journal article·2015-01

Nano-chemo-mechanical signature of conventional oil-well cement systems: Effects of elevated temperature and curing time

Konrad J. Krakowiak, Jeffrey J. Thomas, Simone Musso, Simon James, Ange-Therese Akono, Franz-Josef Ulm

Publisher page

Abstract

Abstract With ever more challenging (T,p) environments for cementing applications in oil and gas wells, there is a need to identify the fundamental mechanisms of fracture resistant oil well cements. We report results from a multi-technique investigation of behavior and properties of API class G cement and silica-enriched cement systems subjected to hydrothermal curing from 30 °C to 200 °C; including electron probe microanalysis, X-ray diffraction, thermogravimetry analysis, electron microscopy, neutron scattering (SANS), and fracture scratch testing. The results provide a new insight into the link between system chemistry, micro-texture and micro-fracture toughness. We suggest that the strong correlation found between chemically modulated specific surface and fracture resistance can explain the drop in fracture properties of neat oil-well cements at elevated temperatures; the fracture property enhancement in silica-rich cement systems, between 110° and 175 °C; and the drop in fracture properties of such systems through prolonged curing over 1 year at 200 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Drilling and Well Engineering · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (83)

Show source-provided references
1. Nelson · 2006
2. 2013
3. The derivation of kinetic parameters on analysis of Portland cement for portlandite and carbonate by thermogravimetry
4. Russ · 2006
5. The surface area of hardened cement paste as measured by various techniques
6. Composition and density of nanoscale calcium–silicate–hydrate in cement10.1038/nmat1871 ↗
7. Relationships between composition and density of tobermorite, jennite, and nanoscale CaO–SiO2–H2O10.1021/jp910733x ↗
8. Density and water content of nanoscale solid C–S–H formed in alkali-activated slag (AAS) paste and implications for chemical shrinkage10.1016/j.cemconres.2011.11.003 ↗
9. Adsorption of gases in multimolecular layers10.1021/ja01269a023 ↗
10. Experimental determination of the fracture toughness via microscratch tests: application to polymers, ceramics, and metals10.1557/jmr.2011.402 ↗
11. “Surface roughness criteria for cement paste nanoindentation”10.1016/j.cemconres.2007.11.014 ↗
12. CITZAF — a package of correction programs for the quantitative electron microbeam X-ray analysis of thick polished materials, thinfilms, and particles
13. Heinrich · 1991
14. Goldstein · 2008
15. Taylor · 1997
16. Maximum likelihood from incomplete data via the EM algorithm10.1111/j.2517-6161.1977.tb01600.x ↗
17. McLachlan · 200010.1002/0471721182 ↗
18. A model for two types of calcium silicate hydrate in the microstructure of Portland cement pastes10.1016/S0008-8846(00)00257-X ↗
19. The steam curing of Portland cement products
20. The hydration of tricalcium and β-dicalcium silicates in pastes under normal and steam curing conditions10.1002/jctb.5010090306 ↗
21. High-temperature curing of concrete under high pressure
22. Monte Carlo simulation of electron–solid interactions in cement-based materials10.1016/j.cemconres.2006.03.006 ↗
23. Abuhaikal · 2011
24. An electron microprobe study of a mature cement paste10.1016/0008-8846(84)90134-0 ↗
25. Chemistry of cement hydration
26. CaO/SiO2 mole ratio of calcium silicate hydrate in fully hydrated tricalcium silicate paste10.1016/0008-8846(80)90006-X ↗
27. Estimating the dimension of the model
28. Optimizing the electron microprobe analysis of hydrous alkali aluminosilicate glasses10.2138/am-1996-9-1016 ↗
29. Analysis of oxygen with the electron microprobe: Applications to hydrated glass and minerals
30. Microstructure and microanalysis of hardened ordinary Portland cement pastes10.1007/BF00349061 ↗
31. The calcium silicate hydrates
32. Stability and phase relations of dicalcium silicate hydrates under hydrothermal conditions10.2109/jcersj.114.174 ↗
33. Phase studies of pozzolanic stabilized calcium silicate hydrates at 180°C10.1016/j.cemconres.2004.05.021 ↗
34. Thermal decomposition of ettringite Ca6[Al(OH)6]2(SO4)3·26H2O10.1039/FT9969202125 ↗
35. C4A3 S¯ hydration ettringite formation, and its expansion mechanism: I. Expansion; ettringite stability10.1016/0008-8846(81)90032-6 ↗
36. Thermodynamic investigation of the CaO-Al2O3-CaSO4-H2O system at 50°C and 85°C10.1016/0008-8846(92)90047-Y ↗
37. Chemical composition of cement pore solutions10.1016/0008-8846(89)90022-7 ↗
38. Effect of temperature on the pore solution, microstructure and hydration products of Portland cement pastes10.1016/j.cemconres.2006.11.016 ↗
39. Effect of temperature on the hydration of the main clinker phases in Portland cements: Part I, neat cements10.1016/S0008-8846(98)00115-X ↗
40. Composition, morphology and microstructure of C–S–H in white Portland cement pastes hydrated at 55°C10.1016/j.cemconres.2007.09.001 ↗
41. Christensen · J. Solid State Chem. · 2004 · 177 · 194410.1016/j.jssc.2003.12.030 ↗
42. Impact of prolonged warm (85°C) moist cure on Portland cement paste10.1016/S0008-8846(00)00286-6 ↗
43. The reactions of cement hydration at elevated temperatures
44. Prolonged hydrothermal treatment of cement mixes, I. Curing in water under saturated steam pressure at 140-170°C
45. Prolonged hydrothermal treatment of cement mixes, II. Curing under saturated steam pressure followed by treatment in superheated steam
46. Quantitative phase compositions of autoclaved cement-quartz cubes10.1016/0008-8846(72)90070-1 ↗
47. A transmission electron study on the decomposition of synthetic hillebrandite (Ca2SiO4∙H2O)10.1557/JMR.1995.3084 ↗
48. Thermal decomposition of α-dicalcium silicate hydrate10.1016/0040-6031(77)85079-X ↗
49. Low-temperature synthesis of β-Ca2SiO4 from hillebrandite10.1111/j.1151-2916.1992.tb05595.x ↗
50. Quantitative study of Portland cement hydration by X-ray diffraction/Rietveld analysis and independent methods10.1016/j.cemconres.2004.04.014 ↗
51. Critical examination of drying damage to cement pastes10.1680/adcr.2000.12.2.79 ↗
52. Changes in crystal structure of ettringite on dehydration. 110.1016/0008-8846(75)90093-9 ↗
53. Changes in crystal structure of ettringite on dehydration. 210.1016/0008-8846(75)90017-4 ↗
54. Structural changes during thermal dehydration of ettringite10.1680/adcr.2001.13.2.77 ↗
55. Contribution of analysis by means of an electron microprobe to the cement chemistry
56. Electron microprobe studies of the hydration of 3CaO.SiO210.1038/223492a0 ↗
57. Calcium hydroxide distribution and calcium silicate hydrate composition in tricalcium silicate and β-dicalcium silicate pastes10.1016/0008-8846(84)90084-X ↗
58. Hydrothermal formation of calcium silicate hydrates10.1111/j.1151-2916.1965.tb14673.x ↗
59. Xonotlite: cell parameters, thermogravimetry and analytical electron microscopy10.1016/0008-8846(77)90093-X ↗
60. The calcium silicate hydrates10.1016/j.cemconres.2007.11.005 ↗
61. Backscattered electron imaging of cement pastes hydrated at different temperatures10.1016/0008-8846(90)90085-C ↗
62. A multi-technique investigation of the nanoporosity of cement paste10.1016/j.cemconres.2006.03.021 ↗
63. Permeability and elastic modulus of cement paste as a function of curing temperature10.1016/j.cemconres.2011.11.012 ↗
64. Mindess · 2002
65. Fracture toughness of cement-based materials10.1007/BF02472850 ↗
66. The scratch test for strength and fracture toughness determination of oil well cements cured at high temperature and pressure10.1016/j.cemconres.2011.04.014 ↗
67. Theory of rock cutting10.1007/BF01525361 ↗
68. The Scratch Test as a Means to Measure Strength of Sedimentary Rocks
69. Scratching as a fracture process: from butter to steel
70. Scratch test model for the determination of fracture toughness10.1016/j.engfracmech.2010.09.017 ↗
71. Rock strength determination from scratch tests10.1016/j.enggeo.2012.07.011 ↗
72. Can scratch tests give fracture toughness?10.1016/j.engfracmech.2013.06.002 ↗
73. Discussion: Strength-to-Fracture Scaling in Scratching10.1016/j.engfracmech.2014.02.025 ↗
74. Strength and volume change of steam cured concrete
75. Strength and volume change of steam-cured Portland cement mortar and concrete
76. Long-term effects of high temperature on strength retrogression of cements
77. A realistic molecular model of cement hydrates10.1073/pnas.0902180106 ↗
78. Confined water dissociation in the microporous defective silicates: mechanism, dipole distribution, and impact on substrate properties10.1021/ja209152n ↗
79. Manzano · 2009
80. Hydrothermal processing of xonotlite based compositions10.1179/174367607X228124 ↗
81. Structure, bonding and morphology of hydrothermally synthesised xonotlite10.1179/174367608X353638 ↗
82. Hydrothermal synthesis and characterization of aluminum and sulfate substituted 1.1nm tobermorites10.1016/j.jallcom.2007.11.130 ↗
83. Hydrothermal synthesis of aluminum substituted tobermorite by using various crystal phases of alumina10.2109/jcersj2.119.375 ↗