journal article·2022-03

Effects of Solution Heat Treatment Temperatures on Microstructures and Mechanical Properties of SP-700 Ti Alloys

Yang-Chun Chiu, Jun-Hao Chen, Sheng-Long Lee

Publisher page

Abstract

The aim of this study is to explore the effects of solution heat treatment temperatures on the microstructures and mechanical properties of water-quenched SP-700 Ti alloys. The main objective is to determine whether the tensile strength and ductility of the SP-700 Ti alloys conform to the quality requirements of armor materials for aircraft, spacecraft, other transportation vehicles, sporting goods, and turbine blades. Therefore, we have experimented with different solution heat treatment temperatures in order to obtain alloys with more excellent tensile strength and ductility. The results showed that after SP-700 Ti alloys (β transus temperatures is 900°C) were subjected to solution heat treatment and then quenched with water, the microstructures of the high-temperature single-phase region (950°C and 900°C) were composed of the soft residual βr base phase and distributed, hard, and brittle needle-like α" martensite phase. The tensile strength and ductility of this material were not good. In the comparatively lower-temperature dual-phase region (750°C), the microstructure of the water-quenched alloy was composed of a residual β base phase and a pro-eutectoid α phase. Because no martensite phase occurred in the alloy, we observed no obvious work hardening characteristics. However, it exhibited the highest impact toughness and hardness of all the fabricated materials. By contrast, in the high-temperature dual-phase region (850°C and 800°C), because the room temperature was still between the martensite start (Ms) and martensite finish (Mf) temperatures, the microstructures of the alloys were composed of the softer βr base phase, hard brittle pro-eutectoid α phase (αp) and α" martensite phase. With the “stress-induced martensite phase transformation” that occurred during the tensile test, the SP-700 Ti alloys experienced a high strength increase and high ductility characteristics. Especially, when the solution heat treatment temperature was 800°C, the alloy had the highest strength and ductility, and therefore best met the requirements of armor material standards (MIL-DTL-46077).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. C. Ouchi, H. Fukai and K. Hasegawa, Microstructural Characteristic and Unique Properties Obtained By Solution Treating or Aging in β-Rich α+β Titanium Alloy, Mater. Sci. Eng. A, 1999, 263, p 132–136.10.1016/S0921-5093(98)01171-X ↗
2. P. Mengucci, A. Gatto, E. Bassoli, L. Denti, F. Fiori, E. Girardin, P. Bastianoni, B. Rutkowski, A. Czyrska-Filemonowicz and G. Barucca, Effects of Build Orientation and Element Partitioning on Microstructure and Mechanical Properties of Biomedical Ti-6Al-4V Alloy Produced by Laser Sintering, J. Mech. Behav. Biomed. Mater., 2017, 71, p 1–9.10.1016/j.jmbbm.2017.02.025 ↗
3. F.H. Froes and I.L. Caplan, Titanium 92: Science and Technology, Titan. Comm. Miner. Metals Mater. Struct., 1993, 2, p 141.
4. P. Parvizian, M. Morakabati and S. Sadeghpour, Effect of Hot Rolling and Annealing Temperatures on the Microstructure and Mechanical Properties of SP-700 Alloy, Int. J. Miner. Metall. Mater., 2020, 27, p 374–383.10.1007/s12613-019-1922-6 ↗
5. C.R. Brooks, Heat Treatment, Structure and Properties of Non Ferrous Alloys, ASM International, Metals Park (Ohio), 1982, p 329
6. R. Boyer, E.W. Collings and G. Welsch, Materials Properties Handbook: Titanium Alloys, ASM International, Netherlands, 1994, p 11
7. B. Gunawaram and M. Ninomi, Effect of β Phase Stability at Room Temperature on Mechanical Properties in β-Rich α+β Type Ti-4.5Al-3V-2Mo-2Fe Alloy, ISIJ Int., 2002, 42, p 191–199.10.2355/isijinternational.42.191 ↗
8. Y.L. Kao, G.C. Tu, C.A. Huang and T.T. Liu, A Study on the Hardness Variation of α- and β-Pure Titanium with Different Grain Sizes, Mater. Sci. Eng. A, 2005, 398, p 93–98.10.1016/j.msea.2005.03.004 ↗
9. N. Gey, P. Bocher, E. Uta, L. Germain and M. Humbert, Texture and Microtexture Variations in a Near-α Titanium Forged Disk of Bimodal Microstructure, Acta Mater., 2012, 60, p 2647–2655.10.1016/j.actamat.2012.01.031 ↗
10. T. Grosdidier and M.J. Philippe, Deformation Induced Martensite and Superelasticity in a β-Metastable Titanium Alloy, Mater. Sci. Eng. A, 2000, 291, p 218–223.10.1016/S0921-5093(00)00921-7 ↗
11. L. Meng, T. Kitashima, T. Tsuchiyama and M. Watanabe, Effect of α Precipitation on β Texture Evolution During β-Processed Forging in a Near-β Titanium Alloy, Mater. Sci. Eng. A, 2020, 771, p 138640.10.1016/j.msea.2019.138640 ↗
12. S. Shekhar, R. Sarkar, S.K. Kar and A. Bhattacharjee, Effect of Solution Treatment and Aging on Microstructure and Tensile Properties of High Strength β Titanium Alloy, Ti-5Al-5V-5Mo-3Cr, Mater. Des., 2015, 66, p 596–610.10.1016/j.matdes.2014.04.015 ↗
13. R.E. Reed-Hill and R. Abbaschian, Physical Metallurgy Principles, PWS Publishing Company, Boston, 1994, p 579
14. J.K. Nieh, C.T. Wu, Y.L. Chen, C.N. Wei and S.L. Lee, Effect of Cooling Rate During Solution Heat Treatment on the Microstructure and Mechanical Properties of sp-700 Titanium Alloys, J. Mar. Sci. Technol., 2016, 24, p 99–106.
15. B. Gunawarman, M. Niinomi, T. Akahori, J. Takeda and H. Toda, Mechanical Properties of Ti–4.5Al–3V–2Mo–2Fe and Possibility for Healthcare Applications, Mater. Sci. Eng. C, 2005, 25, p 296–303.10.1016/j.msec.2004.12.012 ↗
16. C. Huang, Y. Zhao, S. Xin, W. Zhou, Q. Li and W. Zeng, Effect of Microstructure on Tensile Properties of Ti-Al-5Mo-5V-3Cr-1Zr Alloy, J. Alloys Compd., 2017, 693, p 582–591.10.1016/j.jallcom.2016.09.233 ↗
17. Z. Du, S. Xiao, L. Xu, J. Tian, F. Kong and Y. Chen, Effect of Heat Treatment on Microstructure and Mechanical Properties of a New β High Strength Titanium Alloy, Mater. Des., 2014, 55, p 183–190.10.1016/j.matdes.2013.09.070 ↗
18. “Detail specification: armor plate, Titanium alloy”, MIL-DTL-46077F, Weldable (29-DEC-1998) [SUPERSEDING MIL-A- 46077E].
19. “Standard Test Methods for Tension Testing of Metallic Materials”, E8/E8M-11, ASTM, 2011, pp. 1-30.
20. “Standard Test Methods for Notched Bar Impact Testing of Metallic Materials”, E23-12C, ASTM, 2012, pp.1-25.
21. W.D. Brewer, R.K. Bird and T.A. Wallace, Titanium Alloys and Processing for High Speed Aircraft, Mater. Sci. Eng. A, 1998, 243, p 299–304.10.1016/S0921-5093(97)00818-6 ↗
22. D. Banerjee and J.C. Williams, Perspectives on Titanium Science and Technology, Acta Metall., 2013, 61(3), p 844–879.
23. G. Singh and U. Ramamurty, Boron Modified Titanium Alloys, Prog. Mater. Sci., 2020, 111, p 1006553.10.1016/j.pmatsci.2020.100653 ↗
24. T.W. Duerig, J. Albrecht, D. Richter and P. Fischer, Formation and Reversion of Stress Induced Martensite in Ti-10V-2Fe-3Al, Acta Metall., 1982, 30–12, p 2161–2172.10.1016/0001-6160(82)90137-7 ↗
25. A. Dasm and S. Tarafder, Geometry of Dimples and its Correlation with Mechanical Properties in Austenitic Stainless Steel, Scr. Mater., 2008, 59–9, p 1014–1017.