Abstract

Al–Cu–Li alloys have shown great potential for aerospace application due to their good combination of high strength and low density, but their high planar anisotropy have always hindered their application. In the present work, the influence of different deformation processes, including hot rolling (HR), cold rolling (CR), hot rolling + cold rolling (HR + CR), hot rolling + intermediate annealing + cold rolling (HR + IA + CR) on the microstructure and property anisotropy is systematically investigated for a 2195 Al–Cu–Li alloy. Among the four rolling processes, the HR sample exhibits the lowest yield strength, the highest elongation and the highest anisotropy level. The CR and HR + CR samples have a higher yield strength, decreased elongation and anisotropy level. While the HR + IA + CR sample achieves the combination high yield strength, good elongation and the lowest anisotropy level. The different rolling processes can affect the number density and size of the coarse Al 7 Cu 2 Fe phase (>1 μm), which can promote the recrystallization by PSN mechanism. As the number density of Al 7 Cu 2 Fe phase in the four samples follow: HR + IA + CR > CR > HR + CR > HR. The HR + IA + CR sample with the highest PSN particles density exhibits highest level of recrystallization and random texture distribution, giving rise to the low anisotropy of the alloy. The low number density of PSN particle and the occurrence of dynamic recrystallization suppress the recrystallization of the HR sample during solution treatment, resulting in strong anisotropy of the alloy. These results can provide key information for optimizing the mechanical properties of Al–Cu–Li alloys for aerospace applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Alloying and micro-alloying in Al-Cu-Li series alloys
2. Effects of heat treatment and pre-stretching on the mechanical properties and microstructure evolution of extruded 2050 Al–Cu–Li alloy
3. The evolution of Al-Li base products for aerospace and space applications
4. Aluminum alloys in aircraft in the periods of 1970 - 2000 and 2001 - 2015
5. Fabrication methods to manufacture isotropic Al-Li alloys and products for space and aerospace applications10.1016/S0921-5093(98)00827-2 ↗
6. Texture and anisotropy in Al-Li alloy 2195 sheet and near-net-shape extrusions10.1016/S0921-5093(98)00834-X ↗
7. Effect of initial orientation on the anisotropy in microstructure and mechanical properties of 2195 Al-Li alloy sheet during hot tensile deformation10.3390/ma16145012 ↗
8. Investigation of microstructure, texture evolution and plastic anisotropy of short-time homogenized MS-DC cast 2024 aluminum alloy during rolling and annealing10.1016/j.msea.2024.146392 ↗
9. Deformation, recrystallization and plastic anisotropy of asymmetrically rolled aluminum sheets10.1016/j.msea.2010.09.023 ↗
10. The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys10.1016/j.actamat.2012.12.041 ↗
11. Effect of pre-deformation on Creep age forming of AA2219 plate: springback, microstructures and mechanical properties10.1016/j.jmatprotec.2015.10.030 ↗
12. Effect of pre-deformation on microstructure and mechanical properties of 2219 aluminum alloy sheet by thermomechanical treatment10.1016/S1003-6326(12)61733-6 ↗
13. Effect of cross-rolling on microstructure and texture evolution and tensile behavior of aluminium-copper-lithium (AA2195) alloy10.1016/j.msea.2018.10.089 ↗
14. Mechanical properties and microstructure evolution of an Al-Cu-Li alloy subjected to rolling and aging
15. Microstructure evolution, mechanical response, and corrosion resistance for a 2195 Al-Li alloy under different rolling reductions during cryorolling10.1016/j.jallcom.2024.174973 ↗
16. Enhanced formability of Al-Mg-Si-Zn alloy sheet via dislocation structure and texture during cold rolling10.1016/j.jmrt.2023.12.246 ↗
17. The dependence of microstructure, texture evolution and mechanical properties of Al-Mg-Si-Cu alloy sheet on final cold rolling deformation10.1016/j.jallcom.2015.10.070 ↗
18. Texture, microstructure and mechanical properties of 6111 aluminum alloy subject to rolling deformation
19. Aging behavior of Al-Li-(Cu, Mg) alloys processed by different deformation methods10.1016/j.matdes.2020.109139 ↗
20. Influence of different rolling processes on microstructure and strength of the Al-Cu-Li alloy AA219510.1016/j.pnsc.2021.10.009 ↗
21. Effect of intermediate annealing-on texture evolution and plastic anisotropy in an Al-Mg autobody alloy10.1007/s11661-000-0057-7 ↗
22. Research on the grain structure and performance control of spray-deposited 2195 aluminum-lithium alloy rolled plates. Rare. Metal
23. Abnormal grain growth of 2196 Al-Cu-Li alloy weld seams during extrusion and heat treatment10.1016/j.jallcom.2021.159043 ↗
24. Effect of solution time on microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloys10.1016/j.msea.2015.07.059 ↗
25. Controlling grain structure and texture in Al-Mn from the competition between precipitation and recrystallization10.1016/j.actamat.2017.09.032 ↗
26. Relationship of particle stimulated nucleation, recrystallization and mechanical properties responding to Fe and Si contents in hot-extruded 7055 aluminum alloys10.1016/j.jmst.2019.07.014 ↗
27. Effect of particles on texture banding in an aluminium alloy10.1016/j.scriptamat.2009.09.032 ↗
28. Influence of homogenization treatment on microstructure and recrystallization behavior of 2195 Al-Li alloy10.1016/S1003-6326(23)66257-0 ↗
29. Microstructural evolution of aluminum alloy during friction stir welding under different tool rotation rates and cooling conditions10.1016/j.jmst.2018.12.024 ↗
30. The effect of Fe content on recrystallization texture evolution, microstructures, and earing of cold rolled continuous cast AA5052 alloy sheets10.1007/s11661-016-3357-2 ↗
31. A model for the yield strength of overaged Al-Zn-Mg-Cu alloys10.1016/S1359-6454(03)00363-X ↗
32. Hall-Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
33. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al-Cu-Li alloy10.1016/j.msea.2014.03.024 ↗
34. Microstructural design of high-strength aluminum alloys10.1361/105497198770341734 ↗
35. Quantification and modelling of the microstructure/strength relationship by tailoring the morphological parameters of the T1phase in an Al-Cu-Li alloy10.1016/j.actamat.2014.04.046 ↗
36. Effect of the aging process and pre-deformation on the precipitated phase and mechanical properties of 2195 Al-Li alloy10.1016/j.msea.2021.142394 ↗
37. Microstructure evolution and mechanical properties of the 2195 Al-Li alloy via different annealing and ramp heating-up treatments10.3390/met10070910 ↗
38. Strength and structure variation of 2195 Al-Li alloy caused by different deformation processes of hot extrusion and cold-rolling10.1016/S1003-6326(20)65258-X ↗