The microstructure of concrete made with municipal waste incinerator bottom ash as an aggregate component
Source abstract
Abstract
The interaction of municipal solid waste incinerator bottom ash (MSWI bottom ash), when utilized as an aggregate in concrete, with the cement matrix was investigated. The most prominent reaction observed in lab and field concrete was the formation of aluminium hydroxide and the release of hydrogen gas from aluminium grains reacting in the alkaline environment. The expansive aluminium reaction was identified as a main cause of extensive spalling on the concrete surface. Due to the higher content of bottle glass as part of the ash, in all samples, reaction products of an alkali-silica reaction (ASR) could be observed as well. However, damage due to ASR were less severe than those caused by the aluminium reaction. The expansion rates were low and only a few of the lab samples showed cracking. Microstructural analysis of the samples indicated clearly that a large quantity of the alkali-silica gel which was formed was accommodated in the pores and voids without exerting any strain on the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Nuclear materials and radiation effects · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Utilization of aggregate materials in road construction and bulk fill10.1016/S0921-3449(01)00067-2 ↗
2. Behaviour of cement-treated MSWI bottom ash10.1016/S0956-053X(00)00094-5 ↗
3. Technical properties and environmental compatibility of MSWI bottom ashes and other industrial by-products used as recycled materials in road construction
4. Characterization of bottom ash in municipal solid waste incinerators for its use in road base10.1016/j.wasman.2004.07.004 ↗
5. Production of glass-ceramic bodies from the bottom ashes of municipal solid waste incinerators10.1016/S0955-2219(03)00264-4 ↗
6. MSWI ashes as mineral additions in concrete10.1016/j.cemconres.2004.02.001 ↗
7. Physical and mechanical properties of cement-based products containing incineration bottom ash10.1016/S0956-053X(02)00041-7 ↗
8. A. Polettini, R. Pomi, G. Carcani, The effect of Na and Ca salts on MSWI bottom ash activation for reuse as a pozzolanic admixture, Resources, Conservation and Recycling In Press, Corrected Proof.
9. Petrology and geochemistry of a municipal solid waste incinerator residue treated at high temperature
10. Characterization of ecocement pastes and mortars produced from incineration ashes10.1016/S0008-8846(00)00467-1 ↗
11. Behavior of chloride ions in hardened eco-cement: a new type of Portland cement made from municipal waste incinerator ash
12. Eco-cement: A new Portland cement to solve municipal and industrial waste problems
13. Utilization of municipal solid wastes for mortar production10.1016/S0921-3449(02)00018-6 ↗
14. Compatibility between ecocement produced from incinerator ash and reactive aggregates in ASR expansion of mortars10.1016/S0008-8846(02)01023-2 ↗
15. Utilisation des mâchefers d'incinérateur d'ordures ménagères dans la fabrication de pavés en béton10.1007/BF02483156 ↗
16. Verwertung von Müllverbrennungsrückständen zur Herstellung zementgebundener Baustoffe
17. Use of incinerator bottom ash in concrete10.1016/S0008-8846(96)00193-7 ↗
18. Schwer- und Leichtbeton aus Müll-Schlackensinter
19. Prüfverfahren für chemische Eigenschaften von Gesteinskörnungen
20. DAfStb · 2001
21. Characterization of the bottom ash in municipal solid waste incinerator10.1016/S0304-3894(98)00246-5 ↗
22. Vergleichende mineralogische und chemische Untersuchungen an Rostschlacken aus Anlagen zur thermischen Abfallbehandlung
23. The micro-XRF — a new technique for the analysis of building materials
24. Hollemann · 1995
25. Short-term natural weathering of MSWI bottom ash10.1016/S0304-3894(00)00270-3 ↗
26. St. John · 1998
27. Alkali-silica reactivity of some frequently used lightweight aggregates10.1016/j.cemconres.2004.01.017 ↗
28. Value-added utilization of waste glass in concrete10.1016/S0008-8846(03)00251-5 ↗
29. F. Winnefeld, E. Warianka, D. Knöfel, Dauerhaftigkeit von Recyclingglas als Zuschlag in Beton in Abhängigkeit von der Rezeptur, In: F.H. Wittmann, A. Gerdes (eds.), Material Science and Restoration V, Vol. 2 of 2, Esslingen, Germany, Aedificatio, Freiburg, (1999), 1619–1630.
30. Glaseinstreuungen in Betonwerkstein
31. Aggregate-cement reactions in MSWI-bottom ash based concrete — a petrographic assesment
32. Lightweight aggregate based on waste glass and its alkali-silica reactivity10.1016/S0008-8846(01)00663-9 ↗