journal article·2024-07Open access

Degradation of alkali-activated Fe-rich slag in sulfuric acid

Nana Wen, Arne Peys, Tobias Hertel, Ziyou Yu, Dimitrios Sakellariou, Yiannis Pontikes

Abstract

Alkali-activated Fe-rich non-ferrous metallurgical slag (AA-NFS), within the FeO x-SiO 2-Al 2O 3 -CaO-MgO system, were tested in 2 wt% sulfuric acid for 6 months. Corrosion depth and rate were measured non-destructively by micro X-ray computed tomography. Both intact and corroded areas were characterized by XRD, FTIR, SEM-EDX and NMR. AA-NFS with higher Ca/Si showed a higher resistance to sulfuric acid. The presence of Mg negatively affected the resistance, whereas higher Al concentrations slightly enhanced the resistance in the investigated chemical composition range. The corrosion degree is closely related to the NFS reaction extent in AA-NFS, and this corrosion process is diffusion-controlled. Leaching of the elements (Al, Ca, Mg, Fe and Na) leaves behind mostly silica-rich gels, causing the failure of the framework structure after long-term exposure. The leached Ca 2+ reacted with SO 4 2− in acid solution and formed expansive sulfate products, which possibly clog pores and offer an additional protective barrier for AA-NFS against sulfuric acid.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Mine drainage and remediation techniques · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Environmental impacts and decarbonization strategies in the cement and concrete industries10.1038/s43017-020-0093-3 ↗
2. Mechanism of geopolymerization and factors influencing its development: a review10.1007/s10853-006-0401-4 ↗
3. The effects of ground granulated blast-furnace slag blending with fly ash and activator content on the workability and strength properties of geopolymer concrete cured at ambient temperature10.1016/j.matdes.2014.05.001 ↗
4. Sustainable iron-rich cements: raw material sources and binder types10.1016/j.cemconres.2022.106834 ↗
5. Upcycling of non-ferrous metallurgy slags: identifying the most reactive slag for inorganic polymer construction materials10.1016/j.resconrec.2019.104627 ↗
6. High-temperature behavior of CaO-FeOx-Al2O3-SiO2-rich alkali activated materials10.3390/app12052572 ↗
7. Inorganic polymers from CaO-FeOx-SiO2 slag: the start of oxidation of Fe and the formation of a mixed valence binder10.3389/fmats.2019.00212 ↗
8. Chemical, microbiological, and in situ test methods for biogenic sulfuric acid corrosion of concrete10.1016/S0008-8846(00)00219-2 ↗
9. Environmental, physical and structural characterisation of geopolymer matrixes synthesised from coal (co-)combustion fly ashes10.1016/j.jhazmat.2007.10.008 ↗
10. Microbiologically induced concrete corrosion: a case study from a combined sewer network10.1016/j.cemconres.2015.06.011 ↗
11. Resistance of self-consolidating concrete to sulfuric acid attack with consecutive pH reduction10.1016/j.cemconres.2007.04.014 ↗
12. Performance of alkali-activated slag mortars exposed to acids
13. Nanoscale chemical degradation mechanisms of sulfate attack in alkali-activated slag10.1021/acs.jpcc.7b11270 ↗
14. Hydration mechanisms of super sulphated slag cement10.1016/j.cemconres.2008.03.004 ↗
15. Investigation on some factors affecting the characteristics of alkali-phosphorus slag cement10.1016/0008-8846(89)90004-5 ↗
16. Corrosion of hardened cement paste by acetic and nitric acids - part I: calculation of corrosion depth
17. Geopolymerization of solid waste of non-ferrous metallurgy - a review10.1016/j.jenvman.2019.109571 ↗
18. The durability of alkali-activated materials in comparison with ordinary Portland cements and concretes: a review10.1016/j.eng.2019.08.019 ↗
19. Evidence of formation of an amorphous magnesium silicate (AMS) phase during alkali activation of (Na-Mg) aluminosilicate glasses10.1016/j.cemconres.2021.106464 ↗
20. Resistance of alkali-activated binders to organic acid attack: assessment of evaluation criteria and damage mechanisms10.1016/j.conbuildmat.2017.06.117 ↗
21. An overview of the utilisation of Fe-rich residues in alkali-activated binders: mechanical properties and state of iron10.1016/j.jclepro.2021.129900 ↗
22. Durability of alkali-activated Fe-rich Fayalite slag-based mortars subjected to different environmental conditions10.1016/j.cemconres.2022.106984 ↗
23. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag — part I: effect of MgO10.1016/j.cemconres.2011.05.002 ↗
24. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
25. Phase formation and evolution in Mg(OH)2–zeolite cements10.1021/acs.iecr.7b04201 ↗
26. Structure characterization of hydration products generated by alkaline activation of granulated blast furnace slag10.1007/s10853-008-3028-9 ↗
27. Sulfuric acid degradation of alkali-activated metakaolin cements supplemented with brucite10.1016/j.cemconcomp.2021.104063 ↗
28. A.B. E. Douglas, V.M. Malhotra, Properties and durability of alkali-activated slag concrete, ACI Mater. J., 89.
29. Sulfuric acid attack on hardened paste of geopolymer cements part 1. Mechanism of corrosion at relatively high concentrations
30. Durability test methods and their application to AAMs: case of sulfuric-acid resistance
31. Acid resistance of inorganic polymer binders. 1. Corrosion rate10.1617/s11527-011-9744-7 ↗
32. Sorptivity and acid resistance of ambient-cured geopolymer mortars containing nano-silica10.1016/j.cemconcomp.2016.06.017 ↗
33. Chemical research and climate change as drivers in the commercial adoption of alkali activated materials10.1007/s12649-010-9015-9 ↗
34. Provis · 2014
35. Binary, ternary and quaternary Fe-rich slags: influence of Fe and Si substitution by Ca and Al on the atomic structure and reactivity
36. Slag or reacted binder, which dissolves first in sulphuric acid?10.1007/978-3-031-33211-1_65 ↗
37. A comparative study on the pore structure of alkali-activated fly ash evaluated by mercury intrusion porosimetry, N2 adsorption and image analysis10.1007/s10853-017-1965-x ↗
38. Sulfate attack monitored by microCT and EDXRD: influence of cement type, water-to-cement ratio, and aggregate10.1016/j.cemconres.2005.06.004 ↗
39. Yu · 2023
40. The influence of air and temperature on the reaction mechanism and molecular structure of Fe-silicate inorganic polymers10.1016/j.jnoncrysol.2019.119675 ↗
41. The unique mechanism of analcime dissolution by hydrogen ion attack10.1021/la061576q ↗
42. A quantitative comparison between chemical dosing and electrocoagulation10.1016/S0927-7757(02)00285-6 ↗
43. Deterioration mechanism of alkali-activated materials in sulfuric acid and the influence of Cu: a micro-to-nano structural, elemental and stable isotopic multi-proxy study10.1016/j.cemconres.2021.106373 ↗
44. An assessment of complex formation between aluminium and silicic acid in acidic solutions10.1016/0016-7037(94)90088-4 ↗
45. Occurrence of polymerized silicic acid and aluminum species in two forest soil solutions with different acidity10.1016/j.geoderma.2007.11.022 ↗
46. Sulfuric acid attack on hardened paste of geopolymer cements - part 1. Mechanism of corrosion at relatively
47. Sulfuric acid resistance of one-part alkali-activated mortars10.1016/j.cemconres.2018.04.009 ↗
48. Inorganic polymers made of fayalite slag: on the microstructure and behavior of Fe10.1111/jace.15420 ↗
49. Resistance of geopolymer materials to acid attack10.1016/j.cemconres.2004.06.005 ↗
50. Influence of CaO/FeO ratio on the formation mechanism and properties of alkali-activated Fe-rich slags10.1016/j.cemconres.2021.106466 ↗
51. The defect structure of sol−gelderived silicapolytetrahydrofuran hybrid films by FTIR10.1016/S0022-3093(01)00418-5 ↗
52. Synthesis and characterization by FTIR spectroscopy of silica aerogels prepared using several Si(OR)4 and R″Si(OR′)3 precursors10.1016/j.molstruc.2008.08.025 ↗
53. Gypsophile chemistry unveiled: Fourier transform infrared (FTIR) spectroscopy provides new insight into plant adaptations to gypsum soils10.1371/journal.pone.0107285 ↗
54. Solid-state nuclear magnetic resonance spectroscopy of cements
55. Studies using 27Al MAS NMR of AFm and AFt phases and the formation of Friedel’s salt10.1016/S0008-8846(02)00901-8 ↗
56. Alkali-activation of CaO-FeOx-SiO2 slag: formation mechanism from in-situ X-ray total scattering10.1016/j.cemconres.2019.04.019 ↗
57. Study of acidic degradation of alkali-activated materials using synthetic C-(N)-A-S-H and N-A-S-H gels10.1016/j.compositesb.2021.109510 ↗
58. Acid attack on hydrated cement — effect of mineral acids on the degradation process10.1016/j.cemconres.2015.03.011 ↗
59. New selective dissolution process to quantify reaction extent and product stability in metakaolin-based geopolymers10.1016/j.compositesb.2019.107172 ↗
60. Generalized structural description of calcium–sodium aluminosilicate hydrate gels: the cross-linked substituted tobermorite model10.1021/la4000473 ↗
61. Contribution of silica gels to superimposed 29Si MAS NMR spectra of Y zeolites dealuminated by steaming10.1002/1521-3749(200111)627:11<2559::AID-ZAAC2559>3.0.CO;2-0 ↗
62. Impact of Ca, Al, and Mg on reaction kinetics, pore structure and performance of Fe-rich alkali-activated slag10.1111/jace.19727 ↗