Investigations of Tungsten Inert Gas and Metal Active Gas Joints of SUS301L Stainless Steel: Electron Backscatter Diffraction Characterization and Fatigue Performance
Source abstract
Abstract
SUS301L stainless steel joints with thickness of 2 mm were manufactured via the tungsten inert gas (TIG) and metal active gas arc (MAG) techniques, respectively. Electron backscatter diffraction results indicated that δ-ferrites with volume fraction of approximately 1.8% were formed in the weld seam of TIG joints, which was unbeneficial for the mechanical strength. By contrast, the microstructures were relatively fine and no δ-ferrites were formed in the MAG joints, showing a better microstructural quality compared with that of TIG joints. Nevertheless, the fatigue test results indicated that fatigue strength of TIG joints was higher compared with that of MAG joints. This was because that the lower weld reinforcement of TIG joints decreased the stress concentration at weld toe than that of MAG joints, which resulted in the better fatigue performance, implying that the fatigue behavior of welded joints was more influenced by the welding quality instead of microstructures.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. X. Gu, L. Zhu, S. Wu, Z. Duan, and L. Zhu, Effect of Welding Parameters on Weld Formation Quality and Tensile-Shear Property of Laser Welded SUS301L Stainless Steel Lap Filet Weld, J. Market. Res., 2020, 9, p 4840–4854.
2. Y. Zhang, D. Sun, X. Gu, and H. Li, Microstructure and Mechanical Property Improvement of Dissimilar Metal Joints for TC4 Ti Alloy to 301L Stainless Steel, J. Mater. Sci., 2018, 53, p 2942–2955.10.1007/s10853-017-1708-z ↗
3. X. Wang, G. Yi, Q. Sun, M. Xiao, Y. Gao, Z. Zhang et al., Study on δ-Ferrite Evolution and Properties of Laser Fusion Zone During Post-Weld Heat Treatment on Al-Si Coated Press-Hardened Steel, J. Mater. Res. Technol., 2020, 9, p 5712–5722.10.1016/j.jmrt.2020.03.096 ↗
4. J.Y. Cho, F. Czerwinski, and J.A. Szpunar, The Effect of Reheating Conditions and Chemical Composition on δ Ferrite Content in Austenitic Stainless Steel Slabs, J. Mater. Sci., 2000, 35, p 1997–2003.10.1023/A:1004734906671 ↗
5. A. Dehghan-Manshadi and P.D. Hodgson, Effect of δ-Ferrite Co-existence on Hot Deformation and Recrystallization of Austenite, J. Mater. Sci., 2008, 43, p 6272–6277.10.1007/s10853-008-2907-4 ↗
6. M. Shojaati, S.F. KashaniBozorg, M. Vatanara, M. Yazdizadeh, and M. Abbasi, The Heat Affected Zone of X20Cr13 Martensitic Stainless Steel after Multiple Repair Welding: Microstructure and Mechanical Properties Assessment, Int. J. Pres. Ves. Pip., 2020, 188, p 104205.10.1016/j.ijpvp.2020.104205 ↗
7. J.W. Fu, Y.S. Yang, J.J. Guo, and W.H. Tong, Effect of Cooling Rate on Solidification Microstructures in AISI 304 Stainless Steel, Mater. Sci. Technol. Lond., 2008, 24, p 941–944.10.1179/174328408X295962 ↗
8. Q. Wang, S. Chen, and L. Rong, Δ-Ferrite Formation and its Effect on the Mechanical Properties of Heavy-Section AISI 316 Stainless Steel Casting, Metall. Mater. Trans. A., 2020, 51, p 2998–3008.10.1007/s11661-020-05717-0 ↗
9. Z.H. Fu, B.J. Yang, M.L. Shan, T. Li, Z.Y. Zhu, C.P. Ma et al., Hydrogen Embrittlement Behavior of SUS301L-MT Stainless Steel Laser-Arc Hybrid Welded Joint Localized Zones, Corros. Sci., 2020, 164, p 108337.10.1016/j.corsci.2019.108337 ↗
10. D. Tang, C. Wang, M. Tian, J. Wang, and X. Hu, Contrasting Study on Quality of SUS301L-HT Jointsin Fiber Laser Welding and MIG Welding, Chin. J. Lasers, 2015, 42, p 98–105.
11. J. Jeong, Y. Lee, J.M. Park, D.J. Lee, I. Jeon, H. Sohn et al., Metastable δ-Ferrite and Twinning-Induced Plasticity on the Strain Hardening Behavior of Directed Energy Deposition-Processed 304L Austenitic Stainless Steel, Addit. Manuf., 2021, 47, p 102363.
12. X. Hu, N. Xiao, X. Luo, and D. Li, Effects of δ-Ferrite on the Microstructure and Mechanical Properties in a Tungsten-Alloyed 10%Cr Ultra-Supercritical Steel, Acta Metall. Sin., 2009, 45, p 553–558.
13. M. Su, L. Xu, C. Feng, Y. Han, L. Zhao, and G. Xiao, Microstructural Investigation and Model of Fatigue Short Crack in EH36 Steels, Fatigue Fract. Eng. Mater., 2022, 45, p 2227–2242.10.1111/ffe.13731 ↗
14. M. Su, L. Xu, C. Peng, Y. Han, and L. Zhao, Fatigue Short Crack Growth, Model and EBSD Characterization of Marine Steel Welding Joint, Int. J. Fatigue, 2022, 156, p 106689.10.1016/j.ijfatigue.2021.106689 ↗
15. M. Su, C. Feng, C. Peng, L. Xu, Y. Han and L. Zhao, A unified approach for describing metallic fatigue short and long crack growth behaviors via plastic accumulated damage, Int. J. Fatigue, 2023, 166, p 107258.10.1016/j.ijfatigue.2022.107258 ↗
16. L.H.S. Barbosa, P.J. Modenesi, L.B. Godefroid, and A.R. Arias, Fatigue Crack Growth Rates on the Weld Metal of High Heat Input Submerged Arc Welding, Int. J. Fatigue, 2019, 119, p 43–51.10.1016/j.ijfatigue.2018.09.020 ↗
17. H. Luo, G. Kang, and Q. Kan, A Low-Cycle Fatigue Life-Prediction Model for SUS301L Stainless Steel Butt-Welded Joint with Considering Ratchetting, Int. J. Fatigue, 2020, 139, p 105777.10.1016/j.ijfatigue.2020.105777 ↗
18. K.A. Vasudeven, A Review of Crack Closure, Fatigue Crack Threshold and Related Phenomena, Mater. Sci. Eng. A, 1994, 188, p 1–22.10.1016/0921-5093(94)90351-4 ↗
19. J. Xing, F. Yuan, and X. Wu, Enhanced Quasi-Static and Dynamic Shear Properties by Heterogeneous Gradient and Lamella Structures in 301 Stainless Steels, Mater. Sci. Eng., A, 2017, 680, p 305–316.10.1016/j.msea.2016.10.111 ↗
20. L.P. Kubin and A. Mortensen, Geometrically Necessary Dislocations and Strain-Gradient Plasticity: A Few Critical Issues, Scr. Mater., 2003, 48, p 119–125.10.1016/S1359-6462(02)00335-4 ↗
21. C. Han, H. Gao, Y. Huang, and W.D. Nix, Mechanism-Based Strain Gradient Crystal Plasticity—I, Theory. J. Mech. Phys. Solids, 2005, 53, p 1188–1203.10.1016/j.jmps.2004.08.008 ↗
22. Metallic Materials—Tensile Testing—Part 1: Method of Test at Room Temperature. ISO 6892-1 (2016)
23. ASTM E647-15e1, Standard Test Method for Measurement of Fatigue Crack Growth Rates (ASTM, International, West Conshohocken, PA, 2015)
24. Metallic materials—Fatigue testing—Statistical planning and analysis of data (ISO 12107, 2003)
25. H. Luo, G. Kang, Q. Kan, and Y. Huang, Experimental Investigation on the Heterogeneous Ratchetting of SUS301L Stainless Steel Butt Weld Joint During Uniaxial Cyclic Loading, Int. J. Fatigue, 2017, 105, p 169–179.10.1016/j.ijfatigue.2017.08.027 ↗
26. S. Fan, H. Hao, L. Meng, and X. Zhang, Effect of Deep Cryogenic Treatment Parameters on Martensite Multi-level Microstructures and Properties in a Lath Martensite/Ferrite Dual-Phase Steel, Mater. Sci. Eng., A, 2021, 810, p 141022.10.1016/j.msea.2021.141022 ↗
27. Y. Li, Z. Wang, S. Zhang, N. Liu, Y. Wang, P. Zhu et al., High Pressure Induced Ultra-Hard Twinned Lath Martensite in Binary Fe-15wt.%Cr Alloy, Scr. Mater., 2020, 187, p 163–168.10.1016/j.scriptamat.2020.06.004 ↗
28. Y. Mine, K. Hirashita, H. Takashima, M. Matsuda, and K. Takashima, Micro-tension Behaviour of Lath Martensite Structures of Carbon Steel, Mater. Sci. Eng., A, 2013, 560, p 535–544.10.1016/j.msea.2012.09.099 ↗
29. D. Lin, L. Xu, Y. Han, Y. Zhang, H. Jing, L. Zhao et al., Structure and Mechanical Properties of a FeCoCrNi High-Entropy Alloy Fabricated via Selective Laser Melting, Intermetallics, 2020, 127, p 106963.10.1016/j.intermet.2020.106963 ↗
30. J.A. Brooks, J.C. Williams, and A.W. Thompson, STEM Analysis of Primary Austenite Solidified Stainless Steel Welds, Metall. Trans. A, 1983, 14, p 23–31.10.1007/BF02643733 ↗
31. Y. Chen, B. Jessel, B. Fu, X. Yu, and J. Pittock, Ecosystem Services and Management Strategy in China, Springer, Berlin, 2013.
32. C.C. Roth and D. Mohr, Ductile Fracture Experiments with Locally Proportional Loading Histories, Int. J. Plasticity, 2016, 79, p 328–354.10.1016/j.ijplas.2015.08.004 ↗
33. A. Pineau, A.A. Benzerga, and T. Pardoen, Failure of Metals I: Brittle and Ductile Fracture, Acta Mater., 2016, 107, p 424–483.10.1016/j.actamat.2015.12.034 ↗
34. Erratum to: Recommendations for fatigue design of welded joints and components (Springer, 2017)
35. P. White, S. Barter, and L. Molent, Observations of Crack Path Changes Caused by Periodic Underloads in AA7050-T7451, Int. J. Fatigue, 2008, 30, p 1267–1278.10.1016/j.ijfatigue.2007.08.021 ↗
36. K. Manigandan, T.S. Srivatsan, T. Quick, S. Sastry, and M.L. Schmidt, Influence of Microstructure and Load Ratio on Cyclic Fatigue and Final Fracture Behavior of Two High Strength Steels, Mater. Des., 2014, 55, p 727–739.10.1016/j.matdes.2013.10.003 ↗
37. P. White, S.A. Barter, and C. Wright, Small Crack Growth Rates from Simple Sequences Containing Underloads in AA7050-T7451, Int. J. Fatigue, 2009, 31, p 1865–1874.10.1016/j.ijfatigue.2009.01.014 ↗