Corrosion and corrosion-fatigue behavior of cp-Ti and Ti–6Al–4V laser-marked biomaterials
Source abstract
Abstract
The aim of this work was to determine the influence of laser surface modification treatments on mechanical and electrochemical behavior in Ti and Ti-6Al-4V implants. For each metal, different samples were laser modified simulating the markings according to the international requirements. (It is necessary in each metallic biomaterial to mark the serial, batch and company numbers.) Microstructural changes produced by this treatment were observed: (a) the melting zone with small grain sizes and martensitic structures in above-mentioned metals and (b) the heat-affected zone (HAZ) with alpha phase in cp-Titanium with bigger grain sizes and Widmanstatten structure in Ti-6Al-4V. Positive tensile residual stress was determined by means X-ray analysis in the zones marked by laser. Furthermore, corrosion behavior was studied in a simulated body fluid at 37°C. Pitting was observed in different zones near the HAZ and the results showed a decrease of the corrosion resistance in the laser treated samples. Residual stresses and the martensitic microstructures favoured the decrease of the corrosion-fatigue life around 20% of both metals under physiological conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Margolin H, Farar PA, Greenfield M. In: Jaffe I, Promisel N, editors. The science technology and application of Titanium. New York: Pergamon Press; 1970. p. 795.10.1016/B978-0-08-006564-9.50086-5 ↗
2. Lautenschlager EP, Monaghan P. Titanium and titanium alloys as dental materials. Int Dent J. 1993;43:253–257.
3. Gil FJ, Rodríguez D, Planell JA, Cortada M, Giner Ll, Costa S. Galvanic corrosion behaviour of titanium implants coupled to dental alloys. J Mater Sci Mater Med. 2000;11:287–291.10.1023/A:1008905229522 ↗
4. Geis-Gerstorfer J. In vitro corrosion measurements of dental alloys. J Dent. 1994;22:247–250.10.1016/0300-5712(94)90124-4 ↗
5. Sjögen G, Andersson M, Bergman M. Laser welding of titanium in dentistry. Acta Odontol Scand. 1988;46:253–257.
6. Tambasco J, Anthony T, Sandven O. Laser welding in dental laboratory: an alternative to soldering. J Dent Technol. 1996;13:31–35.
7. Sevilla P, Martorell F, Libenson C, Planell JA, Gil FJ. Laser welding of NiTi orthodontic archwires for selective force application. J Mater Sci Mater Med. 2008;19:525–9.10.1007/s10856-007-0164-8 ↗
8. Singh R, Kurella A, Dahotre NB. Laser surface modification of Ti–6Al–4V: wear and corrosion characterization in simulated biofluid. J Biomater Appl. 2006;21(1):49–73.10.1177/0885328206055998 ↗
9. Zavanelli RA, Guilherme AS, Pessanha-Henriques GE, Nobilo M, Mesquita MF. Corrosion-fatigue of laser-repaired commercially pure titanium and Ti–6Al–4V alloy under different test environments. J Oral Rehabil. 2004;31(10):1029–34.10.1111/j.1365-2842.2004.01336.x ↗
10. Baboian R. Electrochemical techniques for predicting galvanic corrosion. In: Baboian R, France R, Roew J, Rynewicz JF, editors. Galvanic and pitting corrosion-field and laboratory studies. ASTM STP 576. Philadelphia: American Society for Testing and Materials; 2004. p. 6.
11. Mansfeld F, Meyers RL, Lauer G. Instrumentation for corrosion studies in low conductivity media. Technical Report, Rockwell International; 2003.
12. Canay S, Öktemer M. In vitro corrosion behaviour of 13 prosthodontic alloys. J Dent Res. 1992;23(4):279–282.
13. Lucas L, Lemons JE. Biodegradation of restorative metallic systems. Adv Dent Res. 1992;6:32–37.10.1177/08959374920060011301 ↗