Advancement of eco-friendly slag-based high-strength geopolymer concrete
Source abstract
Abstract
This study investigates the production and testing of slag-based high-strength geopolymer concrete (HSGC) by incorporating various waste materials as partial substitutes for slag. The focus is on replacing slag with alternative materials such as fly ash (FA), metakaolin (MK), ceramic waste (CW), glass waste (GW), rice husk ash (RHA), and charcoal ash (CA). These alternatives are not only cheaper but also have a lower environmental impact, offering additional benefits such as reduced CO 2 emissions, representing a significant step towards sustainability. Key variables, such as geopolymer binder proportions (30% and 50%), curing methods (water + steam, heat, and water), and mixing procedures, were examined. Scanning electron microscope (SEM) and energy dispersive X-ray (EDX) spectroscopy analyses were performed on selected HSGC mixes. In addition, cost and energy efficiency analyses were performed on all HSGC blends. Among the mixes tested, CA30, FA30, and FA50 showed increases in both workability (by 30%, 46%, and 79%, respectively) and compressive strength (by 39%, 28%, and 15.4%, respectively) compared to the control mix. The steam + water curing method resulted in the highest compressive strength for all mixtures, except CA30, CA50, and the control mixtures. Furthermore, CA30 and FA30 blends achieved the lowest water permeability (1.9 cm and 1.5 cm, respectively) and sorptivity (3.1 mm and 3.8 mm, respectively), compared to the control mix. Shrinkage of CA50, CW30, and GW50 mixes decreased by an average of 57%, 53%, and 79%, respectively, at all ages. Microstructure analyses revealed a dense and homogeneous matrix for these mixtures, confirming their compressive strength results and identifying them as ideal mixtures. In addition, CA50, FA50, and CW30 mixtures demonstrated higher environmental efficiency, with lower carbon emissions, reduced energy consumption, and improved cost efficiency compared to the control mix. Their values were 139, 144, and 131 MPa/t-CO 2 /m³, 0.573, 0.575, and 0.586 t–CO 2 –e/m³, and 2.98, 2.99, and 3.07 GJ/m³, respectively, with cost efficiencies of 0.13, 0.159, and 0.103 MPa-$-m³.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (78)
Show source-provided references
1. Bond strength of eco-friendly class C fly ash-based thermally cured alkali-activated concrete to portland cement concrete10.1016/j.jclepro.2019.06.268 ↗
2. Development of fly ash- and slag-based geopolymer concrete with calcium carbonate or microsilica10.1061/(ASCE)MT.1943-5533.0002527 ↗
3. Geopolymer concrete with lightweight fine aggregate: material performance and structural application
4. Assessment of the durability of grout submitted to accelerated carbonation test10.1016/j.conbuildmat.2017.10.111 ↗
5. Mechanical properties of fly-ash-based geopolymer concrete
6. Durability, microstructure, and optimization of high-strength geopolymer concrete incorporating construction and demolition waste
7. Investigation oncompressive strength development of geopolymer concrete using manufactured sand10.1016/j.matpr.2019.06.284 ↗
8. Alkali activation of Australian slag cements10.1016/S0008-8846(98)00170-7 ↗
9. Synthesis of high strength ambient cured geopolymer composite by using low calcium fly ash10.1016/j.conbuildmat.2016.08.097 ↗
10. Sintered and unsintered pressed fly ash geopolymer: a comprehensive study on structural transformation in nitric and sulfuric acid
11. Influence of sodium silicate powder silica modulus for mechanical and chemical properties of dry-mix alkali-activated slag mortar10.1016/j.conbuildmat.2019.117354 ↗
12. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
13. Strength assessment of geopolymer concrete using M-sand
14. Improving strength of calcinated coal gangue geopolymer mortars via increasing calcium content10.1016/j.conbuildmat.2018.02.005 ↗
15. Effect of particle size and thermal activation on the coal gangue based geopolymer
16. Mechanical properties and chloride permeability of green concrete mixed with fly ash and coal gangue10.1016/j.conbuildmat.2019.117166 ↗
17. Use of geopolymer concrete for a cleaner and sustainable environment – a review of mechanical properties and microstructure10.1016/j.jclepro.2019.03.051 ↗
18. Effect of magnetized water-based alkaline activator on geopolymer concrete mechanical performance and durability10.3390/su152316315 ↗
19. Material characterization and thermal performance of polyethylene fiber-reinforced lightweight engineered geopolymer composites subjected to sulfate attacks10.1016/j.conbuildmat.2024.139156 ↗
20. Magnesium sulphate resistance of fly ash one-part geopolymers: influence of solid alkali activators on physical, mechanical and chemical performance10.1016/j.conbuildmat.2024.137971 ↗
21. The mechanical performance evaluation of fly-ash derived geopolymer mortar for concrete patch repair10.31893/multiscience.2025161 ↗
22. Performance of blended metakaolin/blastfurnace slag alkali-activated mortars10.1016/j.cemconcomp.2016.04.008 ↗
23. Physical evolution of Na-geopolymer derived from metakaolin up to 1000 °c10.1007/s10853-006-0535-4 ↗
24. The heavy metal adsorption characteristics on metakaolin-based geopolymer10.1016/j.clay.2011.11.027 ↗
25. Development and optimization of an eco-friendly geopolymer brick production process for sustainable masonry construction
26. Effects of metakaolin and sodium silicate solution on workability and compressive strength of sustainable Geopolymer mortar10.1016/j.matpr.2021.10.399 ↗
27. Factors affecting the performance of metakaolin geopolymers exposed to elevated temperatures10.1007/s10853-007-2205-6 ↗
28. A comparative study of high- and low-Al2O3 fly ash based-geopolymers: the role of mix proportion factors and curing temperature10.1016/j.matdes.2016.01.084 ↗
29. Effect of thermal treatment on reactivity and mechanical properties of alkali activated shale–slag binder10.1016/j.conbuildmat.2015.02.024 ↗
30. Comparison of feldspar and meta-halloysite geopolymers by alkaline and acidic activation10.1016/j.conbuildmat.2024.135953 ↗
31. Assessment of the suitability of ceramic waste in geopolymer composites: an appraisal10.3390/ma14123279 ↗
32. Potential use of ceramic waste as precursor in the geopolymerization reaction for the production of ceramic roof tiles
33. Alkaline activation of low-reactivity ceramics: peculiarities induced by the precursors' dual character
34. Influence of the activator concentration and calcium hydroxide addition on the properties of alkali-activated porcelain stoneware10.1016/j.conbuildmat.2014.04.023 ↗
35. Influences of parameters on slump flow and compressive strength properties of aluminosilicate based flowable geopolymer concrete using taguchi method10.1007/s12633-019-00166-w ↗
36. Effect of synthesis parameters on the quality of construction and demolition wastes (CDW) geopolymers10.1016/j.apt.2014.11.012 ↗
37. Valorization of construction and demolition (C&D) and industrial wastes through alkali activation10.1016/j.conbuildmat.2016.06.051 ↗
38. Evaluation of structural performances of metakaolin based geopolymer concrete10.1016/j.jmrt.2022.08.020 ↗
39. Mechanical and durability properties of fly ash and slag based geopolymer concrete
40. Mechanical properties of fly ash and silica fume based geopolymer concrete made with magnetized water activator10.1016/j.conbuildmat.2023.134376 ↗
41. Energy consumption and CO2 emissions of the European glass industry10.1016/j.enpol.2010.09.022 ↗
42. Effective function of activated bagasse ash for high early strength geopolymer
43. Properties of inorganic polymer (geopolymer) mortars made of glass cullet10.1007/s10853-011-6107-2 ↗
44. Strength, microstructure, efflorescence behavior and environmental impacts of waste glass geopolymers cured at ambient temperature10.1016/j.jclepro.2019.119610 ↗
45. Green concrete partially comprised of rice husk ash as a supplementary cementitious material – a comprehensive review10.1016/j.rser.2017.10.081 ↗
46. A review on utilization of rice husk ash in concrete
47. Comparison of two processes for treating rice husk ash for use in high performance concrete10.1016/j.cemconres.2009.05.006 ↗
48. A structural investigation relating to the pozzolanic activity of rice husk ashes10.1016/j.cemconres.2007.10.004 ↗
49. Title No . 116-M16 false positives in ASTM C618 speci cations for natural pozzolans compressive strength testing
50. Using of recycled clay brick/fine soil to produce sodium hydroxide alkali activated mortars10.1177/13694332211015742 ↗
51. 1998
52. The effect of nano metakaolin material on some properties of concrete10.24237/djes.2013.06105 ↗
53. Astm · 2017
54. ASTM - C78–16 Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading).
55. Astm · 2009
56. Guidebook on non-destructive testing of concrete structures
57. As · 2014
58. Activated alkali cement based on blast furnace slag: effect of curing type and concentration of Na2010.1016/j.jmrt.2023.02.088 ↗
59. Compressive strength performance of alkali activated concretes under different curing conditions
60. Concrete retrofitting using metakaolin geopolymer mortars and CFRP10.1016/j.conbuildmat.2011.03.006 ↗
61. Strength and durability of geopolymer concrete with high volume rubber replacement
62. Development of rubberized geopolymer concrete: strength and durability studies10.1016/j.conbuildmat.2019.01.185 ↗
63. Investigation of engineering properties of normal and high strength fly ash based geopolymer and alkali-activated slag concrete compared to ordinary Portland cement concrete10.1016/j.conbuildmat.2018.11.083 ↗
64. Fracture behaviour of heat cured fly ash based geopolymer concrete10.1016/j.matdes.2012.08.005 ↗
65. Engineering and durability properties of eco-friendly mortar using cement-free SRF binder10.1016/j.conbuildmat.2017.11.040 ↗
66. “A study of compressive strength and durability of Mae Moh fly ash geopolymer [Ph. D. thesis],”
67. Water sorptivity of mortars and concretes: a review10.1680/macr.1989.41.147.51 ↗
68. Sustainable geopolymer concrete using ground granulated blast furnace slag and rice husk ash: strength and permeability properties10.1016/j.jclepro.2018.08.313 ↗
69. Influence of slag as additive on compressive strength of fly ash-based geopolymer10.1061/(ASCE)0899-1561(2007)19:6(470) ↗
70. Influence of recycled glass content and curing conditions on the properties of self-compacting concrete after exposure to elevated temperatures10.1016/j.cemconcomp.2011.08.010 ↗
71. Kinetics of geopolymerization: role of Al2O3 and SiO210.1016/j.cemconres.2007.01.003 ↗
72. Mechanical and fresh properties of sustainable oil palm shell lightweight concrete incorporating palm oil fuel ash10.1016/j.jclepro.2015.12.051 ↗
73. Barriers and enablers for green concrete adoption: a scientometric aided literature review approach
74. Energy and CO2 emission assessments of alkali-activated concrete and Ordinary Portland Cement concrete: a comparative analysis of different grades of concrete
75. University of Bath · 2011 · 136
76. Life cycle inventories for the production of detergent ingredients10.1007/BF02979499 ↗
77. Decarbonising the cement sector: a bottom-up model for optimising carbon capture application in the UK10.1016/j.jclepro.2016.08.129 ↗
78. Carbon dioxide equivalent (CO2-e) emissions: a comparison between geopolymer and OPC cement concrete10.1016/j.conbuildmat.2013.01.023 ↗