journal article·2021-12

Synthesis, microstructures, and corrosion behaviors of multi-components rare-earth silicates

Wei Liao, Yongqiang Tan, Chaowen Zhu, Zhen Teng, Peng Jia, Haibin Zhang

Ceramics International· Volume 47· Issue 23
Publisher page

Abstract

Abstract Multi-components and equimolar rare earth monosilicates, (Y1/3Dy1/3Er1/3)2SiO5, (Y1/3Dy1/3Lu1/3)2SiO5, (Y1/4Dy1/4Ho1/4Er1/4)2SiO5 and (Yb1/4Dy1/4Ho1/4Er1/4)2SiO5, were prepared by solid-state reactions and the following hot-pressing. Dense microstructures with uniform elemental distributions were obtained for all samples. These investigated multi-components monosilicates exhibit low thermal conductivities and similar coefficients of thermal expansion with SiC. Moreover, they exhibit high corrosion resistances in 1400 °C water vapor, especially, four-components (Y1/4Dy1/4Ho1/4Er1/4)2SiO5 and (Yb1/4Dy1/4Ho1/4Er1/4)2SiO5 experienced almost invariable weights after small weight losses during the initial 0.5 h. All those results indicate that multi-components rare earth monosilicates are promising candidates of environmental barrier coatings for SiC/SiC composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Thermal properties of rare‐earth monosilicates for EBC on Si‐based ceramic composites10.1111/jace.13982 ↗
2. Thermal and environmental barrier coatings for SiC/SiC CMCs in aircraft engine applications10.1111/j.1744-7402.2004.tb00181.x ↗
3. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
4. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
5. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
6. Observations of accelerated silicon carbide recession by oxidation at high water-vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
7. Development and environmental durability of mullite and mullite/YSZ dual layer coatings for SiC and Si3N4 ceramics10.1016/S0257-8972(96)03074-5 ↗
8. Water vapor corrosion behaviors of plasma sprayed RE2SiO5 (RE = Gd, Y, Er) coatings10.1016/j.corsci.2020.108529 ↗
9. Thermochemical stability of Y2Si2O7 in high-temperature water vapor10.1111/jace.17114 ↗
10. Robust hydrophobicity and evaporation inertness of rare-earth monosilicates in hot steam at very high temperature10.1111/jace.16315 ↗
11. Rare earth silicate environmental barrier coatings: present status and prospective10.1016/j.ceramint.2017.01.153 ↗
12. Water vapour corrosion of rare earth monosilicates for environmental barrier coating application10.1016/j.ceramint.2017.02.123 ↗
13. Recession behavior of Lu2SiO5 under a high speed steam jet at high temperatures10.1016/j.ceramint.2010.11.029 ↗
14. Water vapor corrosion behavior of scandium silicates at 1400°C10.1111/j.1551-2916.2008.02864.x ↗
15. Recession behavior of Yb2Si2O7 phase under high speed steam jet at high temperatures10.1016/j.corsci.2007.06.014 ↗
16. Response of ytterbium disilicate–silicon environmental barrier coatings to thermal cycling in water vapor10.1016/j.actamat.2015.12.053 ↗
17. Degradation of ytterbium disilicate environmental barrier coatings in high temperature steam atmosphere10.1016/j.jeurceramsoc.2019.04.034 ↗
18. Tailoring thermal properties of multi-component rare earth monosilicates10.1016/j.actamat.2020.06.012 ↗
19. Study on water vapor corrosion resistance of rare earth monosilicates RE2SiO5 (RE = Lu, Yb, Tm, Er, Ho, Dy, Y, and Sc) from first-principles calculations10.1016/j.heliyon.2018.e00857 ↗
20. High temperature water vapour corrosion of rare earth disilicates (Y,Yb,Lu)2Si2O7 in the presence of Al(OH)3 impurities10.1016/j.jeurceramsoc.2006.09.013 ↗
21. Synthesis and structures of high-entropy pyrochlore oxides10.1016/j.jeurceramsoc.2019.12.008 ↗
22. From high-entropy ceramics to compositionally-complex ceramics: a case study of fluorite oxides10.1016/j.jeurceramsoc.2020.01.015 ↗
23. High-entropy alumino-silicides: a novel class of high-entropy ceramics10.1007/s40843-019-9585-3 ↗
24. High temperature corrosion of (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 environmental barrier coating material subjected to water vapor and molten calcium–magnesium–aluminosilicate (CMAS)10.1016/j.corsci.2020.108881 ↗
25. Theoretical investigation of phonon contributions to thermal expansion coefficients for rare earth monosilicates RE2SiO5 (RE = Dy, Ho, Er, Tm, Yb and Lu)10.1016/j.jeurceramsoc.2019.09.042 ↗
26. High entropy (Yb0.25Y0.25Lu0.25Er0.25)2SiO5 with strong anisotropy in thermal expansion10.1016/j.jmst.2019.07.022 ↗
27. Equiatomic quaternary (Y1/4Ho1/4Er1/4Yb1/4)2SiO5 silicate: a perspective multifunctional thermal and environmental barrier coating material10.1016/j.scriptamat.2019.04.018 ↗
28. Towards thermal barrier coating application for rare earth silicates RE2SiO5 (RE= La, Nd, Sm, Eu, and Gd)10.1016/j.jeurceramsoc.2018.12.015 ↗
29. Theoretical and experimental determination of the major thermo-mechanical properties of RE2SiO5 (RE=Tb, Dy, Ho, Er, Tm, Yb, Lu, and Y) for environmental and thermal barrier coating applications10.1016/j.jeurceramsoc.2015.09.013 ↗
30. Yttrium silicate coatings for oxidation protection of carbon-silicon carbide composites10.1111/j.1151-2916.2000.tb01392.x ↗