Effect of brief heat-curing on microstructure and mechanical properties in fresh cement based mortars
Source abstract
Abstract
Abstract The effect of temperature on fresh mortar and cement paste was evaluated by simulating the curing conditions of external buildings plastering applied under extremely hot weather. The specimens were heated at controlled temperatures in the 40−80 °C range by exposure to IR radiation over short periods. The effect of soaking for a short time was also examined. The results of compressive strength tests, scanning electron microscopy, infrared spectroscopy and mercury porosimetry helped to characterize the mechanical and physico-chemical properties of the studied sample. Early age behaviour (28 days) in neat cement was barely affected by the temperature. By contrast, exposure to high temperatures caused significant microstructural changes in the mortar. However, successive soaking over short periods was found to reactivate the mechanism of curing and restore the expected mechanical properties. Based on the results, application of cement based mortar at high temperatures is effective when followed by a short, specific soaking process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Concrete and Cement Materials Research · Conservation Techniques and Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Rodríguez-Mora · 2003
2. Development of microstructures in plain cement pastes hydrated at different temperatures10.1016/0008-8846(91)90044-I ↗
3. Effect of temperature on the hydration of the main clinker phases in Portland cements: Part I, neat cements10.1016/S0008-8846(98)00115-X ↗
4. Hydration characteristics of Portland cement after heat curing: I, degree of hydration of the anhydrous cement phases10.1111/j.1151-2916.2001.tb00707.x ↗
5. Effect of temperature on the pore solution, miscrostructure and hydration products of Portland cement pastes10.1016/j.cemconres.2006.11.016 ↗
6. Delayed ettringite formation in heat-cured Portland cement mortars10.1016/S0008-8846(98)00168-9 ↗
7. Delayed ettringite formation symptoms on mortars induced by high temperature due to cement heat hydration or late thermal cycle10.1016/j.cemconres.2004.05.041 ↗
8. Effects of an early or a late heat treatment on the microstructure and composition of inner C–S–H products of Portland cement mortars10.1016/S0008-8846(01)00670-6 ↗
9. Use of limestone obtained from waste of the mussel cannery industry for the production of mortars10.1016/j.cemconres.2007.01.004 ↗
10. The effects of heat treatment on inner product C–S–H10.1016/0008-8846(92)90051-V ↗
11. Structure of calcium silicate hydrate (C–S–H): near-, mid-, and far- infrared spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
12. Microstructural characterisation of leaching effects in cement pastes due to neutralisation of their alkaline nature. Part I: Portland cement pastes10.1016/j.cemconres.2006.10.002 ↗
13. La spectrométrie infrarouge à transformée de Fourier (IRTF). Une méthode intéressante pour la caractérisation des ciments
14. Influence of silica fume and fly ash additions on calcium aluminate cement hydration. A spectroscopic study and scanning electron microscopic evaluation10.1111/j.1551-2916.2008.02283.x ↗
15. Farmer · 1974
16. Microstructural changes induced in Portland cement-based materials due to natural and supercritical carbonation10.1007/s10853-008-2521-5 ↗
17. Masonry repair lime-based mortars: factors affecting the mechanical behaviour10.1016/S0008-8846(03)00210-2 ↗
18. Mercury porosimetry of hardened cement pastes10.1016/S0008-8846(99)00083-6 ↗
19. Effect of environmental conditions on the properties of fresh and hardened concrete10.1016/S0958-9465(01)00007-5 ↗
20. Internal communication from Grupo PUMA producer; www.grupopuma.com.