journal article·2003-08

Alkali mass balance during the accelerated concrete prism test for alkali–aggregate reactivity

Patrice Rivard, Marc-André Bérubé, Jean-Pierre Ollivier, Gérard Ballivy

Cement and Concrete Research· Volume 33· Issue 8
Publisher page

Abstract

The alkali mass balance was calculated in concrete specimens submitted to the storage conditions of the Canadian standard CSA A23.2-14A concrete prism test for expansion because of alkali-aggregate reaction (AAR). The alkali concentration of both the concrete pore solution expressed under high pressure and the water below specimens in storage pails (bottom water) was measured. Measurements were conducted over a 1-year period that corresponds to the length of the above test. Two reactive aggregates were testes [Potsdam sandstone (PO) and Spratt limestone (SP)]. Each aggregate was incorporated in two concrete mixtures (mass concrete and structural concrete), for a total of four batches. Significant alkali leaching occurred at 38 degrees centigrade while performing tests in high moisture storage conditions even though prisms were covered with plastic sleeves. After 52 weeks, the alkali loss ranged from 12% to 25% of the original Na(2)O(e) content of the concrete, depending on the mixture proportioning and the aggregate type. After estimation of the proportion of alkalis fixed in cement hydrates, it appears that about 23% to 39% of the original alkalis released by the cement are quickly sorbed on aggregate surfaces or have rapidly migrated inside aggregate particles, which may have been incorporated with time in the AAR product. After 52 weeks at 38 degrees centigrade, the pore solution alkalinity expressed from mass concrete made with PO was 250 mmol/l, whereas the alkalinity was 270 mmol/l in mass concrete incorporating SP. Since prisms of both mixtures were still expanding at 1 year, these alkalinity values are above the thresholds required for sustaining AAR in these concrete mixtures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Reduction in mortar and concrete expansion with reactive aggregates due to alkali leaching10.1520/CCA10548J ↗
2. Alkali–silica reaction in concrete related to alkali diffusion through the cement pore network
3. Influence of the storage conditions on the dimensional changes of heat-cured mortars10.1016/S0008-8846(01)00480-X ↗
4. Measurement of the alkali content of concrete using hot-water extraction
5. The effect of alkalis in Portland cement on the durability of concrete
6. The influence of test specimen dimension on expansion of alkali reactive aggregates in concrete
7. Effects of environmental conditions on AAR and preventive measures
8. M. Landry, Influence de l'air occlus, du rapport eau/ciment, de la granulométrie des granulats et de la dimension des éprouvettes testées sur la réaction alcalis-granulats dans le béton, MSc thesis, Université Laval, 1994, 105 pp.
9. Influence of different procedures on accelerated mortar bar and concrete prism tests: assessment of seven Norwegian alkali-reactive aggregates
10. Bérubé · 2003
11. Alkali levels required to induce cracking due to ASR in UK concretes
12. P. Rivard, Contribution to the evaluation of the residual expansion of concrete affected by alkali–silica reaction, PhD thesis, Université de Sherbrooke-INSA de Toulouse, 2002, 245 pp., in French.
13. Effect of supplementary cementing materials on the composition of cement hydration products10.1016/1065-7355(95)90024-1 ↗
14. Taylor · 1997
15. Quantitative petrographic technique for concrete damage due to ASR: experimental and application10.1520/CCA10465J ↗
16. Characterization of the ASR-reaction rim: application to the Potsdam sandstone10.1016/S0008-8846(02)00765-2 ↗
17. Threshold alkali contents for expansion of concrete containing British aggregates10.1016/0008-8846(92)90123-D ↗
18. Effectiveness of supplementary cementing materials in suppressing expansion due to ASR: Part 2. Effect on the pore solution chemistry10.1016/0008-8846(94)90047-7 ↗
19. New UK guidance and specifications to minimise risk of damage to concrete from ASR
20. Long-term effectiveness of supplementary cementing materials against alkali-reaction10.1016/S0008-8846(01)00538-5 ↗