Effect of cement type and limestone particle size on the durability of steam cured self-consolidating concrete
Source abstract
Abstract
Abstract This paper describes a laboratory program to investigate the influence of cement and limestone filler (LF) particle size on the hardened properties and durability performance of steam cured self-consolidating concrete. In addition, the interplay between cement type and LF particle size was investigated. CSA (Canadian Standards Association) Type GU (General Use) and HE (High Early-strength) cements were used with 5% silica fume (SF) [1]. The water-to-cement ratio was 0.34. LF with two nominal particle sizes of 17 μm and 3 μm, which correspond to Blaine fineness of 475 and 1125 m2/kg, respectively, were used. In addition to fresh concrete properties, hardened properties including compressive strength, elastic modulus, ultrasonic pulse velocity and density were measured at 12 h and 16 h, and at 3, 7 and 28 days. Indicators of durability performance including rapid chloride permeability testing (RCPT), sulfate resistance, linear shrinkage, salt scaling resistance and freeze-thaw resistance were evaluated. The results showed that LF improved the 12 and 16-h strength with no influence on later age strength (i.e., 3–28 days). The linear shrinkage and RCPT decreased with the addition of LF. This reduction was linked to the production of calcium mono-carboaluminate. LF did not impact the sulfate resistance, salt scaling resistance or freeze-thaw resistance of concrete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. CSA A3000 · 2013
2. Correlating rheology of self-consolidating concrete to corresponding concrete-equivalent mortar
3. Daczko · 2006 · 637
4. Performance of self-compacting concrete containing different mineral admixtures10.1007/s12205-013-1882-8 ↗
5. Study of limestone addition on the mechanical and rheological characteristics in the SCC
6. Khayat · 2009 · vol. 628
7. Adding limestone fines as cementitious paste replacement to improve tensile strength, stiffness and durability of concrete10.1016/j.cemconcomp.2015.02.006 ↗
8. De Schutter · 2007
9. Hydration kinetics and compressive strength of steam-cured cement pastes and mortars containing limestone filler10.1016/j.conbuildmat.2016.03.031 ↗
10. Cement with interground additives - capabilities and environmental relief: part 1
11. Nisbet · 1996 · 1
12. Effect of limestone filler as mineral addition in self-compacting concrete
13. Shi · 2004 · 115
14. Influence of paste volume, addition content and addition type on shrinkage cracking of self-compacting concrete
15. Effects in the solubility of CaCO3: experimental study and model description10.1016/j.fluid.2012.03.020 ↗
16. Simple methods to estimate the influence of limestone fillers on reaction and property evolution in cementitious materials10.1016/j.cemconcomp.2013.05.002 ↗
17. Hawkins · 2003
18. Adding limestone fines as cement paste replacement to reduce shrinkage of concrete10.1680/macr.13.00028 ↗
19. Babuskin · 1985
20. Optimization of steam-curing regime for high-strength, self-consolidating concrete for precast, prestressed concrete applications10.15554/pcij.06012012.48.62 ↗
21. ASTM C187 · 2011
22. ASTM C191 · 2008
23. ASTM C1702 · 2009
24. Maria · 2011 · 13
25. Evaluation of the hydration of Portland cement containing various carbonates by means of thermal analysis
26. Modeling the influence of limestone filler on cement hydration using CEMHYD3D10.1016/j.cemconcomp.2005.10.006 ↗
27. Hydration of calcium aluminate cements in the presence of calcium carbonate10.1127/ejm/8/1/0129 ↗
28. Determining the slag fraction, water/binder ratio and degree of hydration in hardened cement pastes10.1016/j.cemconres.2013.12.002 ↗
29. Investigation of blended cement hydration by isothermal calorimetry and thermal analysis10.1016/j.cemconres.2004.10.027 ↗
30. ASTM C109 · 2012
31. CSA A23.1/A23.2 · 2009
32. ASTM C1621 · 2009
33. ASTM C1610 · 2010
34. MTO LS-440 · 2007
35. ASTM C231 · 2010
36. ASTM C597 · 2009
37. ASTM C469 · 2004
38. ASTM C138 · 2010
39. ASTM C1202 · 2010
40. ASTM C1012 · 2010
41. ASTM C666 · 2008
42. Role of the filler on Portland cement hydration at early ages10.1016/j.conbuildmat.2011.07.021 ↗
43. The effects of limestone addition, clinker type and fineness on properties of Portland cement10.1016/S0008-8846(00)00427-0 ↗
44. Siddique · 2011 · 67
45. Hydration kinetics modeling of Portland cement considering the effects of curing temperature and applied pressure10.1016/j.cemconres.2009.01.014 ↗
46. De Weerdt · 2009 · 257
47. Influence of limestone filler and viscosity-modifying admixture on the porous structure of self-compacting concrete
48. Interaction between ettringite and polynapthalene sulfonate superplasticizer in cementitious paste10.1016/S0008-8846(01)00632-9 ↗
49. Soniscope tests concrete structures
50. BS 1881: Part 203 · 1986
51. On the relationship between pore structure and charge passed from RCPT in mineral-free cement-based materials10.1016/j.matchemphys.2005.03.044 ↗
52. Durability of the hydrated limestone - silica fume Portland cement mortars under sulphate attack10.1016/S0008-8846(99)00049-6 ↗
53. Compressive strength and sulfate resistance of limestone and/or silica fume mortars10.1016/j.conbuildmat.2011.06.064 ↗
54. MTO-SP-SCC · 2013
55. Sirkin · 2006 · 438