journal article·2023-11Open access

Regulate the microstructure, tensile properties and fatigue crack growth behavior of an Al–Zn–Mg–Cu alloys fabricated by laser powder bed fusion via post-heat treatment

Dehua Li, Shengci Li, Zhiqian Zhang, Jiqiang Chen, Yu Zhang, Jiamin Yang, Weirong Li, Yanfang Li, Olanrewaju A. Ojo

Abstract

An Al–Zn–Mg–Cu–Si–Zr–Er alloy was fabricated by laser powder bed fusion technology. A unique cellular structure consisting of α-Al, Mg2Si, and Al2CuMg phases was observed in both as-printed (AP) and direct aging (DA) alloys. Direct aging treatment at 150 °C × 4 h can improve the yield strength and hardness of the alloy, and precipitation strengthening and fine grain strengthening are dominant mechanisms. The strength of the regression re-aging (RRA) heat treated alloy decreased, while the elongation was obviously improved, and the grain boundary was continuous without precipitates free zones. DA could not significantly hinder the fatigue crack growth rate of the as-printed alloy, but the improvement of plasticity, elimination of residual stress, and the effect of precipitates in RRA alloy extend the life of the fatigue crack growth stage, thereby improving the overall fatigue life of the alloy from 1.17 × 105 cycles to 3.93 × 106 cycles.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Additive manufacturing of functionally graded metallic materials using laser metal deposition[J]
2. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting[J]10.1016/j.jmst.2019.08.049 ↗
3. Microstructure evolution and mechanical properties at high temperature of selective laser melted AlSi10Mg[J]10.1016/j.jmst.2020.04.066 ↗
4. An additively manufactured Al–14.1Mg–0.47Si–0.31Sc–0.17Zr alloy with high specific strength, good thermal stabilitv and excellent corrosion resistance[J]10.1016/j.jmst.2020.06.036 ↗
5. Ultra strong and ductile eutectic high entropy alloy fabricated by selective laser melting[J]10.1016/j.jmst.2021.08.015 ↗
6. Selective laser melting of 7075 aluminum alloy inoculated by Al–Ti–B: grain refinement and superior mechanical properties[J]10.1016/j.vacuum.2022.111030 ↗
7. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments[J]10.1016/j.msea.2017.08.029 ↗
8. Effect of direct aging treatment on microstructure, mechanical and corrosion properties of a Si–Zr–Er modified Al–Zn–Mg–Cu alloy prepared by selective laser melting technology[J]
9. Microstructure, mechanical properties, aging behavior, and corrosion resistance of a laser powder bed fusion fabricated Al–Zn–Mg–Cu–Ta alloy [J]10.1016/j.msea.2021.142364 ↗
10. Effects of retrogression and re-aging treatment on precipitation behavior, mechanical and corrosion properties of a Zr + Er modified Al–Zn–Mg–Cu alloy10.1016/j.matchar.2021.111617 ↗
11. Effects of Sc addition and retrogression and re-aging on microstructure and mechanical properties of Al–8Zn–2Mg–2Cu–0.15Zr Alloy[J]10.1007/s11665-022-06620-y ↗
12. Effect of T6 heat treatment on the surface tribological and corrosion properties of AlSi10Mg samples produced by selective laser melting[J]10.1016/j.matchar.2020.110769 ↗
13. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): microstructure, high cycle fatigue, and fracture behavior[J]10.1016/j.matdes.2011.07.067 ↗
14. Effect of heat treatment on the microstructure and mechanical properties of an Al–5Mg2Si–2Mg alloy processed by laser powder bed fusion[J]10.1016/j.jallcom.2022.165944 ↗
15. Effect of heat treatment on microstructure, hardness and corrosion resistance of 7075 Al alloys fabricated by SLM[J]10.1016/j.jmapro.2020.10.071 ↗
16. Selective laser melting additive manufacturing of 7xxx series Al–Zn–Mg–Cu alloy: cracking elimination by co–incorporation of Si and TiB2[J]
17. Effect of heat treatment on the microstructure and mechanical properties of Er–containing Al–7Si–0.6Mg alloy by laser powder bed fusion[J]10.1016/j.jmrt.2022.04.023 ↗
18. Selective laser melting of Al–12Si alloy: enhanced densification via powder drying[J]
19. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg[J]10.1016/j.jmatprotec.2015.02.013 ↗
20. Role of melt pool boundary condition in determining the mechanical properties of selective laser melting AlSi10Mg alloy[J]10.1016/j.msea.2018.10.083 ↗
21. Effects of heat treatment on microstructure and mechanical properties of SLMed Sc–modified AlSi10Mg alloy[J]10.1016/j.pnsc.2021.08.003 ↗
22. Effect of heat treatment on SLM–fabricated TiN/AlSi10Mg composites: microstructural evolution and mechanical properties [J]10.1016/j.jallcom.2020.156722 ↗
23. Effect of heat treatment on properties of Al–Mg–Sc–Zr alloy printed by selective laser melting[J]10.1016/j.apsusc.2021.151471 ↗
24. Heat treatment of Al–Cu–Li–Sc–Zr alloy produced by laser powder bed fusion[J]10.1016/j.matchar.2022.112505 ↗
25. Li · 2012
26. The Portevin–Le Chatelier (PLC) effect in an Al–Cu aluminum alloy fabricated by selective laser melting[J]10.1016/j.matchar.2021.111198 ↗
27. Selective laser melting of advanced Al–Al2O3 nanocomposites: simulation, microstructure and mechanical properties[J]10.1016/j.msea.2017.05.061 ↗
28. Microstructure, mechanical properties and strengthening mechanisms of AlCu5MnCdVA aluminum alloy fabricated by selective laser melting[J]10.1016/j.msea.2019.04.114 ↗
29. Selective laser melting of Al–7Si–0.5Mg–0.5Cu: effect of heat treatment on microstructure evolution, mechanical properties and wear resistance[J]10.1007/s40195-021-01279-1 ↗
30. Influence of post-heat treatment on the microstructure and mechanical properties of Al–Cu–Mg–Zr alloy manufactured by selective laser melting[J]10.1016/j.jmst.2021.09.036 ↗
31. Microstructure, mechanical properties and fatigue crack growth behavior of an Al–Zn–Mg–Cu–Si–Zr–Er alloy fabricated by laser powder bed fusion[J]10.1016/j.ijfatigue.2023.107636 ↗
32. Al2O3 particle erosion induced phase transformation: structure, mechanical property, and impact toughness of an SLM Al–10Si–Mg alloy[J]10.3390/nano11082131 ↗
33. Improving the applicability of wear-resistant Al–10Si–0.5 Mg alloy obtained through selective laser melting with T6 treatment in high-temperature, and high-wear environments[J]10.1016/j.jmrt.2020.06.078 ↗
34. Research progress on high cycle fatigue performance of selective laser melting formed Al-Si Alloy[J]
35. On mechanical properties of SLM Al–Si alloy: role of heat treatment-induced evolution of silicon morphology[J]10.1016/j.msea.2022.144157 ↗
36. Fatigue and dynamic aging behavior of a high strength Al–5024 alloy fabricated by laser powder bed fusion additive manufacturing[J]10.1016/j.actamat.2021.117312 ↗