Petrographic analysis of in-service cementitious mortar subject to freeze-thaw cycles and deicers
Source abstract
Abstract
Abstract Chloride-based deicers, especially CaCl2 and MgCl2, can damage cementitious materials due to the formation of mineral phases such as calcium oxychloride and brucite. However, there are only limited direct observations of calcium oxychloride formed in cementitious materials in the field. This paper uses petrographic methods to evaluate damage of an in-service cementitious mortar substrate subject to freeze-thaw cycles and deicers for six years. The amount of calcium hydroxide in the mortar was quantified using thermogravimetric analysis. Changes in hydration products and microstructure were characterized by optical microscopy. Scanning electron microscopy coupled with energy dispersive X-ray spectroscopy was used to examine the morphology and elemental composition of secondary deposits related to the deicer damage. The mortar with less than 3% air exhibits horizontal cracks and microcracks cutting around aggregate particles. The cracks and microcracks are partially filled with calcium oxychloride due to the application of CaCl2. A densified crust of brucite and calcite, likely associated with the usage of MgCl2, covers the top surface of the damaged mortar. The deicer exposure results in leaching of calcium hydroxide mainly due to the formation of calcium oxychloride. Calcium leaching increases the apparent paste porosity in the damaged mortar, which likely weakens the physicomechanical properties of the mortar and accelerates the ingress of external deicer solutions. Moreover, the deicer application results in air-void-filling by calcium oxychloride and secondary ettringite, which may reduce the space available to release the internal stresses associated with ice formation and thus compromises the freeze-thaw durability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Smart Materials for Construction · Concrete and Cement Materials Research · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Yehia · 1998 · 51
2. Fischel · 2001 · 9
3. Relative effects of sodium chloride and magnesium chloride on reinforced concrete: state of the art10.3141/1866-08 ↗
4. Environmental Impact of Chemical Deicers – A Review10.1007/s11270-005-8265-9 ↗
5. Chloride penetration in nonsaturated concrete10.1061/(ASCE)0899-1561(2003)15:2(183) ↗
6. A comprehensive probabilistic model of chloride ingress in unsaturated concrete10.1016/j.engstruct.2010.11.008 ↗
7. Role of calcium on chloride binding in hydrated Portland cement–metakaolin–limestone blends10.1016/j.cemconres.2017.02.003 ↗
8. Ingress of NaCl in concrete with alkali reactive aggregate: effect on silicon solubility10.1617/s11527-015-0788-y ↗
9. Alkali-aggregate reaction under the influence of deicing salts in the Hokuriku district, Japan10.1016/j.matchar.2004.07.003 ↗
10. Damage in cement pastes exposed to MgCl2 solutions10.1617/s11527-018-1191-2 ↗
11. Flexural strength reduction of cement pastes exposed to CaCl2 solutions10.1016/j.cemconcomp.2017.11.021 ↗
12. Mechanism of the CaCl2 attack on Portland cement concrete10.1016/0008-8846(78)90026-1 ↗
13. Measuring volume change due to calcium oxychloride phase transformation in a Ca(OH)2-CaCl2-H2O system10.1520/ACEM20160065 ↗
14. Durability of high performance concrete in magnesium brine10.1016/0008-8846(96)00034-8 ↗
15. Effect of magnesium on calcium silicate hydrate (C-S-H)10.1016/j.cemconres.2017.03.012 ↗
16. Durability of concrete structures exposed to CaCl2 based deicing salts
17. The influence of calcium chloride deicing salt on phase changes and damage development in cementitious materials10.1016/j.cemconcomp.2015.09.006 ↗
18. Resistance of concrete to different exposures with chloride-based salts10.1016/j.cemconres.2017.09.001 ↗
19. Calcium oxychloride: a critical review of the literature surrounding the formation, deterioration, testing procedures, and recommended mitigation techniques10.1016/j.cemconcomp.2020.103663 ↗
20. Impact of chloride-rich environments on cement paste mineralogy10.1016/j.cemconres.2014.10.017 ↗
21. Phase diagram and volume change of the Ca(OH)2-CaCl2-H2O system for varying Ca(OH)2/CaCl2 molar ratios10.1061/(ASCE)MT.1943-5533.0002145 ↗
22. Chloride binding of cement pastes with fly ash exposed to CaCl2 solutions at 5 and 23 °C10.1016/j.cemconcomp.2018.12.011 ↗
23. Research on 3CaO·CaCl2·15H2O identified in concretes damaged by CaCl2 attack
24. 2019 · 6
25. Whiting · 2016 · 60
26. Accelerated expansion test sample report: DRP
27. Microstructural evaluation of durability of different cementitious mixtures in microbial induced corrosion environments
28. Petrographically quantifying the damage to field and lab-cast mortars subject to freeze-thaw cycles and deicer application10.1186/s43065-021-00024-3 ↗
29. 2020
30. 2020
31. Effects of sample preparation and interpretation of thermogravimetric curves on calcium hydroxide in hydrated pastes and mortars, Transportation Research Record10.3141/2290-02 ↗
32. Walker · 2006 · 351
33. 2016 · 84
34. Determining the freeze-thaw performance of mortar samples using length change measurements during freezing10.1016/j.cemconcomp.2020.103869 ↗
35. Todak · 2015
36. Quantifying the freeze-thaw performance of air-entrained concrete using the time to reach critical saturation modelling approach10.1016/j.cemconcomp.2019.103479 ↗
37. Service-life of concrete in freeze-thaw environments: critical degree of saturation and calcium oxychloride formation10.1016/j.cemconres.2019.04.014 ↗
38. Quantifying fluid absorption in air-entrained concrete using neutron radiography
39. Electrical resistivity and formation factor of air-entrained concrete
40. Multi-scale simulation of freeze-thaw damage to RC column and its restoring force characteristics10.1016/j.engstruct.2017.11.066 ↗
41. Observations of chloride ingress and calcium oxychloride formation in laboratory concrete and mortar at 5° C10.1016/j.cemconres.2013.01.001 ↗
42. The development and stability of surface layers on concrete exposed to sea-water10.1016/0008-8846(86)90046-3 ↗
43. Damage development in cementitious materials exposed to magnesium chloride deicing salt10.1016/j.conbuildmat.2015.06.004 ↗
44. Thermogravimetric analysis
45. Microscopy techniques for determining water–cement (w/c) ratio in hardened concrete: a round-robin assessment10.1617/s11527-020-1458-2 ↗
46. Hydration of binary portland cement blends containing silica fume: a decoupling method to estimate degrees of hydration and pozzolanic reaction
47. Weiss · 2018 · 59
48. Impact of chloride on the mineralogy of hydrated Portland cement systems10.1016/j.cemconres.2010.03.002 ↗
49. Friedel's salt, Ca2Al(OH)6(Cl,OH)·2H2O: its solid solutions and their role in chloride binding10.1016/S0008-8846(98)00162-8 ↗
50. Wetting and drying of concrete using aqueous solutions containing deicing salts10.1016/j.cemconcomp.2011.02.009 ↗
51. Influence of the storage conditions on the dimensional changes of heat-cured mortars10.1016/S0008-8846(01)00480-X ↗
52. Stutzman · 1999 · 82