Abstract
The microstructure and frictional behavior of candidate protective coatings for steel continuous casting copper molds were studied. A number of conventional coatings, consisting of the hard chromium deposited by electroplating, nickel-phosphorus deposited by electroless plating, and WC-17Co deposited by high-velocity oxy-fuel spraying, were compared with copper aluminide and nickel aluminide coatings. The copper aluminide coating was formed via pack cementation diffusion and aluminized in the Al-AlCl3-Al2O3 powder mixture at 500 °C. The nickel aluminide coating was obtained using the same aluminizing treatment, yet after depositing an electroless nickel-phosphorus interlayer. The microstructure of the coated specimens was characterized by scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction phase analysis. Cu9Al4 was identified as the main phase of the copper aluminide coating, whereas Ni2Al3 and NiAl phases were identified in the nickel aluminide coating. The evaluation of the coatings frictional behavior through a pin-on-disk machine applying a 12 N loading showed that the copper aluminide coating is worn away and that the nickel aluminide coating remains intact up to the end of the test. The reference coatings revealed negligible wear with the material transfer from the pin to their surface. The copper aluminide coating demonstrated the least friction coefficient among the entire evaluated coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. S. Ozturk, M. Merih Arikan, and Y. Kacar, Effects of Nickel Coating of Mold Plates on Star Crack Defects, Met. Mat. Trans., 2013, 44B, p 706–71010.1007/s11663-013-9821-0 ↗
2. S. Barella, A. Gruttadauria, C. Mapelli, and D. Mombelli, Investigation of Failure and Damages on a Continuous Casting Copper Mould, Eng. Fail. Anal., 2014, 36, p 432–43810.1016/j.engfailanal.2013.11.004 ↗
3. Z.D. Xiang and P.K. Datta, Relationship Between Pack Chemistry and Aluminide Coating Formation for Low-Temperature Aluminisation of Alloy Steels, Acta Mater., 2006, 54, p 4453–446310.1016/j.actamat.2006.05.032 ↗
4. Y.Q. Wang, Y. Zhang, and D.A. Wilson, Formation of Aluminide Coatings on Ferritic-Martensitic Steels by a Low-Temperature Pack Cementation Process, Surf. Coat. Technol., 2010, 204, p 2737–274410.1016/j.surfcoat.2010.02.025 ↗
5. T. Yener, Low Temperature Aluminising of Fe-Cr-Ni Super Alloy by Pack Cementation, Vacuum, 2019, 162, p 114–12010.1016/j.vacuum.2019.01.040 ↗
6. P.S. Chauhan, A. Choubey, Z. Wei Zhong, and M.G. Pecht, Copper Wire Bonding, Springer, New York, 201410.1007/978-1-4614-5761-9 ↗
7. Y. Terada, K. Ohkubo, T. Mohri, and T. Suzuki, Thermal Conductivity of Intermetallic Compounds with Metallic Bonding, Mater. Trans., 2002, 43, p 3167–317610.2320/matertrans.43.3167 ↗
8. H. Wang, T. Webb, and J.W. Bitler, Study of Thermal Expansion and Thermal Conductivity of Cemented WC-Co Composite, Int. J. Refract. Met. Hard, 2015, 49, p 170–17710.1016/j.ijrmhm.2014.06.009 ↗
9. A. Sanz, Tribological Behavior of Coatings for Continuous Casting of Steel, Surf. Coat. Technol., 2001, 146–147, p 55–6410.1016/S0257-8972(01)01475-X ↗
10. G.C. Rego, G.S. Takeya, A.N. Lombardi, G.E. Totten, and L.C. Castelet, Production of Aluminide Layers on Copper and Copper Alloy, Mater. Perform. Charact., 2016, 5, p 485–49610.1520/MPC20150068 ↗
11. J. Joseph and D.M. Fabijanic, Characterization and Tribological Performance of Cu-Based Intermetallic Layers, Key Eng. Mater., 2012, 533, p 195–20010.4028/www.scientific.net/KEM.533.195 ↗
12. K.T. Chiang, K.J. Kallenborn, and J.L. Yuen, Aluminization of Copper for Oxidation Protection, Surf. Coat. Technol., 1992, 52, p 135–13910.1016/0257-8972(92)90038-C ↗
13. K. Ishida and T. Nishizawa, The C-Co (Carbon-Cobalt) System, J. Phase Equilib., 1991, 12, p 417–42410.1007/BF02645959 ↗
14. I.V. Samarasekera, D.L. Anderson, and J.K. Brimacombe, The Thermal Distortion of Continuous-Casting Billet Molds, Mater. Trans., 1982, 13B, p p91–104
15. A. Luese and S.R. Sivrikova, Comprehensive Approach to Choice of CBCM Mold Coating, Metallurgist, 2013, 56, p 819–82510.1007/s11015-013-9657-5 ↗
16. V.V. Sobolev, J.M. Guilemany, and J. Nutting, High Velocity Oxy-Fuel Spraying: Theory. Structure-Property Relationships and Applications, Maney Publishing, London, 2004