Formation of sodium iron silicate hydrate (N-F-S-H) in Fe-rich cementitious systems
Source abstract
Abstract
Na 2 O-Fe 2 O 3 -SiO 2 -H 2 O samples with initial bulk Fe/Si molar ratios of 0.1, 0.3, 0.5, 0.8, and 1.0 were produced by mixing high-purity FeCl₃·6H₂O, and NaOH with fumed silica and water. They were equilibrated at a pH between 10.7 and 13.2 at 25 and 50 °C. Phase evolution was investigated over 1 year at 25 °C and 6 months at 50 °C using XRD, FTIR, SEM-EDS and ICP-OES. At 25 °C, sodium iron silicate hydrate (N-F-S-H) initially formed, with FTIR confirming the destabilisation of siliceous ferrihydrite and no evidence of crystalline Fe hydroxides such as goethite ( α- FeO(OH)). At 50 °C, nontronite (Na x (Si 4- x Fe x 3+ )Fe 2 3+ O 10 (OH) 2 ) with 0.5 < x < 1.35 appeared after 180 days of equilibration. The progressive development of characteristic nontronite reflections (at 33 and 41° 2-theta) from the initial N-F-S-H matrix suggests that N-F-S-H acts as a poorly crystalline precursor and evolves toward nontronite. The results provide new insight into the stability of Fe-bearing solid phases in alkaline environments and have implications for the use of Fe-rich materials in civil engineering.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Future and emerging supplementary cementitious materials10.1016/j.cemconres.2023.107199 ↗
2. P. Termkhajornkit, B. Mathieu, K. Kollias, K. Evans, Holcim Innovation Center, (n.d.).
3. Bauxite residue in cement and cementitious applications: current status and a possible way forward10.1016/j.resconrec.2013.01.005 ↗
4. One-part geopolymers based on thermally treated red mud/NaOH blends10.1111/jace.13231 ↗
5. Pozzolanic activity of thermally treated bauxite residue in blends with ordinary Portland cement
6. The influence of curing conditions on the mechanical properties and leaching of inorganic polymers made of fayalitic slag10.1007/s11705-017-1622-6 ↗
7. Identifying hotspots of environmental impact in the development of novel inorganic polymer paving blocks from bauxite residue10.1016/j.resconrec.2018.07.006 ↗
8. Modifications of basic-oxygen-furnace slag microstructure and their effect on the rheology and the strength of alkali-activated binders10.1016/j.cemconcomp.2018.12.013 ↗
9. Co-calcination of bauxite residue with kaolinite in pursuit of a robust and high-quality supplementary cementitious material10.3389/fmats.2022.913151 ↗
10. Solid solution between al-ettringite and fe-ettringite (Ca6[Al1−xFex(OH)6]2(SO4)3·26H2O)10.1016/j.cemconres.2009.03.001 ↗
11. Synthesis and stability of silica-substituted hydrogarnet ca3 al2 si3-x o12-4x (OH)4x10.1680/adcr.1991.4.1.1 ↗
12. Hydration states of AFm cement phases10.1016/j.cemconres.2015.02.011 ↗
13. A Cementitious Compound with Composition 3CaO.Al2 O3 .CaCO3 .11H2 O10.1107/S0108270198004223 ↗
14. Friedel’s salt, Ca2Al(OH)6(Cl,OH)·2H2O: its solid solutions and their role in chloride binding10.1016/S0008-8846(98)00162-8 ↗
15. Solubility of fe–ettringite (Ca6[Fe(OH)6]2(SO4)3·26H2O)10.1016/j.gca.2007.09.035 ↗
16. Iron in carbonate containing AFm phases10.1016/j.cemconres.2010.11.017 ↗
17. Stability of monosulfate in the presence of iron10.1111/j.1551-2916.2012.05335.x ↗
18. Synthesis and characterization of hydrogarnet Ca3(AlxFe1−x)2(SiO4)y(OH)4(3−y)10.1016/j.cemconres.2014.02.001 ↗
19. Fe-containing phases in hydrated cements10.1016/j.cemconres.2013.12.012 ↗
20. Solubility and thermodynamic properties of carbonate-bearing hydrotalcite—pyroaurite solid solutions with a 3: 1 Mg/(Al+Fe) mole ratio10.1346/CCMN.2011.0590301 ↗
21. Investigation about iron(III) incorporation into layered double hydroxides: compositional and structural properties of Mg2FeyAl(1−y)(OH)6-cl and Zn2FeyAl(1−y)(OH)6-cl10.1016/j.jallcom.2021.161184 ↗
22. Pyroaurite-like phases (Mg-Fe3+ LDH) synthesis and solubility10.1016/j.cemconres.2024.107739 ↗
23. Spectroscopic investigations on structural incorporation pathways of FeIII into zeolite frameworks in cement-relevant environments10.1016/j.cemconres.2020.106304 ↗
24. Geopolymers and related alkali-activated materials10.1146/annurev-matsci-070813-113515 ↗
25. The fate of iron during the alkali-activation of synthetic (CaO-)FeOx-SiO2 slags: an FeK-edge XANES study10.1111/jace.15354 ↗
26. Alkali-activation of CaO-FeOx-SiO2 slag: formation mechanism from in-situ x-ray total scattering10.1016/j.cemconres.2019.04.019 ↗
27. Inorganic polymers from CaO-FeOx-SiO2 slag: the start of oxidation of fe and the formation of a mixed valence binder10.3389/fmats.2019.00212 ↗
28. Influence of CaO/FeO ratio on the formation mechanism and properties of alkali-activated fe-rich slags10.1016/j.cemconres.2021.106466 ↗
29. The state of Fe3+ in the C–F–A–S–H system with varying Fe/Si and Ca/Si ratios10.1039/D3TA01929B ↗
30. The effect of the steel–concrete interface on chloride-induced corrosion initiation in concrete: a critical review by RILEM TC 262-SCI10.1617/s11527-019-1387-0 ↗
31. Speciation of iron(II/III) at the iron-cement interface: a review10.1617/s11527-023-02115-x ↗
32. Steel corrosion in concrete – achilles heel for sustainable concrete?10.1016/j.cemconres.2023.107239 ↗
33. Precipitation of corrosion products in macroscopic voids at the steel–concrete interface: observations, mechanisms and research needs10.1617/s11527-025-02614-z ↗
34. Structural investigations of synthetic ferrihydrite nanoparticles doped with si10.1016/j.ssc.2004.03.022 ↗
35. Properties of impurity-bearing ferrihydrite III. Effects of si on the structure of 2-line ferrihydrite10.1016/j.gca.2014.02.018 ↗
36. The influence of silicate on transformation pathways of synthetic 2-line ferrihydrite10.1007/s10973-016-5345-6 ↗
37. The influence of silicon on the formation and transformation of corrosion products10.1016/j.cemconres.2024.107554 ↗
38. Corrosion behavior of iron plates in cementitious solution at 80°c in anaerobic conditions10.1016/j.corsci.2020.108650 ↗
39. Nuclear waste glasses - how durable?10.2113/gselements.2.6.357 ↗
40. Radionuclides containment in nuclear glasses: an overview10.1515/ract-2016-2658 ↗
41. The fate of si and fe while nuclear glass alters with steel and clay10.1038/s41529-021-00160-x ↗
42. SON68 nuclear glass dissolution kinetics: current state of knowledge and basis of the new GRAAL model10.1016/j.jnucmat.2008.06.044 ↗
43. Kinetic study of fe silicates formation during iron corrosion in deaerated and alkaline si-containing solutions at 50°c10.1016/j.corsci.2022.110846 ↗
44. Methodology for pH measurement in high alkali cementitious systems10.1016/j.cemconres.2020.106122 ↗
45. A structural model for natural siliceous ferrihydrite10.1346/CCMN.1992.0400607 ↗
46. Study of short range structure of amorphous silica from PDF using ag radiation in laboratory XRD system, raman and NEXAFS10.1016/j.jnoncrysol.2018.02.037 ↗
47. Structural properties and hyperfine characterization of sn-substituted goethites10.1016/j.matchemphys.2012.01.075 ↗
48. Mineralogy and reactivity of amorphous si-ferrihydrites10.1016/0167-2738(90)90443-U ↗
49. Comparing amorphous silica, short-range-ordered silicates and silicic acid species by FTIR10.1038/s41598-022-15882-4 ↗
50. Weast · 1987
51. A new approach to determine and quantify structural units in silicate glasses using micro-reflectance Fourier-transform infrared spectroscopy10.2138/am.2006.2075 ↗
52. The application of infrared spectroscopy to a study of phosphoric and tannic acids interactions with magnetite (fe304), goethite (a-FeOOH) and lepidocrocite (y-FeOOH)10.1016/S0010-938X(97)00060-7 ↗
53. Oxidation-reduction mechanism of iron in dioctahedral smectites: I. Crystal chemistry of oxidized reference nontronites10.2138/am-2000-0114 ↗
54. Hydrothermal synthesis, between 75 and 150°c, of high-charge, ferric nontronites10.1346/CCMN.2008.0560303 ↗
55. Influence of aqueous si and fe speciation on tetrahedral Fe(III) substitutions in nontronites: a clay synthesis approach10.1346/CCMN.2016.0640309 ↗
56. Experimental evidence of the metastability of ferric smectite10.1016/j.gca.2019.08.040 ↗
57. Hydrothermal synthesis of dioctahedral smectites: the Al–Fe3+ chemical series. Part II: crystal-chemistry10.1016/j.clay.2014.11.014 ↗
58. Synthesis and characterization of Fe(III)-Fe(II)-Mg-Al smectite solid solutions and implications for planetary science10.2138/am-2020-7419CCBYNCND ↗
59. Cristallogenèse expérimentale des smectites magnésiennes: hectorite, stévensite10.3406/bulmi.1980.7423 ↗
60. Synthesis and crystallogenesis of ferric smectite by evolution of Si-Fe coprecipitates in oxidizing conditions10.1180/claymin.1987.022.2.09 ↗
61. Temperature effects on the crystallinity of synthetic nontronite and implications for nontronite formation in columbia river basalts10.1346/CCMN.2014.0620202 ↗