Assessment of the potential reactivity of granitic rocks — Petrography and expansion tests
Source abstract
Abstract
Abstract Granite is one of the most commonly employed materials in the production of aggregates for concrete, and represents 40% of the total volume of aggregates produced in Portugal. This type of rock is traditionally considered as slowly/late reactive or even non-reactive to alkalis. However, a number of cases of damaged concrete structures in Portugal, due to alkali–silica reaction, have been related to granitic aggregates. A research program has been developed in order to define the best test method for evaluating the potential alkali-reactivity of granitic rocks. The present study involved thirteen granites collected from different quarries. The tests carried out included: petrographic examination of the aggregate, as well as mortar and concrete expansion tests. It was concluded that the content of microcrystalline quartz correlates better with the results of concrete prism expansion tests than with the mortar-bar expansion test.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Rock Mechanics and Modeling
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Concrete petrography: an introductory guide for the non-specialist, Report of a Concrete Society Working Party
2. Detection of potential alkali-reactivity of aggregates – petrographic method, TC 191-ARP, alkali-reactivity and prevention – assessment, specification and diagnosis of alkali-reactivity, prepared by I. Sims, P.J. Nixon
3. Strained quartz in relation to alkali–silica reaction
4. The EU “PARTNER” project — European standard tests to prevent alkali reactions in aggregates: final results and recommendations10.1016/j.cemconres.2009.09.004 ↗
5. The petrographic diagnosis of potentially deleterious aggregates
6. Some observations on the mechanism of alkali-aggregate reactions
7. Undulatory extinction in quartz grains of some Chilean granitic rocks of different ages10.1130/0016-7606(1964)75[363:UEIQGO]2.0.CO;2 ↗
8. An evaluation of some common Indian rocks with special reference to alkali-aggregate reactions10.1016/0013-7952(73)90042-2 ↗
9. Vernon · 2004
10. Petrographic and technological methods for evaluation of concrete aggregates
11. Undulatory extinction in quartz used for identifying potentially alkali-reactive rocks
12. Dolar-Mantuani · 1983
13. Alkali reactivity of strained quartz as a constituent of concrete aggregate
14. Alkali–silica reaction: minimizing the risk of damage to concrete. Guidance notes and model specification clauses
15. Is high undulatory extinction in quartz indicative of alkali-expansivity of granitic aggregates?
16. Microcrystalline quartz, undulatory extinction & the alkali–silica reaction
17. Anatomy of a porphyroblastic schist: alkali–silica reactivity10.1016/0013-7952(93)90071-J ↗
18. Application of microscopic and XDR techniques to investigate alkali–silica reactivity potential of rocks and minerals
19. Relationship between aggregate microstructure and mortar expansion. A case study of deformed granitic rocks from Santa Rosa mylonite zone10.1007/s10853-007-2175-8 ↗
20. A note on undulatory extinction of quartz in granite
21. Undulatory extinction of quartz in some British granites in relation to age and potential reactivity10.1144/GSL.QJEGH.1994.027.P1.09 ↗
22. Fernandes · 2005
23. Reactivity study of Brazilian aggregates through silica dissolution analysis
24. ASR of concrete aggregate quarried from a fault zone: results and petrographic interpretation of accelerated mortar bar tests10.1016/0008-8846(92)90119-G ↗
25. Alkali-reactivity of deformed granitic rocks: a case study10.1016/0008-8846(93)90184-B ↗
26. Petrographic aspects of alkali–silica reaction in eastern Australian concretes
27. Examination of microstructural features of Norwegian cataclastic rocks and their use for predicting alkali-reactivity in concrete10.1016/0013-7952(95)00044-5 ↗
28. Influence of equivalent reactive quartz content on expansion due to alkali–silica reaction10.1016/j.cemconres.2011.08.006 ↗
29. Effect of ductile deformation of quartz-bearing rocks on the alkali–silica reaction10.1016/j.enggeo.2010.08.001 ↗
30. Alkali-aggregate reaction in Iceland — new test methods
31. Effect of aggregate deformation on alkali–silica reaction
32. Comparative study of the alkali–silica reaction (ASR) in granitic aggregates10.3989/egeol.40133.091 ↗
33. Alkali–silica reaction (ASR) characteristics of concrete made from granite aggregates
34. On the AAR susceptibility of granitic and quartzitic aggregates in view of petrographic characteristics and accelerated testing
35. Alkali reactive aggregates: the importance of representative samples from the quarries
36. Na2O, K2O, SiO2 and Al2O3 release from potassic and calcic–sodic feldspars into alkaline solutions10.1016/j.cemconres.2010.04.005 ↗
37. Biotite dissolution at 25°C: the pH dependence of dissolution rate and stoichiometry10.1016/S0016-7037(97)00093-8 ↗
38. An experimental study of the dissolution mechanism rates of muscovite10.1016/j.gca.2008.01.040 ↗
39. AAR-7.3, international specification to minimize damage from alkali-reactions in concrete — Part 3: Concrete dams and other hydro structures
40. Geocronologia e petrogénese do plutonismo tardi-Varisco (NW de Portugal): Síntese e inferências sobre os processos de acreção e reciclagem crustal na Zona Centro-Ibérica
41. Granitóides da Zona Centro-Ibérica e seu enquadramento geodinâmico
42. U–Pb zircon and monazite geochronology of postcollisional Hercynian granitoids from the Central Iberian Zone (northern Portugal)10.1016/S0024-4937(98)00039-5 ↗
43. Dias · 2001 · Vol. 34 · 121
44. Durabilidade e vida útil das estruturas hidráulicas de betão e de betão armado
45. Composition of alkali–silica reaction products at different locations within concrete structures10.1016/j.matchar.2009.01.011 ↗
46. Microscopic analysis of alkali-aggregate reaction products in a 50-year-old concrete10.1016/j.matchar.2004.08.005 ↗
47. Examination of the concrete from an old Portuguese dam: texture and composition of alkali–silica gel10.1016/j.matchar.2007.04.007 ↗
48. Santos Silva · 2005
49. Santos Silva · 2000 · 23
50. Appendix A — Portugal
51. Santos Silva · 2008 · 323
52. RILEM recommendations for the prevention of damage by alkali-aggregate reactions in new concrete structures10.1007/978-94-017-7252-5 ↗
53. Prevenção das reacções álcalis-agregado (RAA) no concreto — melhoria do monitoramento da reatividade aos álcalis de agregados
54. Metodologias para prevenir reacções expansivas internas
55. ASTM C 1260 · 2007
56. Alkali reactivity of of granitic rocks in Portugal: a case study
57. Role of granitic aggregates in the deterioration of a concrete dam10.1007/s10064-014-0590-z ↗
58. PARTNER Report 3.1 — experience from using petrographic analysis according to the RILEM AAR-1 method to assess alkali reactions in European aggregates
59. Inertes para argamassas e betões — determinação da reactividade potencial com os álcalis
60. Igneous rocks. A classification and glossary of terms
61. Field evidence for inability of ASTM C 1260 limits to detect slowly reactive Australian aggregates10.1080/14488353.2007.11463917 ↗
62. Petrographic characterization of granitic aggregates. Comparison with the results from laboratory tests
63. Petrographic characterization vs. laboratory test methods applied to granitic aggregates
64. Ramos · 2012
65. Ramos · 2013
66. Alkali–silica reactions (ASR): literature review on parameters influencing laboratory performance testing10.1016/j.cemconres.2011.10.004 ↗
67. Alkali–silica reaction (ASR) — performance testing: influence of specimen pre-treatment, exposure conditions and prism size on concrete porosity, moisture state and transport properties10.1016/j.cemconres.2013.05.020 ↗
68. CSA A23.2-27A · 2014
69. Effect of aggregate particles size on determining alkali–silica reactivity by accelerated tests10.1520/JAI100432 ↗
70. Evaluation of accelerated test methods for determining alkali–silica reactivity of concrete aggregates10.1016/j.cemconcomp.2006.03.001 ↗
71. Effects of aggregate size and alkali content on ASR expansion10.1016/j.cemconres.2009.08.002 ↗
72. Effectiveness of the accelerated mortar bar test to detect rapid reactive aggregates (including the pessimum content) and slowly reactive aggregates10.1016/j.cemconres.2014.01.001 ↗
73. Le Roux · 1999
74. NF P 18-543 · 2015
75. Comparative study of the concrete prism test (CPT 60°C, 100% RH) and other accelerated tests