journal article·2016-05

Low temperature degradation resistant nanostructured yttria-stabilized zirconia for dental applications

Ilenia G. Tredici, Marco Sebastiani, Federico Massimi, Edoardo Bemporad, Alessandro Resmini, Giuseppe Merlati, Umberto Anselmi-Tamburini

Ceramics International· Volume 42· Issue 7
Publisher page

Abstract

Abstract When used in prosthetic dentistry, zirconia encounters severe durability issues due to low temperature degradation: exposure to humidity results in a transition from tetragonal to monoclinic phase, associated to disruptive integrity loss. Recently it has been shown that size-induced stabilization helps maintaining zirconia in tetragonal form, when the grain size is reduced to the nano-range. Objective of this work is to demonstrate the applicability of High Pressure Field Assisted Sintering (HP-FAST) to the preparation of dense, nanostructured samples of tetragonal yttria stabilized zirconia, with yttria content between 0.5 and 3 mol% and showing resistance to low temperature degradation. The yttria stabilized zirconia nanopowders were prepared by a hydrothermal method. Sintering by HP-FAST was performed at 900 °C in 5 min, under a pressure of 620 MPa. Resistance to low temperature degradation was tested at 134 °C, under vapor pressure, for up to 40 h. Both pristine and aged samples were characterized by X-ray diffraction, high-resolution scanning electron microscopy and nanoindentation tests in continuous stiffness measurement mode. The sintered samples presented a grain size between 20 and 30 nm and low or null monoclinic content. Both parameters resulted unaffected by ageing. The best results in terms of phase composition and mechanical properties have been obtained with the material containing 1.5 mol% of yttria. These results induce to reconsider the use of yttria stabilized zirconia as material for dental prosthetic systems requiring long-term durability.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced materials and composites · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
2. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
3. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
4. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
5. Ceramic steel?10.1038/258703a0 ↗
6. Effect of stress induced phase transformation on the properties of polycristalline zirconia-containing tetragonal phase10.1007/BF00553200 ↗
7. Property degradation of tetragonal zirconia induced by low-temperature defect reaction with water molecules10.1021/cm040167h ↗
8. Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing10.1557/JMR.2003.0337 ↗
9. Energy crossovers in nanocrystalline zirconia10.1111/j.1551-2916.2004.00031.x ↗
10. Synthesis of bulk tetragonal zirconia without stabilizer: the role of precursor nanopowders10.1016/j.jeurceramsoc.2011.09.022 ↗
11. Field assisted sintering of nanometric ceramic materials
12. Densification and properties of bulk nanocrystalline functional ceramics with grain size below 50nm10.1016/j.jeurceramsoc.2012.12.004 ↗
13. Synthesis of fully dense nanostabilized undoped tetragonal zirconia10.1111/j.1551-2916.2010.03695.x ↗
14. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
15. US Food and Drug Administration, Steam re-sterilization causes deterioration of zirconia ceramic heads of total hip prostheses. U.S. Department of Health and Human Services, Washington, D.C. Available at 〈http://www.fda.gov/MedicalDevices/Safety/AlertsandNotices/PublicHealthNotifications/ucm062472.htm〉, 1997.
16. Poitout · 2013 · 654
17. ISO standard 13356:2008 implants for surgery. Ceramic materials based on yttria-stabilized tetragonal zirconia (Y-TZP).
18. A new testing protocol for zirconia dental implants10.1016/j.dental.2014.09.002 ↗
19. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
20. Spark plasma sintering and characterization of bulk nanostructured fully stabilized zirconia: Part I. densification studies10.1557/JMR.2004.0423 ↗
21. Fast low-temperature consolidation of bulk nanometric ceramic materials10.1016/j.scriptamat.2005.11.015 ↗
22. Microstructural development in MgO-partially stabilized zirconia (Mg-PSZ)10.1111/j.1151-2916.1979.tb09484.x ↗
23. ISO 14577-1,2,3 Metallic materials – Instrumented indentation test for hardness and materials parameters.
24. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
25. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
26. Mechanical properties of nanometer volumes of material: use of the elastic response of small area indentations
27. On the generality of the relationship among contact stiffness, contact area, and elastic modulus during indentation10.1557/JMR.1992.0613 ↗
28. Porosity-dependence of elastic moduli and hardness of 3Y-TZP ceramics10.1016/S0272-8842(98)00037-6 ↗
29. Low temperature degradation mechanism of tetragonal zirconia ceramics in water: role of oxygen vacancies10.1016/S0167-2738(98)00212-4 ↗
30. Development of a novel zirconia dental post resistant to hydrothermal degradation10.1088/1757-899X/31/1/012016 ↗
31. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
32. Hydrothermal degradation of ground 3Y-TZP10.1016/j.jeurceramsoc.2011.08.029 ↗
33. Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia10.1016/j.dental.2015.09.014 ↗
34. Effect of cation dopant radius on the hydrothermal stability of tetragonal zirconia: grain boundary segregation and oxygen vacancy annihilation10.1016/j.actamat.2015.12.051 ↗
35. Highly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation10.1016/j.actbio.2015.01.037 ↗
36. Nanocrystalline, ultra-degradation-resistant zirconia: its grain boundary nanostructure and nanochemistry10.1038/srep04758 ↗
37. Degradation resistance of 3Y-TZP ceramics sintered using spark plasma sintering