journal article·2011-04

Performance-based assessment of concrete resistance to leaching

E. Rozière, A. Loukili

Cement and Concrete Composites· Volume 33· Issue 4
Publisher page

Abstract

Abstract Leaching of calcium and hydrates from concrete is likely to occur when concrete structures are immersed in pure or poorly mineralised water and acid environments. A performance-based test may be used to design concrete for such exposures, provided that it is representative, sensitive, and repeatable. In the experimental study a leaching test was performed on six vibrated concrete mixtures and five self-compacting concrete mixtures, varying aggregate type, water/binder ratio and mineral admixtures, such as fly ash, ground granulated blast-furnace slag and limestone filler. Two indicators have been used to assess damaged depth, taking limestone aggregates into account. Fly ash (20–30% of binder) and slag (60%) significantly improved behaviour of concrete, whereas leaching rate increased with an increase in limestone filler content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Physicochemical equilibria of cement-based materials in aggressive environments – experiment and modelling10.1016/j.cemconres.2004.04.033 ↗
2. Modelling the leaching kinetics of cement-based materials – influence of materials and environment10.1016/S0958-9465(02)00085-9 ↗
3. Modelling the loss of strength and porosity increase due to the leaching of cement pastes10.1016/S0958-9465(98)00046-8 ↗
4. Long-term performance of cement paste during combined calcium leaching-sulfate attack: kinetics and size effect10.1016/j.cemconres.2004.07.039 ↗
5. Proportioning and testing concrete for durability
6. Performance specifications for durable concrete
7. A performance based approach for durability of concrete exposed to carbonation10.1016/j.conbuildmat.2008.01.006 ↗
8. French Standard NF EN 206-1. Béton – Partie 1: Spécifications, performances, production et conformité, AFNOR; 2004 [in French].
9. Badoz C, Francisco P, Rougeau P. A performance test to estimate durability of concrete products exposed to chemical attacks. In: Proceedings of the second International congress of FIB, June 5–8; 2006.
10. Influence of paste volume on shrinkage cracking and fracture properties of self-compacting concrete10.1016/j.cemconcomp.2007.03.010 ↗
11. Durability of concrete exposed to leaching and external sulphate attacks10.1016/j.cemconres.2009.07.021 ↗
12. Compte-rendu des journées techniques AFPC-AFREM. Durabilité des bétons, Méthodes recommandées pour la mesure des grandeurs associées à la durabilité (in French). Toulouse, December 11–12; 1997.
13. Bourdette B. Durabilité du mortier: prise en compte des auréoles de transition dans la caractérisation et la modélisation des processus physiques et chimiques d’altération, Dissertation, INSA Toulouse; 1994 [in French].
14. Influence of carbonation and carbonation methods on leaching of metals from mortars10.1016/S0008-8846(03)00255-2 ↗
15. Baroghel-Bouny V. et al. Conception des bétons pour une durée de vie donnée des ouvrages (in French). Association Française de Génie Civil; 2004.
16. A separation of scales homogenization analysis for the modelling of calcium leaching in concrete10.1016/j.cma.2005.02.036 ↗
17. Estimates of self-compacting concrete ‘potential’ durability10.1016/j.conbuildmat.2006.06.034 ↗
18. European Standard EN 206-1, Concrete, specification, performance, production and conformity, CEN; 2004.