Alkali-silica reaction (ASR), a detrimental process causing volume expansion and cracking in concrete by forming hygroscopic and swellable gel-like products, has been a long-standing challenge faced by concrete structures across the world. Understanding the underlying mechanisms of formation, moisture uptake and swelling of ASR gels requires thorough characterizations, where an appropriate drying method to remove free water and stop the reactions in the samples is essential. This study aims to elucidate the effect of freeze-drying, an emerging drying technique increasingly employed in sample preparations, on the phase, molecular structure, and moisture absorption behavior of ASR gels. Towards this end, six ASR gels with three calcium-to-silica (Ca/Si) ratios (0.1, 0.3, and 0.5) and two alkali-to-silica [(Na + K)/Si] ratios of 0.3 (low-alkali gels) and 1.0 (high-alkali gels) were studied. The results indicate that the chemical bonds and mineral components of ASR gels can be maintained during the removal of free and loosely bound water in freeze drying, while slight changes in crystallization and relative contents of alkali-silicate hydrate and calcium silicate hydrate phases were observed, in particular, for the high-alkali ASR gels. Although slight decreases in Q 1, Q 2, and Q 3 silica polymerization sites and increases in the mean chain length and degree of polymerization were observed from the nuclear magnetic resonance (NMR) spectroscopy, the intrinsic layered silicate structure of ASR gels remains. The moisture absorption of low-alkali and high-alkali ASR gels was found to be governed by gel pores and mesopores, respectively. After freeze-drying, slight increases in moisture sorption (a 6.8 % increase in absorption and a 2.2 % decrease in desorption) and enhanced hysteresis were observed from the low-alkali gels. The high-alkali gels, however, showed a slight decrease in hygroscopicity along with a 16.6 % reduction of mesopores.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aerogels and thermal insulation · Methane Hydrates and Related Phenomena · Mesoporous Materials and Catalysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. Influence of cement and aggregate on concrete expansion
2. Swamy, R.N., The Alkali-Silica Reaction in Concrete, CRC Press1991.10.4324/9780203036631 ↗
3. The structure of alkali silicate gel by total scattering methods10.1016/j.cemconres.2010.02.006 ↗
4. Atomistic structure of alkali-silica reaction products refined from X-ray diffraction and micro X-ray absorption data10.1016/j.cemconres.2019.105958 ↗
5. The alkali–silica reaction: part I
6. Giebson, C., About the colloidal nature of ASR products, Proceedings of the 16th ICAAR, 2, 2022, pp. 247–258.
7. Osmotic pressure and the swelling of gels10.1016/0008-8846(79)90050-4 ↗
8. The chemistry of ‘alkali-aggregate’reaction10.1016/0008-8846(81)90003-X ↗
9. Swelling properties of synthetic alkali silica gels10.1111/j.1151-2916.1981.tb15864.x ↗
10. Synthesis, characterization, and water uptake property of alkali-silica reaction products10.1016/j.cemconres.2019.04.009 ↗
11. Micro-mechanical modelling of alkali–silica-reaction-induced degradation using the AMIE framework10.1016/j.cemconres.2009.07.024 ↗
12. Relation of expansion due to alkali silica reaction to the degree of reaction measured by SEM image analysis10.1016/j.cemconres.2007.04.016 ↗
13. Different manifestations of the alkali-silica reaction in concrete according to the reaction kinetics of the reactive aggregate10.1016/j.cemconres.2005.12.022 ↗
14. Modified model of alkali-silica reaction10.1016/j.cemconres.2007.06.008 ↗
15. Impact of temperature on expansive behavior of concrete with a highly reactive andesite due to the alkali–silica reaction10.1016/j.cemconres.2019.105888 ↗
16. Moisture stability of crystalline alkali-silica reaction products formed in concrete exposed to natural environment10.1016/j.matdes.2020.109066 ↗
17. Alkali silica reaction in concrete-revealing the expansion mechanism by surface force measurements10.1016/j.cemconres.2023.107392 ↗
18. E-modulus of the alkali–silica-reaction product determined by micro-indentation10.1016/j.conbuildmat.2013.03.018 ↗
19. Crystallized alkali-silica gel in concrete from the late 1890s10.1016/j.cemconres.2006.05.017 ↗
20. Evaluation of drying methods by nitrogen adsorption10.1016/j.cemconres.2019.02.016 ↗
21. The influence of different drying methods on cement paste microstructures as reflected by gas adsorption: comparison between freeze-drying (F-drying)
22. Is freeze-drying an alternative to solvent exchange for the hydration stop of cementitious suspensions?10.1016/j.cemconres.2022.106841 ↗
23. Effect of sample moisture content on XRD-estimated cellulose crystallinity index and crystallite size10.1007/s10570-017-1259-0 ↗
24. Influence of moisture variation on the performance of Raman spectroscopy in quantitative pharmaceutical analyses10.1016/j.jpba.2018.10.022 ↗
25. A new approach to removing interference of moisture from FTIR spectrum10.1016/j.saa.2021.120373 ↗
26. Mineral characterization using scanning electron microscopy (SEM): a review of the fundamentals, advancements, and research directions10.3390/app132312600 ↗
27. Comparison of methods for arresting hydration of cement10.1016/j.cemconres.2011.06.003 ↗
28. Effect of drying on cement-based materials pore structure as identified by mercury intrusion porosimetry: a comparative study between oven-, vacuum-, and freeze-drying10.1016/S0008-8846(01)00594-4 ↗
29. Influence of drying on the microstructure of hardened cement paste: a mercury intrusion porosimetry, nitrogen sorption and SAXS study10.3151/jact.18.83 ↗
30. Report of TC 238-SCM: hydration stoppage methods for phase assemblage studies of blended cements—results of a round robin test10.1617/s11527-018-1237-5 ↗
31. Validity of using methanol for studying the microstructure of cement paste10.1007/BF02472723 ↗
32. The influence of water removal techniques on the composition and microstructure of hardened cement pastes10.1016/j.cemconres.2008.02.012 ↗
33. The effect of drying method on ordinary Portland cement surfaces during the early stages of hydration10.1617/s11527-012-9878-2 ↗
34. Effect of drying method on calcium silicate hydrate (CSH): experiments and molecular dynamics simulations study10.1016/j.conbuildmat.2023.134367 ↗
35. Water removal by freeze-drying of hardened cement paste10.1080/07373937.2012.717326 ↗
37. The influence of alkali–silica reaction (ASR) gel composition on its hydrophilic properties and free swelling in contact with water vapor10.1016/j.cemconres.2017.01.006 ↗
38. Characterization of viscoelastic behavior of synthetic alkali–silica reaction gels10.1016/j.cemconcomp.2019.103359 ↗
39. Quantifying the swelling properties of alkali-silica reaction (ASR) gels as a function of their composition10.1111/jace.14893 ↗
40. Effect of aluminum on the structure of synthetic alkali-silica gels10.1016/j.cemconres.2022.107088 ↗
41. Effect of the chemical composition of synthetic alkali-silica gels on their structure, swelling behavior and water uptake10.1016/j.cemconres.2024.107596 ↗
42. Alkali-silica reaction products: comparison between samples from concrete structures and laboratory test specimens10.1016/j.matchar.2010.09.010 ↗
43. Assessment of the thermodynamics of Na, K-shlykovite as potential alkali-silica reaction products in the (Na, K) 2O-CaO–SiO2-H2O system10.1016/j.cemconres.2023.107253 ↗
44. Influences of composition and reaction conditions on molecular structure, hygroscopicity, and swelling behavior of alkali-silica reaction gels10.1016/j.cemconcomp.2024.105537 ↗
45. Microstructure, crystallinity and composition of alkali-silica reaction products in concrete determined by transmission electron microscopy10.1016/j.cemconres.2020.105988 ↗
46. Structural investigations of alkali silicate gels10.1111/j.1551-2916.2005.00145.x ↗
47. Quantitative microanalyses of alkali-silica gel in concrete10.1016/0008-8846(75)90019-8 ↗
48. Struble · 1979
49. Application of micro X-ray diffraction to investigate the reaction products formed by the alkali–silica reaction in concrete structures10.1016/j.cemconres.2015.07.012 ↗
50. Composition of alkali silica gel and ettringite in concrete railroad ties: SEM-EDX and X-ray diffraction analyses10.1016/0008-8846(95)00219-7 ↗
51. Almond · 1995
52. Experimental and molecular dynamics modeling studies of interlayer swelling: water incorporation in kanemite and ASR gel10.1007/BF02482141 ↗
53. Földvári, M., Handbook of Thermogravimetric System of Minerals and its Use in Geological Practice, Geological Institute of Hungary Budapest 2011.
54. Thermal dehydration of tobermorite and jennite
55. Effect of magnesium on the structure and chemical composition of calcium silicate hydrate at elevated temperature10.1016/j.conbuildmat.2019.117925 ↗
56. The role of aluminium in CASH during sulfate attack on concrete10.1016/j.cemconres.2018.11.012 ↗
57. Direct determination of amorphous number density from the reduced pair distribution function10.1016/j.mex.2019.03.005 ↗
58. Thomson, W., 4. On the equilibrium of vapour at a curved surface of liquid, Proceedings of the Royal Society of Edinburgh, 7, 1872, pp. 63–68.10.1017/S0370164600041729 ↗
59. Investigating temperature change rate and pore confinement effect on thermal properties of phase change materials for de-icing and low-temperature applications in cementitious composites10.1016/j.conbuildmat.2023.134237 ↗
60. Transport due to diffusion, drying, and wicking in concrete containing a shrinkage-reducing admixture10.1061/(ASCE)MT.1943-5533.0001983 ↗
61. Numerical simulation of the freeze–thaw behavior of mortar containing deicing salt solution10.1617/s11527-016-0964-8 ↗
62. Influence of pore structure on compressive strength of cement mortar
63. A thermodynamic and kinetic model for paste–aggregate interactions and the alkali–silica reaction10.1016/j.cemconres.2015.05.004 ↗
64. Formation of ASR gel and the roles of CSH and portlandite10.1016/j.cemconres.2004.03.026 ↗
65. Atomic structure of nanocrystalline and amorphous asr products10.1016/j.cemconres.2024.107521 ↗
66. A structural consideration of kanemite, octosilicate, magadiite and kenyaite10.1039/a606856a ↗
67. Characterization of magnesium silicate hydrate (MSH) gel formed by reacting MgO and silica fume10.3390/ma11060909 ↗
68. Enhanced polymer induced precipitation of polymorphous in calcium carbonate: calcite aragonite vaterite phases10.1007/s10904-017-0520-1 ↗
69. Phase evolution and property development of alkali-silica reaction gel in carbonation
70. Fundamental assessment of graphite Nanoplatelet effects on Progress of alkali-silica reactions
71. Phase evolution and mechanical-hydroscopic properties of alkali-silica reaction gels modified by magnesium nitrate10.1016/j.cemconcomp.2023.105283 ↗
72. A vibrational spectroscopic study of kanemite10.1016/S1387-1811(98)00270-4 ↗
73. Hydrothermal synthesis and characterization of aluminium and sulfate substituted 1.1 nm tobermorites10.1016/j.jallcom.2007.11.130 ↗
74. Synthesis of polypyrrole/Fe-kanemite nanocomposite through in situ polymerization: effect of iron exchange, acid treatment, and CO2 adsorption properties10.1007/s10853-016-0541-0 ↗
75. Nanostructure of calcium silicate hydrates in cements10.1103/PhysRevLett.104.195502 ↗
76. 29Si MAS NMR spectroscopic investigation of alkali silica reaction product gels10.1016/0008-8846(93)90035-8 ↗
77. The structure and stoichiometry of CSH10.1016/j.cemconres.2004.04.035 ↗
78. Solid-state high-resolution 29Si NMR spectroscopy of synthetic 14 Å, 11 Å and 9 Å tobermorites10.1016/0008-8846(82)90081-3 ↗
79. The role of calcium on the formation of alkali-silica reaction products10.1016/j.cemconres.2019.105898 ↗
80. Influence of decalcification on structural and mechanical properties of synthetic calcium silicate hydrate (CSH)10.1016/j.cemconres.2019.105793 ↗
81. Calcium silicate hydrates: solid and liquid phase composition10.1016/j.cemconres.2015.03.019 ↗
82. Effect of calcium and lithium on alkali-silica reaction kinetics and phase development10.1016/j.cemconres.2018.10.007 ↗
83. Effect of Al electronic configuration on the SiO2 thin film growth via catalytic self-assembling deposition10.1021/jp405847r ↗
84. Magnesium and calcium silicate hydrates, part I: investigation of the possible magnesium incorporation in calcium silicate hydrate (CSH) and of the calcium in magnesium silicate hydrate (MSH)10.1016/j.apgeochem.2017.12.005 ↗
85. The study of disorder and nanocrystallinity in C–S–H, supplementary cementitious materials and geopolymers using pair distribution function analysis10.1016/j.cemconres.2011.03.027 ↗
86. Reporting physisorption data for gas/solid systems with special reference to the determination of surface area and porosity (recommendations 1984)10.1351/pac198557040603 ↗
87. Physisorption of gases, with special reference to the evaluation of surface area and pore size distribution (IUPAC technical report)10.1515/pac-2014-1117 ↗
88. Experimental confirmation of different mechanisms of evaporation from ink-bottle type pores: equilibrium, pore blocking, and cavitation10.1021/la026140z ↗