Activity of silica fume and dealuminated kaolin at different temperatures
Source abstract
Abstract
Abstract Silica fume (SF) and dealuminated kaolin (DK) were investigated for their pozzolanic activities. The kinetics of the SF–lime and DK–lime reactions were investigated in pastes at room temperature, 100°C, and 180°C by the determination of unreacted lime and combined water. The hydration products were identified by X-ray diffraction (XRD). The variations in mechanical properties were correlated with the reaction kinetics and the hydration products formed. DK exhibited higher reactivity than SF at all temperatures studied. Tobermorite was formed at 100°C in the high-lime DK mix at 14 days and extensively formed by autoclaving at 180°C curing due to the presence of Al and sulfate in the DK. The very low C/S ratios of SF mixes and low-lime DK mix prevent tobermorite formation and promote the formation of poorly crystalline C-S-H with a higher surface area.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Clay minerals and soil interactions · Soil and Unsaturated Flow · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. ASTM C595, Standard specification for blended hydraulic cements, 1998.
2. Chardra · 1997 · 242
3. Taylor · 1990 · 367
4. Bessey · 1964 · vol. II · 107
5. Mechanical properties evolution during autoclaving process of aerated concrete using slag: I. Tobermorite formation and reaction behavior of slag10.1111/j.1151-2916.1994.tb07101.x ↗
6. Hydration reactivity of crystalline and vitrified diopside under hydrothermal conditions10.1111/j.1151-2916.1990.tb05259.x ↗
7. Formation of jennite from fumed silica10.1016/0008-8846(80)90031-9 ↗
8. Characterization and evaluation the pozzolanic activity of Egyptian industrial by-products: I. Silica fume and dealuminated kaolin10.1016/S0008-8846(00)00485-3 ↗
9. A study of the hydration of lime–pozzolan binders10.1023/A:1010101126587 ↗
10. Effect of the ‘Pozzolit’ active mineral admixture on the properties of cement mortars and concretes: Part 2. Pozzolanic activity10.1016/0008-8846(96)00082-8 ↗
11. Reactivity of SiO2 fume from ferrosilicon production with Ca(OH)2 under hydrothermal conditions10.1016/0008-8846(85)90018-3 ↗
12. Influence of slag substitution on some properties of sand–lime aerated concrete10.1007/BF00553265 ↗
13. ASTM C 373-88, Water absorption, bulk density, apparent porosity and apparent specific gravity of fired whiteware products, 1999.
14. ASTM C114, Standard test methods for chemical analysis of hydraulic cement, 1999.
15. Analyzing SO3-bearing phases in hydrated cement
16. Effect of hydration temperature on cement paste structure, microstructural development during hydration of cement
17. Interaction between gypsum and CSH-phase formed in C3S hydration
18. The incorporation of minor and trace elements into calcium silicate hydrate (C-S-H) gel in hydrated cement paste10.1016/0008-8846(93)90143-W ↗
19. Proposed structure for calcium silicate hydrate gel10.1111/j.1151-2916.1986.tb07446.x ↗
20. Autoclaved lime-quartz materials: I. Some factors influencing strength10.1016/0008-8846(77)90111-9 ↗
21. Influence of SO42− ions on the formation of 11Å-tobermorite
22. N.Y. Mostafa, Factors effecting the hydrothermal reactions in CaO–SiO2–H2O system, MSc thesis, Suez Canal University, December 1995.
23. Formation of 11Å tobermorite from mixtures of lime and colloidal silica with quartz10.1016/0008-8846(78)90001-7 ↗
24. Preparation and characterization of lime–silica solids10.1021/ie990511y ↗
25. Characterization, surface area, and porosity analyses of the solids obtained by acid leaching of a saponite10.1021/la950501b ↗
26. A detailed model of local structure and silanol hydrogen bonding of silica gel surface10.1021/jp9629046 ↗
27. Synthesis of normal and anomalous tobermorite10.1016/0008-8846(77)90071-0 ↗
28. Synthesis of tobermorite: NMR spectroscopy and analytical electron microscopy
29. Effect of starting materials on the synthesis of tobermorite