Source abstract
Abstract
Abstract A petrographic examination of cracked Swedish concrete railroad ties identified delayed ettringite formation (DEF) as the damaging mechanism. This was unexpected because the concrete railroad ties were steam-cured with a maximum concrete temperature below 60 °C. The consensus in the published literature is that DEF only occurs in concrete subjected to heat curing above 70 °C. However, DEF is not only influenced by the curing temperature, but also by various other factors, such as cement composition (alkalis, C3S, C3A, SO3, and MgO), fineness, etc. If an unfavorable combination of these parameters exists, delayed ettringite may occur at lower temperatures than 70 °C. In this paper, the influence of various parameters on DEF is discussed with reference to the investigated concrete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. On the stability of calcium aluminate sulfate hydrates in pure system and in cements
2. Mechanism of subsequent ettringite formation in mortars and concretes after heat treatment
3. Delayed ettringite formation in heat treated mortars and concretes
4. C.D. Lawrence, Laboratory studies of concrete expansion arising from delayed ettringite formation, Technical Report C/16, British Cement Association, 1993.
5. Delayed ettringite formation: an issue?
6. Scrivener · 1996 · 375
7. Delayed ettringite formation: a microstructural and microanalytical study10.1680/adcr.1993.5.20.139 ↗
8. Simultaneous presence of alkali–silica gel and ettringite in concrete10.1680/adcr.1993.5.17.23 ↗
9. Effects of an early or late heat treatment on the microstructure and composition of inner C-S-H products of Portland cement mortars10.1016/S0008-8846(01)00670-6 ↗
10. Combined effects of alkali silica reaction and secondary ettringite deposition in steam cured mortars
11. Delayed ettringite formation and the mode of concrete failure
12. What causes delayed ettringite formation?
13. R.L. Day, The Effect of Secondary Ettringite Formation on the Durability of Concrete: A Literature Analysis, Research and Development Bulletin RD108T, PCA, Skokie, IL, 1992.
14. Delayed ettringite formation
15. Clinker sulfate: a cause for distress and a need for specification
16. Delayed ettringite formation—a concern for precast concrete?10.15554/pcij.07011996.26.30 ↗
17. Delayed ettringite formation—Process and problems10.1016/0958-9465(96)00017-0 ↗
18. Internal sulfate attack: distress mechanism at ambient and elevated temperatures? Ettringite—The sometimes host of destruction
19. Influence of cement composition on volume stability of mortar, ettringite—The sometimes host of destruction
20. The effect of cement composition and fineness on expansion associated with delayed ettringite formation10.1016/0958-9465(95)00013-5 ↗
21. Wieker · 1992 · 125
22. Expansion and cracking in concrete associated with delayed ettringite formation. Ettringite—The sometimes host of destruction
23. Microchemical effects of elevated temperature curing and delayed ettringite formation
24. Heat curing and delayed ettringite formation10.1557/PROC-370-67 ↗
25. Evolution of expansion, weight gain, microstructure, and microchemistry of DEF affected mortar
26. The stability of ettringite10.1680/adcr.1993.5.18.47 ↗
27. The role of sulfate mineralogy and cure temperature in delayed ettringite formation10.1016/0958-9465(96)00015-7 ↗
28. Delayed ettringite formation: the effect of temperature and basicity on the interaction of sulphate and C-S-H phase10.1016/S0008-8846(98)00006-4 ↗
29. The effect of water–cement ratio, sulphonated plasticizer and slica fume on delayed ettringite expansion, durability of high performance concrete
30. Studies on the delayed ettringite formation in heat-cured mortars: II. Characteristics of cement that may be susceptible to DEF10.1016/S0008-8846(02)00894-3 ↗