Formation of carbonate phases and their effect on the performance of reactive MgO cement formulations

N.T. Dung, A. Lesimple, R. Hay, K. Celik, C. Unluer

Abstract

This study investigated the formation of different phases and their influence on the microstructural and mechanical development of carbonated reactive MgO cement formulations. Hydrated magnesium carbonates (HMCs) were identified and quantified via XRD, TG-DTG and SEM. Visual observations of the 3D internal structure at different depths were performed by X-ray computed tomography and confocal Raman microscopy. Elastic modulus of different components was obtained by nano-indentation. The expansive formation of HMCs led to dense microstructures composed of well-connected carbonate networks. The transition of artinite to hydromagnesite/nesquehonite was observed over time. The initial formation of a dense carbonate layer on sample surface inhibited continuous diffusion of CO2, resulting in a slower strength development at later ages. Despite this limitation, the continuation of hydration and evolution of carbonate morphology led to 28-day strengths of 60 MPa in concrete samples, supported by the higher elastic modulus of HMCs than brucite (19.4 vs. 2.5 GPa).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Oxide Properties and Applications · Concrete and Cement Materials Research · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Ultra-green construction: reactive magnesia masonry products10.1680/warm.2009.162.4.185 ↗
2. Performance of magnesia cements in porous blocks in acid and magnesium environments10.1680/adcr.11.00011 ↗
3. Impact of hydrated magnesium carbonate additives on the carbonation of reactive MgO cements10.1016/j.cemconres.2013.08.009 ↗
4. Harrison · 2008
5. Scaled-up commercial production of reactive magnesium cement pressed masonry units. Part I: production10.1680/coma.10.00032 ↗
6. Influence of carbonation on the properties of reactive magnesia cement-based pressed masonry units10.1680/adcr.2008.20.2.53 ↗
7. Scaled-up commercial production of reactive magnesia cement pressed masonry units. Part II: performance10.1680/coma.10.00031 ↗
8. Ab initio thermodynamic model for magnesium carbonates and hydrates10.1021/jp500271n ↗
9. Accelerated carbonation of reactive MgO cements10.1680/adcr.2007.19.2.67 ↗
10. Carbonated MgO concrete with improved performance: the influence of temperature and hydration agent on hydration, carbonation and strength gain10.1016/j.cemconcomp.2017.06.006 ↗
11. Development of MgO concrete with enhanced hydration and carbonation mechanisms10.1016/j.cemconres.2017.10.011 ↗
12. Sequestration of CO2 in reactive MgO cement-based mixes with enhanced hydration mechanisms10.1016/j.conbuildmat.2017.03.038 ↗
13. Influence of mix design on the carbonation, mechanical properties and microstructure of reactive MgO cement-based concrete10.1016/j.cemconcomp.2017.03.004 ↗
14. Enhancing the carbonation of MgO cement porous blocks through improved curing conditions10.1016/j.cemconres.2014.02.005 ↗
15. Accelerated carbonation of brucite in mine tailings for carbon sequestration10.1021/es3012854 ↗
16. Improving the performance of reactive MgO cement-based concrete mixes10.1016/j.conbuildmat.2016.09.090 ↗
17. Influence of nucleation seeding on the performance of carbonated MgO formulations10.1016/j.cemconcomp.2017.07.005 ↗
18. Improving the carbonation of reactive MgO cement concrete via the use of NaHCO3 and NaCl10.1061/(ASCE)MT.1943-5533.0002509 ↗
19. Investigation of carbonation depth and its influence on the performance and microstructure of MgO cement and PC mixes10.1016/j.conbuildmat.2016.05.067 ↗
20. Performance of reactive MgO concrete under increased CO2 dissolution10.1016/j.cemconres.2019.02.007 ↗
21. Pore-scale modelling of relative permeability of cementitious materials using X-ray computed microtomography images10.1016/j.cemconres.2017.02.005 ↗
22. Investigation of self-sealing in high-strength and ultra-low-permeability concrete in water using micro-focus X-ray CT10.1016/j.cemconres.2012.08.014 ↗
23. Monitoring reinforcement corrosion and corrosion-induced cracking by X-ray microcomputed tomography method10.1016/j.cemconres.2017.07.009 ↗
24. Characterization of carbon nanoparticles in thin-film nanocomposites by confocal Raman microscopy10.1021/jp502403r ↗
25. New insights in weathering analysis of anhydrous cements by using high spectral and spatial resolution confocal raman microscopy10.1016/j.cemconres.2017.06.003 ↗
26. Confocal Raman microscopy as a non-destructive tool to study microstructure of hydrating cementitious materials10.1016/j.cemconres.2016.07.005 ↗
27. The micromechanical signature of high-volume natural pozzolan concrete by combined statistical nanoindentation and SEM-EDS analyses10.1016/j.cemconres.2016.10.004 ↗
28. Micromechanics-based investigation of the elastic properties of polymer-modified cementitious materials using nanoindentation and semi-analytical modeling10.1016/j.cemconcomp.2018.01.010 ↗
29. Shand · 2006
30. Characterisation of different commercial reactive magnesia10.1680/adcr.13.00004 ↗
31. Surface roughness criteria for cement paste nanoindentation10.1016/j.cemconres.2007.11.014 ↗
32. The effect of two types of C-S-H on the elasticity of cement-based materials: results from nanoindentation and micromechanical modeling10.1016/S0008-8846(03)00230-8 ↗
33. The nanogranular nature of C–S–H10.1016/j.jmps.2006.06.003 ↗
34. Influence of accelerated hydration and carbonation on the performance of reactive magnesium oxide concrete
35. The mechanism of hydration of MgO-hydromagnesite blends10.1016/j.cemconres.2017.10.003 ↗
36. Controlled rate thermal analysis of hydromagnesite10.1007/s10973-007-8845-6 ↗
37. The thermal decomposition of huntite and hydromagnesite—a review10.1016/j.tca.2010.06.012 ↗
38. Infrared and infrared emission spectroscopy of nesquehonite Mg(OH)(HCO3)· 2H2O–implications for the formula of nesquehonite10.1016/j.saa.2010.12.059 ↗
39. On the thermal decomposition of nesquehonite10.1007/s10973-015-4756-0 ↗
40. Synthesis of magnesium oxide hierarchical microspheres: a dual-functional material for water remediation10.1021/acsami.5b05553 ↗
41. The thermal behaviour and structural stability of nesquehonite, MgCO3·3H2O, evaluated by in situ laboratory parallel-beam X-ray powder diffraction: new constraints on CO2 sequestration within minerals10.1016/j.jhazmat.2010.01.113 ↗
42. Thermal stability of artinite, dypingite and brugnatellite—implications for the geosequestration of green house gases10.1016/j.tca.2008.06.007 ↗
43. Autogenous healing of fiber-reinforced reactive magnesia-based tensile strain-hardening composites10.1016/j.cemconres.2018.09.016 ↗
44. The use of microbial induced carbonate precipitation in healing cracks within reactive magnesia cement-based blends10.1016/j.cemconres.2018.10.018 ↗
45. Properties of binary and ternary reactive MgO mortar blends subjected to CO2 curing10.1016/j.cemconcomp.2013.03.009 ↗
46. Nano-mechanical characterization of synthetic calcium–silicate–hydrate (C–S–H) with varying CaO/SiO2 mixture ratios10.1016/j.cemconcomp.2012.10.001 ↗