Rice husk ash as both pozzolanic admixture and internal curing agent in ultra-high performance concrete
Source abstract
Abstract
Abstract The present study investigated the effects of mesoporous amorphous rice husk ash (RHA) on compressive strength, portlandite content, autogenous shrinkage and internal relative humidity (RH) of ultra-high performance concretes (UHPCs) with and without ground granulated blast-furnace slag (GGBS) under different treatments. The results were compared with those of UHPCs containing silica fume (SF). Because of the mesoporous structure, RHA can absorb an amount of aqueous phase to decrease the free water content and to supply thereafter water for further hydrations of cementitious materials. Hence, compressive strength of RHA-blended samples is enhanced. The highly water absorbing RHA delays and slows down the decrease in the internal RH (self-desiccation) of UHPCs, and hence strongly mitigates autogenous shrinkage of UHPCs compared to SF. The combination of GGBS and RHA or SF improves the properties of UHPC. These results suggest that RHA acts as both highly pozzolanic admixture and internal curing agent in UHPC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Composition of reactive powder concretes10.1016/0008-8846(95)00144-2 ↗
2. Park JJ, Kang ST, Koh KT, Kim SW. Influence of the ingredients on the compressive strength of UHPC as a fundamental study to optimize the mixing proportion. In: Proceedings of the 2nd international symposium on ultra high performance concrete, Kassel, Germany; 2008. p. 105–112.
3. Graybeal BA. Characterization of the behaviour of ultra-high performance concrete. Ph.D. Thesis, USA, University of Maryland; 2005.
4. Resplendino J. State of the art of design and construction of UHPFRC structures in France. In: Proceedings of Hipermat 2012 – the 3rd international symposium on UHPC and nanotechnology for high performance construction materials, Kassel, Germany; 2012. p. 27–41.
5. Schmidt M. Sustainable building with UHPC – coordinated research program in Germany. In: Proceedings of Hipermat 2012 – the 3rd international symposium on UHPC and nanotechnology for high performance construction materials, Kassel, Germany; 2012. p. 17–25.
6. Hydration kinetics, change of relative humidity, and autogenous shrinkage of ultra-high-strength concrete10.1016/S0008-8846(99)00022-8 ↗
7. Autogenous deformations and viscoelasticity of UHPFRC in structures. Part I: experimental results10.1680/macr.2006.58.3.135 ↗
8. Why does Ultrahigh-Performance Concrete (UHPC) exhibit such low shrinkage and such low creep?
9. Autogenous shrinkage of concrete with super-absorbent polymer
10. Mechtcherine V, Dudziak L, Hempel S. Mitigating early age shrinkage of ultra-high performance concrete by using Super Absorbent Polymers (SAP). In: Proceedings of the 8th international conference on creep, shrinkage and durability mechanics of concrete and concrete structures. London: Taylor & Francis; 2008. p. 847–853.10.1201/9780203882955.ch115 ↗
11. Soliman A. Early-age shrinkage of ultra high performance concrete: mitigation and compensation mechanisms. Ph.D. Thesis, Canada, The university of Western Ontario; 2011.
12. Kovler K, Jensen OM. Internal curing of concrete. State-of-the-art report of RILEM technical committe 196-ICC. France: RILEM Publications S.A.R.L.; 2007.
13. Dudziak L, Mechtcherine V. Mitigation of volume changes of Ultra-high performance concrete (UHPC) by using super absorbent polymers. In: Proceedings of the 2nd international symposium on ultra high performance concrete, Kassel, Germany; 2008. p. 425–432.
14. Investigations on the workability and microstructure development of UHPC; Part 2: influence of admixtures and curing on the microstructure of ultra-high strength concretes
15. Mehta PK. Rice husk ash – a unique supplementary cementing material. In: Advances in concrete technology. 2nd ed. CANMET; 1994. p. 419–444.
16. Reply to the discussion by Ayhan Demirbas of the paper “Study on the pozzolanic properties of rice husk ash by hydrochloric acid pretreatment”10.1016/j.cemconres.2004.10.009 ↗
17. Mesoporous structure and pozzolanic reactivity of rice husk ash in cementitious system10.1016/j.conbuildmat.2013.02.004 ↗
18. Review processing, properties and applications of reactive silica from rice husk—an overview10.1023/A:1025157114800 ↗
19. A structural investigation relating to the pozzolanic activity of rice husk ashes10.1016/j.cemconres.2007.10.004 ↗
20. Study on the pozzolanic properties of rice husk ash by hydrochloric acid pretreatment10.1016/j.cemconres.2003.09.005 ↗
21. Comparison of two processes for treating rice husk ash for use in high performance concrete10.1016/j.cemconres.2009.05.006 ↗
22. Particle size effect on the strength of rice husk ash blended gap-graded Portland cement concrete10.1016/j.cemconcomp.2004.05.002 ↗
23. Van V-T-A, Ludwig H-M. Proportioning optimization of UHPC containing rice husk ash and ground granulated blast-furnace slag. In: Proceedings of Hipermat 2012 – 3rd international symposium on ultra-high performance concrete and nanotechnology for high performance construction materials, Kassel, Germany; 2012. p. 197–205.
24. Nguyen VT. Rice husk ash as a mineral admixture for ultra high performance concrete. Ph.D. Thesis, The Netherlands, Delft University; 2011.
25. Effects of RHA on autogenous shrinkage of Portland cement pastes10.1016/j.cemconcomp.2008.06.014 ↗
26. Rizwan SA. High-performance mortars and concretes using secondary raw materials. Ph.D. Thesis, Germany, Faculty of Maschinenbau, Verfahrens-und Energietechnik der Technischen Bergakademie Freiberg; 2006.
27. Rice husk ash concrete: the effect of RHA average particle size on mechanical properties and drying shrinkage
28. Use of the second-derivative differential thermal curve in the evaluation of cement-quartz pastes with metakaolin addition autoclaved at 180°C10.1016/S0040-6031(97)00409-7 ↗
29. Ramachandran · 2002
30. Schachinger I, Schmidt K, Heinz D, Schießl P. Early-age cracking risk and relaxation by restrained autogenous deformation of ultra high performance concrete. In: The 6th international symposium on utilization of high strength/high performance concrete, Leipzig, Germany; 2002. p. 1341–1354.
31. Hydration and microstructure of ultra high performance concrete incorporating rice husk ash10.1016/j.cemconres.2011.06.009 ↗
32. Heinz D, Ludwig H-M. Heat treatment and the risk of DEF Delayed Ettringite Formation in UHPC. In: Proceedings of the 1st international symposium on ultra high performance concrete, Kassel, Germany; 2004. p. 717–730.
33. Schachinger I, Hilbig H, Stengel T. Effect of temperature at an early age on the long-term strength development of UHPC. In: Proceedings of the 2nd international symposium on ultra high performance concrete, Kassel, Germany; 2008. p. 205–212.
34. Autogenous shrinkage in high-performance cement paste: an evaluation of basic mechanisms10.1016/S0008-8846(02)00890-6 ↗