An ASR exposure site after 30 years – Chemical composition of hydrates and ASR products
Source abstract
Abstract
Concrete specimens containing two aggregates susceptible to alkali-silica reaction (ASR) and various supplementary cementitious materials (SCMs) have been exposed outdoors since 1992. After 30 years of expansion monitoring, some specimens were cored to conduct an in-depth analysis of their condition. The chemical compositions of the hydrates and the ASR products were quantified with SEM-EDS. All SCMs increased the Si/Ca of the C-(A)-S-H, but the extent varied depending on their composition, amount and degree of reaction. Larger amounts of SCMs resulted in lower degrees of reaction. The ASR products inside aggregate particles of non-boosted concrete mixtures were crystalline. Their Ca/Si was in the range 0.21–0.24, independent of the binder and the aggregate types. The (Na + K)/Ca was usually in the range 0.31–0.35. The Na/K varied more, correlating with the respective ratios in the binder. The Al content of the ASR products inside aggregate particles was not influenced by the presence of Al-rich SCMs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Graphite, nuclear technology, radiation studies · Nuclear materials and radiation effects · Chemical Synthesis and Characterization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (79)
Show source-provided references
1. Sims · 2017
2. Chemistry of alkali–silica reaction and testing of aggregates10.1016/j.cemconcomp.2005.03.005 ↗
3. Alkali silica reaction - sequence, products and possible mechanism of expansion. Keynote lecture
4. An interpretation of some published researches on the alkali-aggregate reaction part 1-the chemical reactions and mechanism of expansion
5. Swelling properties of synthetic alkali silica gels10.1111/j.1151-2916.1981.tb15864.x ↗
6. Experimental and molecular dynamics modeling studies of interlayer swelling: water incorporation in kanemite and ASR gel10.1007/BF02482141 ↗
7. The influence of alkali–silica reaction (ASR) gel composition on its hydrophilic properties and free swelling in contact with water vapor10.1016/j.cemconres.2017.01.006 ↗
8. Alkali silica reaction in concrete - revealing the expansion mechanism by surface force measurements10.1016/j.cemconres.2023.107392 ↗
9. Types of alkali–aggregate reactions and the products formed
10. The effect of supplementary cementing materials on alkali-silica reaction: a review10.1016/j.cemconres.2010.11.003 ↗
11. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
12. Alkali binding in cement pastes: Part I. The C-S-H phase10.1016/S0008-8846(99)00187-8 ↗
13. Calcium silicate hydrates: solid and liquid phase composition10.1016/j.cemconres.2015.03.019 ↗
14. Alkali uptake in calcium alumina silicate hydrate (C-A-S-H)10.1016/j.cemconres.2016.03.009 ↗
15. A method for predicting alkali ion concentrations in cement pore solutions10.1680/adcr.1987.1.1.5 ↗
16. Outcomes of the RILEM round robin on degree of reaction of slag and fly ash in blended cements10.1617/s11527-017-1002-1 ↗
17. The addition of caesium to concrete with alkali-silica reaction: Implications on product identification and recognition of the reaction sequence10.1016/j.cemconres.2019.03.016 ↗
18. Synthesis of alkali-silica reaction product structurally identical to that formed in field concrete10.1016/j.matdes.2020.108562 ↗
19. Composition of alkali silica gel and ettringite in concrete railroad ties: SEM-EDX and X-ray diffraction analyses10.1016/0008-8846(95)00219-7 ↗
20. Crystallized alkali-silica gel in concrete from the late 1890s10.1016/j.cemconres.2006.05.017 ↗
21. Microanalysis of crystalline ASR products from a 50 year-old concrete structure
22. E-modulus of the alkali-silica-reaction product determined by micro-indentation10.1016/j.conbuildmat.2013.03.018 ↗
23. An attempt to validate the ultra-accelerated microbar and the concrete performance test with the degree of AAR-induced damage observed in concrete structures10.1016/j.cemconres.2013.03.014 ↗
24. Application of micro X-ray diffraction to investigate the reaction products formed by the alkali–silica reaction in concrete structures10.1016/j.cemconres.2015.07.012 ↗
25. Raman microscopy of alkali-silica reaction (ASR) products formed in concrete10.1016/j.cemconres.2017.08.014 ↗
26. Nano-mechanical properties of alkali-silica reaction (ASR) products in concrete measured by nano-indentation10.1016/j.conbuildmat.2017.10.006 ↗
27. Oldest example of alkali-silica reaction in Japan - Takyo Bay sea forts no. 2 and 3, constructed 120–100 years ago
28. Microstructure, crystallinity and composition of alkali-silica reaction products in concrete determined by transmission electron microscopy10.1016/j.cemconres.2020.105988 ↗
29. Characterization of amorphous and crystalline ASR products formed in concrete aggregates10.1016/j.cemconres.2020.106190 ↗
30. Moisture stability of crystalline alkali-silica reaction products formed in concrete exposed to natural environment10.1016/j.matdes.2020.109066 ↗
31. Concrete cancer : characterization of Alkali Silica Reaction early stage products by electron microscopy, PhD Thesis, Ecole Polytechnique Fédérale de Lausanne
32. PARTNER project post-documentation study. Condition assessment of field exposure site cubes. Results of microstructural analyses10.1016/j.cemconres.2022.107006 ↗
33. ASR gels and their crystalline phases in concrete—universal products in alkali-silica, alkali-silicate and alkali-carbonate reactions
34. Long-term efficiency of silica fume and fly ash to suppress ASR in field structures10.3989/mc.2022.15821 ↗
35. Evaluating the efficiency of SCMs to avoid or mitigate ASR-induced expansion and deterioration through a multi-level assessment10.1016/j.cemconres.2023.107262 ↗
36. Alkali-Aggregate Reaction Combined with Freeze/Thaw in Newfoundland, Canada Petrography using EPMA
37. Comparative field and laboratory investigations on the use of supplementary cementing materials to control alkali-silica reaction in concrete
38. Comparative field and laboratory investigations on the use of supplementary cementing materials (SCMs) to control alkali-silica reaction (ASR) in concrete
39. Field and laboratory investigations on the use of fly ash and Li-based admixtures to prevent ASR in concrete
40. Alkali metal distribution in composite cement pastes and its relation to accelerated ASR tests10.1016/j.cemconres.2023.107283 ↗
41. The geology, properties and field performance of alkali-aggregate reactive Spratt, Sudbury and Pittsburg aggregate distributed by the Ontario Ministry of Transportation
42. Multilaboratory study of the concrete prism and accelerated mortar bar expansion tests with Spratt aggregate
43. The influence of the alkali-silicate reaction on structures in the vicinity of Sudbury, Ontario
44. Outlier Labeling
45. A rapid furnace-based gravimetry test for assessing reactivity of supplementary cementitious materials10.1617/s11527-022-02029-0 ↗
46. Scrivener · 2016
47. Gem-selektor geochemical modeling package: TSolMod library and data interface for multicomponent phase models10.3749/canmin.50.5.1173 ↗
48. GEM-Selektor geochemical modeling package: revised algorithm and GEMS3K numerical kernel for coupled simulation codes
49. Paul Scherer Institut
50. Cemdata18: a chemical thermodynamic database for hydrated Portland cements and alkali-activated materials10.1016/j.cemconres.2018.04.018 ↗
51. A structurally-consistent CASH+ sublattice solid solution model for fully hydrated C-S-H phases: Thermodynamic basis, methods, and Ca-Si-H2O core sub-model10.1016/j.cemconres.2021.106585 ↗
52. Extensions of CASH+ thermodynamic solid solution model for the uptake of alkali metals and alkaline earth metals in C-S-H10.1016/j.cemconres.2021.106667 ↗
53. Supplementary data to the journal article “An ASR exposure site after 30 years – Chemical composition of hydrates and ASR products”
54. Reactivity of supplementary cementitious materials (SCMs) in cement blends10.1016/j.cemconres.2019.105799 ↗
55. Report of RILEM TC 301-ASR: modelling the impact of SCMs, alkali level and w/b ratio on alkali concentration in pore solution10.1617/s11527-025-02583-3 ↗
56. Segmentation of elemental EDS maps by means of multiple clustering combined with phase identification10.1111/jmi.12309 ↗
57. Distribution of sulphate and aluminium in hydrated cement pastes10.1016/j.cemconres.2024.107467 ↗
58. Retardation effect of the pozzolanic reaction of low-calcium supplementary cementitious materials on clinker hydration at later age: Effects of pore solution, foreign ions, and pH10.1016/j.cemconres.2023.107416 ↗
59. M.D.A. Thomas, B. Fournier, K.J. Folliard, Alkali-aggregate reactivity (AAR) facts book, United States. Federal Highway Administration. Office of Pavement Technology, 2013. https://rosap.ntl.bts.gov/view/dot/26838/dot_26838_DS1.pdf (accessed August 27, 2025).
60. Recent applications of a modified gel pat test to determine the potential alkali-silica reactivity of carbonate aggregates10.1016/0958-9465(93)90038-B ↗
61. ASR potential of volcanic aggregates using the gel-pat test and the phosphoric acid method
62. Viscosities and densities of highly concentrated aqueous MOH solutions (M+ = Na+, K+, Li+, Cs+, (CH3)4N+) at 25.0 °C10.1021/je000019h ↗
63. Aggregation and gel formation in basic silico−calco−alkaline solutions studied: a SAXS, SANS, and ELS study10.1021/jp990151s ↗
64. Role of granitic aggregates in the deterioration of a concrete dam10.1007/s10064-014-0590-z ↗
65. Internal alkali transport in recycling concrete and its impact on alkali-silica reaction10.1016/j.cemconres.2023.107334 ↗
66. Effect of environmental conditions on expansion in concrete due to alkali-silica reaction (ASR)10.1016/j.matchar.2008.12.018 ↗
67. The combined effect of potassium, sodium and calcium on the formation of alkali-silica reaction products10.1016/j.cemconres.2019.105914 ↗
68. Alkali-silica reactions (ASR): literature review on parameters influencing laboratory performance testing10.1016/j.cemconres.2011.10.004 ↗
69. Impact of NaOH addition on the ASR expansion of ternary concrete incorporating ground glass
70. Internal composition of 20-year-old fly ash and slag-blended ordinary portland cement pastes10.1111/j.1551-2916.2008.02783.x ↗
71. Hydration of Portland cement with high replacement by siliceous fly ash10.1016/j.cemconres.2012.06.009 ↗
72. Effect of temperature on the hydration of Portland cement blended with siliceous fly ash10.1016/j.cemconres.2013.07.006 ↗
73. ASR prevention—effect of aluminum and lithium ions on the reaction products10.1016/j.cemconres.2015.06.002 ↗
74. The effect of aluminum in solution on the dissolution of amorphous silica and its relation to cementitious systems10.1111/jace.12098 ↗
75. Effect of different ions on dissolution rates of silica and feldspars at high pH10.1016/j.cemconres.2021.106644 ↗
76. ASR in concrete with supplementary cementitious materials—effect of pore solution composition on damage
77. Mitigation of alkali-silica reaction by limestone calcined clay cement (LC3)10.1016/j.cemconres.2020.106176 ↗
78. The distribution, structure, and chemical composition of alkali-silica gels in calcined clay concretes10.3390/buildings15020218 ↗
79. Impact of alkali release from aggregates on pore solution of mortars