Clinkerless ultra-high strength concrete based on alkali-activated slag at high temperatures
Source abstract
Abstract
Abstract This work investigates the degradation mechanisms of clinkerless alkali-activated slag based ultra-high strength concrete (AAS-UHSC) upon exposure to high temperatures up to 800 °C. The heat-induced mechanical, mineralogical, molecular, microstructural, and pore structure alterations of AAS-UHSC prepared with various activator types, water-to-powder ratios, and fiber incorporation are studied. The results demonstrate the beneficial roles of potassium incorporation on improving the thermal stability and integrity of AAS-UHSC, via suppressing deleterious crystallization and transformation of aluminosilicate phases at high temperature. In contrast to Portland cement clinker-based UHSC, no sign of explosive spalling is observed in AAS-UHSC, likely due to the presence of microcracks that enhance the pore network connectivity. The mechanical degradation of AAS-UHSC at high temperature below 600 °C is resulted from dehydration and decomposition of phases and consecutive thermal cracking, together with enlarged porosity and coarsened pore structure. As the temperature rising to 800 °C, crystallization and transformation of phases, as well as formation of porous microstructure, considerably aggravate the mechanical degradation of AAS-UHSC. In contrast to the thermal damage mitigation by polymeric fibers in conventional UHSC, the fiber incorporation has little positive impact on the thermal resistance of AAS-UHSC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Fire effects on concrete materials · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Alkali-activated slag cement concrete
2. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
3. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
4. Comparative life cycle assessment of conventional, glass powder, and alkali-activated slag concrete and mortar10.1061/(ASCE)IS.1943-555X.0000211 ↗
5. Sequestration and release of nitrite and nitrate in alkali-activated slag: a route toward smart corrosion control10.1016/j.cemconres.2021.106398 ↗
6. Mechanism of sulfate attack on alkali-activated slag: the role of activator composition10.1016/j.cemconres.2019.105868 ↗
7. Resistance of alkali-activated slag concrete to chloride-induced corrosion10.1155/2015/273101 ↗
8. Electrochemical performance of reinforcing steel in alkali-activated slag extract in the presence of chlorides10.1016/j.corsci.2018.01.043 ↗
9. Chemical and mechanical stability of sodium sulfate activated slag after exposure to elevated temperature10.1016/j.cemconres.2011.10.007 ↗
10. Residual strength properties of sodium silicate alkali activated slag paste exposed to elevated temperatures10.1617/s11527-009-9546-3 ↗
11. Resistance of alkali-activated slag mortar to abrasion and fire10.1680/adcr.2011.23.6.289 ↗
12. Studies on high performance alkali activated slag concrete mixes subjected to aggressive environments and sustained elevated temperatures10.1016/j.conbuildmat.2019.116887 ↗
13. Phase transformations and mechanical strength of OPC/Slag pastes submitted to high temperatures10.1617/s11527-007-9247-8 ↗
14. Dehydration kinetics of Portland cement paste at high temperature10.1007/s10973-012-2303-9 ↗
15. Behaviour of cement concrete at high temperature
16. Physicochemical properties of binder gel in alkali-activated fly ash/slag exposed to high temperatures10.1016/j.cemconres.2016.08.004 ↗
17. Microstructural alteration of alkali activated slag mortars depend on exposed high temperature level10.1016/j.conbuildmat.2015.12.070 ↗
18. Compressive strength and microstructure of alkali-activated fly ash/slag binders at high temperature10.1016/j.cemconcomp.2017.09.011 ↗
19. Characterization of alkali activated slag paste after exposure to high temperatures10.1016/j.conbuildmat.2013.06.070 ↗
20. Thermal properties of alkali-activated slag subjected to high temperatures10.1177/1744259106075234 ↗
21. Comparative performance of alkali activated slag/metakaolin cement pastes exposed to high temperatures10.1016/j.cemconcomp.2017.09.007 ↗
22. Influence of silica fume on properties of fresh and hardened ultra-high performance concrete based on alkali-activated slag10.1016/j.cemconcomp.2019.03.023 ↗
23. The effect of fiber properties on high performance alkali-activated slag/silica fume mortars10.1016/j.compositesb.2012.09.080 ↗
24. High temperature resistance of alkali-activated slag-and portland cement-based reactive powder concrete
25. Development of ultra-high-performance geopolymer concrete10.1680/macr.13.00057 ↗
26. Development of ultra-high performance geopolymer concrete (UHPGC): influence of steel fiber on mechanical properties
27. Compressive strength and pore structure of high-performance concrete after exposure to high temperature up to 800 C10.1016/S0008-8846(99)00240-9 ↗
28. Effect of transient high temperature on high-strength concrete
29. High-strength self-compacting concrete exposed to fire test10.1061/(ASCE)0899-1561(2006)18:6(754) ↗
30. High temperature and residual properties of reactive powder concrete–a review10.1016/j.conbuildmat.2017.04.083 ↗
31. A new perspective on nature of fire-induced spalling in concrete10.1016/j.conbuildmat.2018.06.204 ↗
32. High-temperature behaviour of HPC with polypropylene fibres: from spalling to microstructure10.1016/S0008-8846(01)00596-8 ↗
33. How do polypropylene fibers improve the spalling behavior of in-situ concrete?10.1016/j.cemconres.2005.12.018 ↗
34. Limits of spalling of fire-exposed concrete10.1016/S0379-7112(02)00051-6 ↗
35. Microstructural investigation of calcium aluminate cement-based ultra-high performance concrete (UHPC) exposed to high temperatures10.1016/j.cemconres.2017.09.004 ↗
36. Effect of various polymer fibers on spalling mitigation of ultra-high performance concrete at high temperature10.1016/j.cemconcomp.2020.103815 ↗
37. Effect of spatial distribution of polymer fibers on preventing spalling of UHPC at high temperatures10.1016/j.cemconres.2020.106281 ↗
38. “Metakaolin-slag-clinker blends.” The role of Na+ or K+ as alkaline activators of theses ternary blends10.1111/jace.12272 ↗
39. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
40. Alkali cation effects on chloride binding of alkali-activated fly ash and metakaolin geopolymers10.1016/j.cemconcomp.2020.103721 ↗
41. Dispersion of fibers in ultra-high-performance concrete
42. Ultra-high performance concrete with compressive strength exceeding 150 MPa (22 ksi): a simpler way
43. Fehling · 2015
44. Influence of dolomite on the properties and microstructure of alkali-activated slag with and without pulverized fly ash10.1016/j.cemconcomp.2019.05.011 ↗
45. Incorporation of micro-cracking and fibre bridging mechanisms in constitutive modelling of fibre reinforced concrete10.1016/j.jmps.2019.103732 ↗
46. Tensile performance of sustainable strain-hardening cementitious composites with hybrid PVA and recycled PET fibers10.1016/j.cemconres.2018.02.013 ↗
47. Role of carbonates in the chemical evolution of sodium carbonate-activated slag binders10.1617/s11527-014-0412-6 ↗
48. Influence of binder composition on the gel structure in alkali activated fly ash/slag pastes exposed to elevated temperatures10.1016/j.ceramint.2016.11.042 ↗
49. Structure of calcium silicate hydrate (C-S-H): near-, mid-, and far-infrared spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
50. Effect of alkalis on fresh C–S–H gels. FTIR analysis10.1016/j.cemconres.2009.01.003 ↗
51. Infrared and Raman spectral studies in cement and concrete10.1016/0008-8846(80)90005-8 ↗
52. Shrinkage mechanisms of alkali-activated slag10.1016/j.cemconres.2016.07.001 ↗
53. Understanding the drying shrinkage performance of alkali-activated slag mortars10.1016/j.cemconcomp.2016.11.010 ↗
54. Spalling prevention of ultra-high performance concrete: comparative effectiveness of polyethylene terephthalate and polypropylene fibers10.1061/(ASCE)MT.1943-5533.0003980 ↗