pulitura dei dipinti. Quaderno n.1/Cesmar7, Il Prato Casa Editrice, Saonara, p 48
60. Zumbühl S, Wülfert S (1994) An evaluation of the bookeeper mass deacidification process. In: Melinick SM (ed) Technical evaluation team report for the preservation directorate, library of congress, Washington, Pittsburgh
61. Zumbühl S, Wülfert S (2001) Chemical aspects of the BookKeeper deacidification of cellulosic materials: the influence of surfactants. Stud Conserv 16:169–180