Corrosion of 1.4016 Ferritic Steel by Urea at High Temperature

Anastasiia Galakhova, Fabian Kadisch, Gregor Mori, Susanne Heyder, Helmut Wieser, Bernhard Sartory, Jaroslaw Wosik, Sabine Schwarz, Simon Burger

Abstract

Abstract The corrosion behavior of a ferritic unstabilized stainless steel 1.4016 during decomposition of aqueous urea solution at high temperature has been investigated. Corrosion was obtained from 100 h of cyclic heating (from room temperature up to 600 °C) and injection of aqueous urea solution on the steel plate in a laboratory-scale test bench. The evaluation procedure covered the metallographic analysis of corroded steel samples by high-resolution scanning electron microscopy (HR-SEM) and transmission electron microscopy (TEM). Uniform corrosion underneath deposits was found as one of the drivers for degradation of the steel. Damage happened by high-temperature depassivation of stainless steel due to the excess of the aggressive medium. Besides uniform corrosion, a nitridation layer underneath surface oxides together with chromium carbonitride particles precipitated through the whole depth of the sample was identified resulting in intergranular attack.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. L.L. Wei, L.Q. Chen, M.Y. Ma, H.L. Liu, and R.D.K. Misra, Oxidation Behavior of Ferritic Stainless Steels in Simulated Automotive Exhaust Gas Containing 5 vol.% Water Vapor, Mater. Chem. Phys., 2018, 205, p 508–517. https://doi.org/10.1016/j.matchemphys.2017.11.05110.1016/j.matchemphys.2017.11.051 ↗
2. X.L. Wang, A.R. Huang, M.X. Li, W. Zhang, C.J. Shang, J.L. Wang, and Z.J. Xie, The significant Roles of Nb and Mo on Enhancement of High Temperature Urea Corrosion Resistance in Ferritic Stainless Steel, Mater. Lett., 2020, 269, p 127660. https://doi.org/10.1016/j.matlet.2020.12766010.1016/j.matlet.2020.127660 ↗
3. X. Wang, Q. Lu, W. Zhang, Zh. Xie, and Ch. Shang, Investigation on the Correlation Between Inclusions and High Temperature Urea Corrosion Behavior in Ferritic Stainless Steel, Metals, 2021, 11, p 1823–1832. https://doi.org/10.3390/met1111182310.3390/met11111823 ↗
4. Floyd R, Kotrba A, Martin S, Prodin K. Material Corrosion Investigations for Urea SCR Diesel Exhaust Systems. SAE Int. (2009)10.4271/2009-01-2883 ↗
5. J. Nockert and M. Norell, Corrosion at the Urea Injection in SCR-System during Component Test, Mater. Corros., 2013, 64, p 34–42. https://doi.org/10.1002/maco.20100598310.1002/maco.201005983 ↗
6. M. Milutinovic, R. Lendjel, S. Balos, D. Zlatanovic, L. Sevsek, and T. Pepelnjak, Characterisation of Geometrical and Physical Properties of a Stainless Steel Denture Framework Manufactured by Single-Point Incremental Forming, J. Mater. Res. Technol., 2021, 10, p 605–623. https://doi.org/10.1016/j.jmrt.2020.12.01410.1016/j.jmrt.2020.12.014 ↗
7. J. Nockert, L. Nyborg, and M. Norell, Corrosion of Stainless Steels in Simulated Diesel Exhaust Environment with Urea, Mater. Corros., 2012, 63, p 388–395. https://doi.org/10.1002/maco.20100578310.1002/maco.201005783 ↗
8. C. Miraval, S. Saedlou, R. Evrard, P. Santacreu, and J. Leseux, Influence of Selective Catalytic Reduction (SCR) System on Stainless Steel Durability, REM: Rev Esc. Minas., 2013, 66, p 153–158.
9. B. Won-Jin, Y. Kwi-Suba, P. Chan-Jin, R. Han-Jin, and K. Young-Ho, Comparison of Influences of NaCl and CaCl2 on the CORROSION of 11% and 17% Cr Ferritic Stainless Steels during Cyclic Corrosion Test, Corros. Sci., 2010, 52, p 734–739. https://doi.org/10.1016/j.corsci.2009.10.03310.1016/j.corsci.2009.10.033 ↗
10. J.R. Crum, G.D. Smith, and H.L. Flower, Resistance of Automotive Exhaust Flexible Coupling Alloys to Hot Salt Attack, Stress Corrosion Cracking and High Temperature Embrittlement, SAE Int. J. Mater. Manuf., 1999, 108, p 403–410.
11. H. Zhao, M. Lei, X. Chen, and W. Tang, Facile Route to Metal Nitrides Through Melamine and Metal Oxides, J. Mat. Chem., 2006, 16, p 4407–4412. https://doi.org/10.1039/b611381h10.1039/b611381h ↗
12. M. Lei, H.Z. Zhao, H. Yang, B. Song, and W.H. Tang, Synthesis of Transition Metal Carbide Nanoparticles through Melamine and Metal Oxides, J. Eur. Ceram. Soc., 2008, 28, p 1671–1677. https://doi.org/10.1016/j.jeurceramsoc.2007.11.01310.1016/j.jeurceramsoc.2007.11.013 ↗
13. B. Wei, W. Yang, J. Wang, H. Tan, S. Zhou, and F. Wang, Study on Reduction Mechanism of Fe2O3 by NH3 under SNCR Condition, Fuel, 2019, 255, p 115814. https://doi.org/10.1016/j.fuel.2019.11581410.1016/j.fuel.2019.115814 ↗
14. S. Saedlou, P. Santacreu, and J. Leseux, Suitable Stainless Steel Selection for Exhaust Line Containing a Selective Catalytic Reduction (SCR) System, SAE Int., 2011 https://doi.org/10.4271/2011-01-132310.4271/2011-01-1323 ↗
15. J. Lu, Z. Yang, B. Zhang, J. Huang, and H. Xu, Corrosion Behavior of Candidate Materials Used for Urea Hydrolysis Equipment in Coal-Fired Selective Catalytic Reduction Units, J. Mater. Eng. Perform., 2018, 27, p 3290–3296. https://doi.org/10.1007/s11665-017-3001-310.1007/s11665-017-3001-3 ↗
16. M.L. Morgan, Failure Analysis of an 18% Cr Ferritic Stainless Steel in a Simulated Exhaust Condensate Containing Urea, J. Fail. Anal. Prev., 2018, 18, p 117–120. https://doi.org/10.1007/s11668-018-0387-710.1007/s11668-018-0387-7 ↗
17. A. Galakhova, F. Kadisch, G. Mori, S. Heyder, H. Wieser, B. Sartory, and S. Burger, Corrosion of Stainless Steel by Urea at High Temperature, Corros. Mater. Degrad., 2021, 2, p 461–473. https://doi.org/10.3390/cmd203002410.3390/cmd2030024 ↗
18. R.L. Cowan and C.S. Tedmon, Intergranular Corrosion of Iron-Nickel-Chromium Alloys, Advances in Corrosion Science and Technology. M.G. Fontana, R.W. Staehle Ed., Springer, New York, 1973