Effect of heating and cooling regimes on residual strength and microstructure of normal strength and high-performance concrete
Source abstract
Abstract
Abstract A research program was carried out to investigate the residual compressive strength of high-performance concrete (HPC) and normal strength concrete (NSC) after they were exposed to high temperatures, 800°C and 1100°C, and two cooling regimes. Test results obtained showed that compared with the strength at room temperature, the residual strength of both HPC and NSC dropped sharply after exposure to high temperatures. Water cooling, which resulted in a significant thermal shock, caused a bit more severe deterioration in strength compared to furnace cooling. Thermal shock was not necessarily the primary cause for spalling in HPC. Mercury intrusion porosimetry tests were carried out to measure variation in the pore structure of concrete. Significant changes in the cumulative pore volume curves before and after high temperatures in both NSC and HPC were observed. The cumulative pore volume of HPC increased more remarkably than that of NSC. The difference between the effects of the two cooling regimes on mechanical property as well as the microstructure decreased at 1100°C when compared 800°C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Engineering and Material Science Research · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. High performance concrete — an overview10.1007/BF02486473 ↗
2. Influence of silica fume on the workability and the compressive strength of high-performance concretes10.1016/S0008-8846(98)00010-6 ↗
3. Diederichs · 1988
4. Mechanical properties of high strength concrete at high temperatures
5. Spalling of high-strength silica fume concrete in fire
6. An analytical approach for investigating the causes of spalling of high-strength concrete at elevated temperatures
7. Khoylou · 1996 · 263
8. Effect of transient high temperature on high-strength concrete
9. Material and environmental factors influencing the compressive strength of unsealed cement paste and concrete at high temperatures10.1680/macr.1993.45.162.51 ↗
10. Comparison between high strength concrete and normal strength concrete subjected to high temperature10.1007/BF02485969 ↗
11. Effects of high temperature on the residual compressive strength of high-strength siliceous concretes
12. Compressive strength and pore structure of high performance concrete after exposure to high temperature up to 800°C10.1016/S0008-8846(99)00240-9 ↗
13. Fire resistance of hollow steel columns filled with steel fibre-reinforced concrete
14. Schneider · 1985
15. Effect of microstructure on the mechanical and thermal properties of lightweight concrete prepared from clay, cement, and wood aggregates10.1016/S0008-8846(98)00075-1 ↗