journal article·2025-10

Effect of CO2 partial pressure and temperature on degradation kinetics of cement paste in CO2-rich water

Shuqing Zhang, Jianhui Liu, Leping Liu, Zheng Chen, Caijun Shi

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · CO2 Sequestration and Geologic Interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. A novel treatment method and construction technology of the pipeline gushing water geohazards in karst region10.1016/j.tust.2021.103939 ↗
2. Hydrogeological analysis and remediation strategies for water inrush hazards in highway karst tunnels10.1016/j.tust.2024.105929 ↗
3. Identification of geological structure which induced heavy water and mud inrush in tunnel excavation: a case study on Lingjiao tunnel10.1016/j.tust.2017.06.014 ↗
4. Geological investigation and treatment measures against water inrush hazard in karst tunnels: a case study in Guiyang, southwest China, Tunn10.1016/j.tust.2022.104491 ↗
5. Geological engineering problems associated with tunnel construction in karst rock masses: the case of Gavarres tunnel (Spain)10.1016/j.enggeo.2013.02.010 ↗
6. Huang · 2011
7. Investigation of calcite precipitation in the drainage system of railway tunnels10.1016/j.tust.2018.10.021 ↗
8. Influence of liquid accelerators on shotcrete in Karst area tunnels
9. Attack of cement pastes exposed to organic acids in manure10.1016/j.cemconcomp.2005.06.003 ↗
10. A review on corrosion of cement-based materials in CO2-rich karst groundwater10.1016/j.cemconcomp.2023.105376 ↗
11. Corrosion resistance of cement-based materials with sugarcane bagasse ash-metakaolin-Portland cement binder under carbonic acid water environment
12. Thierry Chaussadent, Degradation modelling of concrete submitted to sulfuric acid attack10.1016/j.cemconres.2013.08.002 ↗
13. Modelling acid attack on concrete: Part I. The essential mechanisms10.1016/j.cemconres.2005.04.002 ↗
14. Performance of alkali-activated slag mortars exposed to acids10.1080/21650373.2012.747235 ↗
15. Summary on the genesis of CO2 in groundwater
16. A decay function model for the integrity loss of rock when subjected to recurrent cycles of freezing–thawing and heating-cooling10.1016/S1365-1609(03)00095-9 ↗
17. Geochemistry of wellbore integrity in CO2 sequestration: portland; cement-steel-brine-CO2 interactions10.2138/rmg.2013.77.15 ↗
18. Degradation of well cement in HPHT acidic environment: effects of CO2 concentration and pressure10.1016/j.cemconcomp.2016.09.006 ↗
19. A solution against well cement degradation under CO2 geological storage environment10.1016/j.ijggc.2008.07.005 ↗
20. Degradation of oilwell cement due to exposure to carbonated brine10.1016/j.ijggc.2009.11.001 ↗
21. CO2 stability of Portland cement based well cementing systems for use on carbon capture & storage (CCS) wells10.1016/j.cemconres.2012.12.001 ↗
22. A system for inspecting karst voids during construction of cast-in-place pile foundations10.1016/j.enggeo.2023.107124 ↗
23. Water inrush-induced failure during deep excavation for a metro station in karst regions in Shenzhen, China: cause diagnosis and post-accident restoration10.1016/j.engfailanal.2024.108346 ↗
24. Construction analysis of Guiyang metro passing across Guiyang railway station in karst zone10.1016/j.tust.2022.104541 ↗
25. Mechanical characterization of subway tunnel construction in urban shallow distributed karst stratums10.1016/j.trgeo.2023.101139 ↗
26. Simultaneous construction of subways and utility tunnels: a case project in Shenzhen, China10.1016/j.tust.2025.106421 ↗
27. The impact of extreme rainfall and drainage system failure on rock tunnels: a case study of deep-buried karst tunnel10.1016/j.engfailanal.2025.109345 ↗
28. Chloride ion transport performance of lining concrete under coupling the action of flowing groundwater and loading10.1016/j.cemconcomp.2021.104166 ↗
29. Failure mechanism analysis and treatment of tunnels built in karst fissure strata: a case study
30. Early mechanical properties and microstructural evolution of slag/metakaolin-based geopolymers exposed to karst water10.1016/j.cemconcomp.2019.03.009 ↗
31. Effect of CO2 on leaching from a cement-stabilized MSWI fly ash10.1016/j.cemconres.2003.11.022 ↗
32. Study on the deterioration mechanism of cement-based materials in acid water containing aggressive carbon dioxide10.1016/j.conbuildmat.2020.118233 ↗
33. Effect of carbonic acid water on the degradation of Portland cement paste: corrosion process and kinetics10.1016/j.conbuildmat.2015.05.046 ↗
34. A new method for improving the resistance of cement-based materials to carbonic acid water corrosion: carbonation curing and further water curing10.1016/j.conbuildmat.2024.135733 ↗
35. Carbonation of hardened cement pastes: influence of temperature10.1016/j.cemconres.2018.09.019 ↗
36. Acidic attack of cement based materials under the common action of high, ambient temperature and pressure10.1016/j.conbuildmat.2012.04.025 ↗
37. Formation characteristics of carbonate thermal water controlled by fault in southeastern Chongqing
38. Hydrogeochemical characteristics of the geothermal field in Wenquan basin, northern Tibet
39. Comparation of concrete carbonization experiment methods in corrosive CO2 groundwater environment
40. Heterogeneous porosity distribution in Portland cement exposed to CO2-rich fluids10.1016/j.cemconres.2008.03.022 ↗
41. Physical and chemical alterations in engineered cementitious composite under geologic CO2 storage conditions10.1016/j.ijggc.2019.01.025 ↗
42. Degradation behavior of concrete under corrosive coal mine environment10.1016/j.ijmst.2018.12.001 ↗
43. Concrete durability affected by aggressive carbon dioxide in groundwater
44. Preliminary experimental study on the deterioration of cementitious materials by an acceleration method10.1016/0029-5493(92)90290-C ↗
45. Leaching tests on different mortars using accelerated electrochemical method10.1016/S0008-8846(00)00377-X ↗
46. Influences of temperature and Pco2 on the solubility of calcite and dolomite
47. Controlling factors of riverine CO2 partial pressure and CO2 outgassing in a large karst river under base flow condition10.1016/j.jhydrol.2020.125638 ↗
48. Geographic and transport controls of temperature response in karst springs10.1016/j.jhydrol.2023.129850 ↗
49. An estimate of the time to degrade the cement sheath in a well exposed to carbonated brine10.1016/j.egypro.2009.02.101 ↗
50. Degradation process of alkali-activated slag/fly ash and Portland cement-based pastes exposed to phosphoric acid
51. Acid resistance of inorganic polymer binders. 1. Corrosion rate10.1617/s11527-011-9744-7 ↗
52. Modelling acid attack on concrete: Part II. A computer model10.1016/j.cemconres.2015.10.012 ↗
53. Corrosion of hardened cement paste by acetic and nitric acids part I: calculation of corrosion depth10.1016/0008-8846(94)90144-9 ↗
54. Dynamics of gas-driven eruptions: experimental simulations using CO2-H2O-polymer system10.1029/96JB03181 ↗
55. Accelerated degradation method for cement under CO2-rich environment: the LIFTCO2 procedure (leaching induced by forced transport in CO2 fluids)10.1016/j.cemconres.2010.03.019 ↗
56. Chemical reactions of portland cement with Aqueous CO2 and their impacts on cement's mechanical properties under geologic CO2 sequestration conditions10.1021/es5063488 ↗
57. The long-term corrosion behavior of abandoned wells under CO2 geological storage conditions: (1) experimental results for cement alteration10.1016/j.egypro.2013.06.501 ↗
58. Real time 3D observations of portland cement carbonation at CO2 storage conditions10.1021/acs.est.0c00578 ↗
59. Meso-damage analysis of concrete based on X-ray CT in-situ compression and using deep learning method
60. Quantifying the influence of microstructure on the corrosion of Mg-Li alloys by using X-ray CT10.1016/j.corsci.2024.111848 ↗
61. Monitoring the evolution of accelerated carbonation of hardened cement pastes by X-ray computed tomography10.1061/(ASCE)MT.1943-5533.0000610 ↗
62. Effect of temperature on CO2 curing, compressive strength and microstructure of cement paste10.1016/j.cemconres.2022.106827 ↗
63. Modelling long-term and short-term evolution of karst in vicinity of tunnels - ScienceDirect10.1016/j.jhydrol.2019.124282 ↗
64. Descriptive and predictive models for Henry's law constant of CO2 in ionic liquids: a QSPR study10.1016/j.cherd.2016.12.020 ↗
65. Precipitation kinetics of calcite in the system CaCO3-H2O-CO2: the conversion to CO2 by the slow process H+ + HCO3- → CO2 + H2O as a rate limiting step10.1016/S0016-7037(97)00201-9 ↗
66. The kinetics of the reaction CO2 + H2O → H+ + HCO3− as one of the rate limiting steps for the dissolution of calcite in the system H2O-CO2-CaCO310.1016/0016-7037(96)00181-0 ↗
67. Tung-Chai Ling, Elucidating the dominant and interaction effects of temperature, CO2 pressure and carbonation time in carbonating steel slag blocks10.1016/j.conbuildmat.2021.124158 ↗
68. Plummer · 1978 · 278
69. Experimental analysis on the carbonation rate of Portland cement at room temperature and CO2 partial pressure from 1 to 51bar10.1016/j.cemconcomp.2021.104271 ↗
70. Modelling karst aquifer evolution in fractured, porous rocks10.1016/j.jhydrol.2016.10.049 ↗
71. Quantitative characterization of recycled cementitious materials before and after carbonation curing: carbonation kinetics, phase assemblage, and microstructure10.1016/j.conbuildmat.2024.135596 ↗
72. Prediction of the corrosion depth of oil well cement corroded by carbon dioxide using GA-BP neural network10.1016/j.conbuildmat.2023.132127 ↗
73. Carbonation of cement paste under different pressures10.1016/j.conbuildmat.2023.130511 ↗
74. Determination of the apparent activation energy of concrete carbonation10.1007/s11595-013-0798-y ↗
75. Degradation of well cements exposed to carbonated brine10.1016/j.ijggc.2009.11.001 ↗
76. Roman Lackner. Differential-scheme based dissolution diffusion model for calcium leaching in cement-based materials accounting for mix design and binder composition10.1016/j.cemconres.2014.01.011 ↗