journal article·2024-01Open access

Accelerated testing of soft soldered, small-diameter, thin-walled CuNi pipes subjected to cyclic internal pressure loading

Sophie A.M. McNair, Kamil Cichy, Jerome Daguin, Antti Onnela, Alexander J.G. Lunt

Abstract

Small-diameter, thin-walled pipes have applications in a wide range of industries including high-energy physics, heat transfer, nuclear, medical and communications. However, there are currently no standards that exist for permanently joining these components either via welding (melting the base material) or soldering. As such it is difficult to determine the likely performance of a thin-walled pipe connection. Porosity is largely inevitable in soldered joints and is a determining factor in the performance of a connection. This study focused on characterisation of failure initiation and propagation within soft soldered CuNi thin-walled pipe joints under cyclic internal pressure loading. A step-stress accelerated life testing regime (SSALT) was developed to simulate the loads the joints would experience over their operational lifetime, in a shorter timescale. 10 soldered joints were studied in total, with varying levels of porosity within the soldered joints prior to testing. Pressurised Nitrogen gas was used to internally pressurise the samples, with cyclic loading between atmospheric conditions and a prescribed maximum pressure value. The results of the SSALT showed that the soldered samples experienced early failure through crack initiation and propagation through the solder. Cracks, or failures, were seen to initiate from existing voids, or porosity, within the soft-soldered joints. From this work, it can be concluded that the performance of soft-soldered joints under cyclic, internal pressure loading is strongly influenced by the presence of voids that are created during the manufacture of such soldered connections.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Manufacturing technologies and joining methods of metallic thin-walled pipes for use in high pressure cooling systems10.1007/s00170-021-07982-8 ↗
2. Review on advances in metal micro-tube forming10.3390/met9050542 ↗
3. Effect of forming conditions on microstructure and room-temperature mechanical characterization of Zn–22Al superplastic microtubes fabricated by direct extrusion10.1016/j.msea.2022.143160 ↗
4. Characterization of a high performance ultra-thin heat pipe cooling module for mobile hand held electronic devices10.1007/s00231-017-2022-7 ↗
5. A review of small heat pipes for electronics10.1016/j.applthermaleng.2015.11.048 ↗
6. Formability assessment of plastic joining by compression instability for thin-walled tubes10.1007/s00170-018-2128-1 ↗
7. Chapter 13 - weld microstructures
8. 3.05 - nonlinear finite element analysis and applications to welded structures
9. 9 - a comparative analysis of techniques used for joining intermetallic MMCs
10. Vacuum brazing of stainless steel depending on the surface preparation method and temperature of the process10.24425/amm.2019.126210 ↗
11. Induction brazing of thin-walled pipes from AISI 304 steel using copper-based solder
12. 2021
13. 2023
14. 2021
15. The effect of porosity on strain evolution and failure of soldered, small-diameter, thin-walled metallic pipes10.1016/j.jmrt.2022.12.088 ↗
16. Brazing residual stresses in components of different metallic materials10.1016/0921-5093(94)91116-9 ↗
17. Chapter 5 - mechanical behavior of metal pipes under internal and external pressure
18. The response of pipes and supports to internal pressure loads generated by gaseous detonations10.1115/1.1427342 ↗
19. Plastic collapse of pipe bends under combined internal pressure and in-plane bending10.1016/j.ijpvp.2004.09.005 ↗
20. Reliability assessments of corroded pipelines based on internal pressure – a review10.1016/j.engfailanal.2019.01.064 ↗
21. Pressure cycling monitoring helps ensure the integrity of energy pipelines
22. Experimental study on cyclic creep of pipes10.1007/s11223-022-00413-3 ↗
23. Numerical investigation of pressure-cycling-induced fatigue failure of wrinkled energy pipelines10.1115/1.4051545 ↗
24. Fatigue analysis of damaged steel pipelines under cyclic internal pressure10.1016/j.ijfatigue.2008.09.006 ↗
25. Fatigue crack propagation of welded steel pipeline under cyclic internal pressure by bézier extraction based XIGA10.1061/(ASCE)PS.1949-1204.0000633 ↗
26. Creep pores in welded joints of steam pipelines10.1007/s11223-023-00523-6 ↗
27. Optimal simple step stress accelerated life test design for reliability prediction10.1016/j.jspi.2008.05.046 ↗
28. Accelerated life testing - step-stress models and data analyses10.1109/TR.1980.5220742 ↗
29. Multiple-steps step-stress accelerated life test
30. Modern high-availability multi-stage power distribution system for the CMS phase-2 upgrade10.1088/1748-0221/18/02/C02053 ↗
31. Contardo · 2015
32. 2019
33. CO2 cooling for the CMS tracker at SLHC
34. Evaporative CO2 cooling system for the upgrade of the CMS pixel detector at CERN
35. Material budget imaging with multi-GeV electrons - calibration and applications for 2D material scanning10.1088/1742-6596/2374/1/012007 ↗
36. CMS Tracker alignment and material budget measurements
37. Estimation of the material budget of the CMS Tracker using the triplet method
38. Two-phase flow patterns and flow-pattern maps: fundamentals and applications10.1115/1.2955990 ↗
39. Fundamental issues related to flow boiling in minichannels and microchannels10.1016/S0894-1777(02)00150-4 ↗
40. Characteristics of gas-liquid two-phase flow in a capillary tube10.1016/0029-5493(93)90092-N ↗
41. The prediction of flow pattern maps in minichannels10.1615/MultScienTechn.v19.i1.20 ↗
42. Factors influencing the formation of voids in chip component solder joints
43. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
44. Numerical assessment of the effect of void morphology on thermo-mechanical performance of solder thermal interface material10.1016/j.applthermaleng.2013.12.006 ↗
45. Effect of soldering temperature on the reliability of Sn-Ag-Cu lead-free solder joints10.1007/s11664-020-08715-5 ↗
46. Effect of voids on the reliability of BGA/CSP solder joints
47. Effect of aging on the microstructure and shear strength of SnPbAg/Ni-P/Cu and SnAg/Ni-P/Cu solder joints10.1007/s11664-004-0272-x ↗
48. Analysis of the redeposition of AuSn4 on Ni/Au contact pads when using SnPbAg, SnAg, and SnAgCu solders10.1007/s11664-005-0186-2 ↗
49. Microstructure, joint strength and failure mechanisms of SnPb and Pb-free solders in BGA packages10.1109/TEPM.2002.801649 ↗
50. A metallurgical assessment of SnPbAg solder for GaAs power devices10.1007/s11837-999-0024-8 ↗
51. Formation of intermetallic compounds in SnPbAg, SnAg, and SnAgCu solders on Ni/Au metallization: physical metallurgical and materials science10.1007/s11661-001-0058-1 ↗
52. Struers