Abstract

Abstract Surface integrity and interface structure of coating materials play a key role in tribological and corrosion behaviors in harsh working environments in nuclear power plants. In this work, we focus on the investigations of tribological behaviors in air and seawater of CrN/TiN superlattice coatings deposited by the combined deep oscillation magnetron sputtering with pulsed dc magnetron sputtering, which were irradiated by high-intensity pulsed ion beam (HIPIB) with ion energy density of 1–3 J/cm2 and shot number of 1–5. At 1 J/cm2, the increased shot number leads to a broaden (111) peak of face-centered cubic crystal structure, indicating grain size refinement. At 3 J/cm2, the increased shot number results in the coarsening grain, and superlattice structure gradually disappeared at 2 shots, finally the coatings fell off from substrate at 5 shots. The highest hardness (H), H/E* (E*, effective Young’s modulus) and H3/E*2 of the coatings irradiated at 1 J/cm2 and 5 shots are achieved at 38.7 GPa, 0.1 and 0.387, respectively. The increased ion energy density and shot number result in the decrease in Rockwell C HF adhesion level from HF1 to HF6. At 1 Jcm−2 and 1 shot, tribological behavior of irradiated coatings in air was dominated by oxidative wear with coefficient of friction (COF) of 0.51 and specific wear rate of 4.2 × 10−7mm3N−1m−1. The irradiated coatings show excellent tribocorrosion properties in seawater with high open circuit potential of 0.32 V, low COF of 0.14 and specific tribocorrosion rate of 6.1 × 10−8mm3N−1m−1 without pitting corrosion under moderate HIPIB irradiation due to high surface integrity and stability of well-defined interfaces and dense microstructure. With an increase of energy density and shot number, wear mechanism in air changes to severe adhesive and oxidative wear, while tribocorrosion mechanism is gradually dominated by plough wear coupled with pitting corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Structure and corrosion resistance of plasma nitrided stainless steel10.1179/sur.1985.1.2.131 ↗
2. Phase changes of the AISI 430 ferritic stainless steels after high-temperature gas nitriding and tempering heat treatment10.1016/j.msea.2007.11.078 ↗
3. Plasma nitriding of stainless steels at low temperatures10.1016/S0257-8972(99)00084-5 ↗
4. Investigation of the thermal stability of laser nitrided iron and stainless steel by annealing treatments10.1023/A:1021287725293 ↗
5. Plasma-based low-energy ion implantation of austenitic stainless steel for improvement in wear and corrosion resistance10.1016/j.surfcoat.2004.08.139 ↗
6. Recent progress in large scale manu-facturing of multilayer superlattice hard coatings10.1016/S0257-8972(00)00959-2 ↗
7. Microstructure and tribological behavior of TiAlSiN coatings deposited by deep oscillation magnetron sputtering10.1111/jace.15769 ↗
8. Recent advances in modulated pulsed power magnetron sputtering for surface engineering10.1007/s11837-011-0092-4 ↗
9. Vacuum-arc chromium-based coatings for protection of zirconium alloys from the high-temperature oxidation in air10.1016/j.jnucmat.2015.06.016 ↗
10. High vacuum arc ion plating NiCrAlY coatings: microstructure and oxidation behavior10.1016/j.corsci.2015.02.032 ↗
11. Structure and mechanicalproperties of CrN/TiN multilayer coatings prepared by a combined HIPIMS/UBMS deposition technique10.1016/j.tsf.2008.06.080 ↗
12. Stress and texturein HIPIMS TiN thin films10.1016/j.tsf.2009.09.069 ↗
13. Tailoring the nanostructure of Ti–Si–N thin films by HiPIMS in deep oscillation magnetron sputtering (DOMS) mode10.1016/j.surfcoat.2014.12.065 ↗
14. Flash post-discharge emission in a reactive HiPIMS process10.1063/1.4962486 ↗
15. Structure and properties of CrSiN nanocomposite coatings deposited by hybrid modulated pulsed power and pulsed dc magnetron sputtering10.1016/j.surfcoat.2012.11.053 ↗
16. Wear and corrosion resistance of CrN/TiN superlattice coatings deposited by a combined deep oscillation magnetron sputtering andpulsed dc magnetron sputtering10.1016/j.apsusc.2015.05.110 ↗
17. Structure, adhesion and corrosion behavior of CrN/TiN superlattice coatings deposited by the combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.surfcoat.2015.10.009 ↗
18. Stability of Ti-Zr-N coatings under Xe-ion irradiation10.1016/j.surfcoat.2009.11.023 ↗
19. Irradiation resistance, microstructure and mechanical properties of nanostructured (TiZrHfVNbTa)N coatings10.1016/j.jallcom.2016.04.064 ↗
20. Triboelectrochemical techniques and interpretation methods in tribocorrosion: a comparative evaluation10.1016/j.triboint.2007.11.003 ↗
21. Tribo-corrosion of coatings: a review10.1088/0022-3727/40/18/S10 ↗
22. Enhanced tribocorrosion performance of Cr/GLC multilayered films for marine protective application10.1021/acsami.8b00628 ↗
23. Tribocorrosion behaviors of CrN coating in 3.5 wt% NaCl solution10.1016/j.tsf.2016.12.023 ↗
24. Tribocorrosion behaviors of PVD CrN coated stainless steel in seawater10.1016/j.wear.2016.05.016 ↗
25. Corrosion and tribocorrosion behaviour of cermet and cermet/nanoscale multilayer CrN/NbN coatings10.1016/j.surfcoat.2009.09.046 ↗
26. High intensity pulsed ion beam sources and their industrial applications10.1016/S0257-8972(99)00058-4 ↗
27. Surface modification of 316L stainless steel with high-intensity pulsed ion beams10.1016/j.surfcoat.2006.10.040 ↗
28. High intensity pulsed ion beams in material processing: equipment and applications10.1016/0168-583X(91)95650-3 ↗
29. Deflection of high-intensity pulsed ion beam in focusing magnetically insulated ion diode with a passive anode10.1063/1.4968837 ↗
30. Reactive-sputter-deposited TiN films on glass substrates10.1016/0040-6090(91)90225-M ↗
31. Mechanical and tribological properties of CrN/TiN multilayer coatings deposited by pulsed dc magnetron sputtering10.1016/j.surfcoat.2015.06.064 ↗
32. A novel shock processing by high-intensity pulsed ion beam10.1115/1.3139214 ↗
33. Surface morphology of Cr2O3 coatings on steel irradiated by high-intensity pulsed ion beam10.1016/j.nimb.2005.09.017 ↗
34. Influence of the carbon content on the corrosion and tribocorrosion performance of Ti-DLC coatings for biomedical alloys10.1016/j.triboint.2015.03.007 ↗
35. Strength enhancement in thin-layered Al-Cu laminates10.1063/1.324518 ↗
36. Evaluation of PVD nitride coatings, using impact, scratch and Rockwell-C adhesion tests10.1016/0040-6090(95)06934-8 ↗
37. Texture, residual stress and structural analysis of thin films using a combined X-ray analysis10.1016/j.tsf.2003.10.150 ↗
38. Model of superlattice yield stress and hardness enhancements10.1063/1.359467 ↗